Orginal Article

Forming Limit of FSW Aluminum Alloy Blank Based on a New Constitutive Model

  • Guannan CHU ,
  • Yanli LIN ,
  • Weining SONG ,
  • Lin ZHANG
Expand
  • 1 School of Materials Science & Engineering, Harbin Institute of Technology at Weihai, Weihai 264209, China;
    2 Weihai Northern Electric Group Company Limited, Weihai 264209, China

Received date: 2016-05-10

  Online published: 2016-11-09

Supported by

Supported by National Natural Science Foundation of China (Nos.51405102 and 51475121), China Postdoctoral Science Foundation (No.2015M570286), Fundamental Research Funds for the Central Universities of China (No.HIT.NSRIF.2016093), and the Scientific Research Foundation of Harbin Institute of Technology at Weihai (No.HIT(WH)201414)

Abstract

Automobile lightweight can effectively save fuel consumption and reduce CO2 emissions. Aluminum and its alloys are desirable for the automotive industry due to their excellent high-strength to weight ratio. However, due to the introduction of the welding seam, it has brought new changes to the forming process, especially to the forming limit. To establish a reasonable forming limit curve (FLC) analysis method of friction stir welding (FSW) aluminum alloy blank, a new theoretical model was proposed based on the new second order function constitutive model. The main idea is using the differences in mechanical property between the welding and heat affected zone substitution for the hypothesis of geometry groove in the classic M-K theoretical model. The new second order function constitutive model was applied to M-K theoretical model. Eventually, a new FLC theoretical model for FSW aluminum alloy blank was established. Such theoretical model also overcomes the low strain hardening exponent of aluminum alloy material, which leads to a poor regression accuracy by power-exponent function model. The forming limit test for FSW aluminum alloy blank was performed, and the real-time strain was measured by three-dimensional digital speckle strain measurement system (XJTUDIC). Finally, the results of experiments and the theoretical analysis are compared. Compared with the traditional power law, the regression result of the new second order function constitutive model on the stress-strain curve no matter in the initial yield stage or in late deformation stage has a good fitting precision. The maximum fitting error of the power law on the stress-strain curve is more than 12%, but the fitting error of the new second order function constitutive model is less than 1%. The theoretical prediction based on the new second order function constitutive model is significantly better than the theoretical predictions based on power law in predicting the forming limit of FSW aluminum alloy blank. The prediction error of the first principal strain based on the new second order function constitutive model is less than 0.01. While the maximum prediction error of the first principal strain based on the power law is 0.14.

Cite this article

Guannan CHU , Yanli LIN , Weining SONG , Lin ZHANG . Forming Limit of FSW Aluminum Alloy Blank Based on a New Constitutive Model[J]. Acta Metall Sin, 2017 , 53(1) : 114 -122 . DOI: 10.11900/0412.1961.2016.00178

References

[1] Liu J A.Make great efforts to develop aluminum parts industry and promote the modernization progress of automobile industry[J]. Alum. Fabr., 2005, (3): 8
[1] (刘静安. 大力发展铝合金零部件产业促进汽车工业的现代化进程[J]. 铝加工, 2005, (3): 8)
[2] Chen Y L.The development status and prospects of automobile lightweight technology[J]. Auto Technol. Mater., 2012, (1): 1
[2] (陈一龙. 汽车轻量化技术发展状况及展望[J]. 汽车工艺与材料, 2012, (1): 1)
[3] Zhu J F.Aluminum alloy used for automobile outer panel at abroad[J]. Metall. Inf. Rev., 2005, (1): 25
[3] (朱久发. 国外汽车面板用铝合金材料[J]. 冶金信息导刊, 2005, (1): 25)
[4] Kumar M, Sotirov N, Chimani C M.Investigations on warm forming of AW-7020-T6 alloy sheet[J]. J. Mater. Process. Tech., 2014, 214: 1769
[5] Zhong Q, Shi Y, Liu B.The application of aluminum alloy in automotive light weighting[J]. Adv. Mater. Ind., 2015, (2): 23
[5] (钟奇, 施毅, 刘博. 铝合金在汽车轻量化中的应用[J]. 新材料产业, 2015, (2): 23)
[6] Ma M T, Li Z G, Yi H L, et al.Polarization of light-weighted cars and application of aluminum alloys[J]. World Nonferrous. Met, 2006, (10): 10
[6] (马鸣图, 李志刚, 易红亮等. 汽车轻量化及铝合金的应用[J]. 世界有色金属, 2006, (10): 10)
[7] Zheng H, Zhao X Y.Lightweight automobile and application of aluminum alloys in modern automobile production[J]. Forg. Stamp. Technol., 2016, 41: 1
[7] (郑晖, 赵曦雅. 汽车轻量化及铝合金在现代汽车生产中的应用[J]. 锻压技术, 2016, 41: 1)
[8] Banabic D.Sheet Metal Forming Processes[M]. Berlin: Springer, 2010: 156
[9] Keeler S P, BackofenW A. Plastic instability and fracture in sheets stretched over rigid punches[J]. Trans. ASM, 1963, 56: 25
[10] Olsen TY.Machines for ductility testing[J]. ASTM, 1920, 20: 398
[11] Banabic D.Forming Limits of Sheet Metal[M]. Berlin: Springer, 2000: 173
[12] Swift H W.Plastic instability under plane stress[J]. J. Mech. Phys. Solids, 1952, 1: 1
[13] Hill R.On discontinuous plastic states, with special reference to localized necking in thin sheets[J]. J. Mech. Phys. Solids, 1952, 1: 19
[14] Hora P, Longchang T, Reissner J, et al.Prediction methods for ductile sheet metal failure using FE-simulation [A]. Proceedings of the IDDRG Congress[C]. Porto: IDDRG, 1994: 363
[15] Marciniak Z, Kuczyński K.Limit strains in the processes of stretch-forming sheet metal[J]. Int. J. Mech. Sci.,1967, 9: 609
[16] Marciniak Z, Kuczyński K, Pokora T.Influence of the plastic properties of a material on the forming limit diagram for sheet metal in tension[J]. Int. J. Mech. Sci.,1973, 15: 789
[17] Hutchinson J W, Neale K W, Needleman A.Sheet necking—I. Validity of plane stress assumptions of the long-wavelength approximation (A). In: Koistinen D P, Wang N M eds., Mechanics of Sheet Metal Forming [M]. New York/London: Plenum Press, 1978: 111
[18] St?ren S, Rice J R.Localized necking in thin sheets[J]. J. Mech. Phys. Solids, 1975, 23: 421
[19] Dudzinski D, Molinari A.Perturbation analysis of thermoviscoplastic instabilities in biaxial loading[J]. Int. J. Solids Struct., 1991, 27: 601
[20] Yu Z Q, Kong Q S, Ma C H, et al.Theoretical and experimental study on formability of laser seamed tube hydroforming[J]. Int. J. Adv. Manuf. Technol., 2014, 75: 305.
[21] Chen X F, Yu Z Q, Hou B, et al.A theoretical and experimental study on forming limit diagram for a seamed tube hydroforming[J]. J. Mater. Process. Technol., 2011, 211: 2012
[22] He Z B, Yuan S J, Lin Y L, et al.Analytical model for tube hydro-bulging test, part I: models for stress components and bulging zone profile[J]. Int. J. Mech. Sci., 2014, 87: 297
[23] He Z B, Yuan S J, Lin Y L, et al.Analytical model for tube hydro-bulging tests, part II: linear model for pole thickness and its application[J]. Int. J. Mech. Sci., 2014, 87: 307
[24] Chu G N, Liu W J.Experimental observations of 5A02 aluminum alloy in electromagnetically assisted tube hydroforming[J]. JOM, 2013, 65: 599
[25] Chu G N, Yang S, Wang J X.Mechanics condition of thin-walled tubular component with rib hydroforming[J]. Trans. Nonferrous Met. Soc. China, 2012, 22(suppl.2): s280
[26] Hu W L, Lin Y L, Yuan S J, et al. Constitutive models for regression of various experimental stress-strain relations [J]. Int. J. Mech. Sci., 2015, 101-102: 1
[27] Hu Z L. Research on the plastic deformation behavior of friction stir welded2024 aluminum alloy tube [D]. Harbin: Harbin Institute of Technology, 201
[27] 3(胡志力. 2024铝合金搅拌摩擦焊管材塑性变形行为研究 [D]. 哈尔滨: 哈尔滨工业大学, 2013)
Outlines

/