Orginal Article

Study on the Microstructural Evolution and Mechanical Properties Control of a Strong Textured AZ31 Magnesium Alloy Sheet During Cryorolling

  • Yaqiong YAN ,
  • Jinru LUO ,
  • Jishan ZHANG ,
  • Linzhong ZHUANG
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2016-04-12

  Online published: 2016-10-28

Supported by

Supported by National Natural Science Foundation of China (No.51401019), China Postdoctoral Science Foundation (No.2014M550612), Fundamental Research Funds for the Central Universities (Nos.FRF-TP-14-048A1 and FRF-TP-15-055A2) and Common Construction Project from Beijing Municipal Commission of Education (No.FRF-SD-13-005B)

Abstract

A strongly basal textured AZ31 magnesium alloy sheet with the normal direction (ND) perpendicular to the c-axis has been cryorolled at the liquid-nitrogen temperature to the strain of different amount to analyze the influence of cryogenic rolling temperature. The microstructure and texture of the cryorolled samples have been investigated by using SEM, EBSD and XRD. And the mechanical properties of the cryorolled sheets have also been tested under quasi-static uni-axial tension at the ambient temperature along the rolling direction (RD) and transverse direction (TD) respectively. The microstructural and textual evolutions of the strongly basal textured AZ31 magnesium alloy sheets during cryorolling and the relationship between mechanical properties and the microstructural and textural evolutions of cryorolled samples has also been discussed in this work. The results show that a lot of twins have been observed in cryorolled sheets, and they were found to be {101?2} tension twins. {101?2} tension twins were the dominant twinning type of the AZ31 magnesium alloy sheet during cryogenic rolling. With the increase of cryogenic rolling pass, new texture component with the c-axis paralleled to the normal direction (ND) was strengthened and the breadth of {101?2} tension twins was also increased. Grains were separated by the twin grain boundaries after cryorolling. The mechanical test results show that the strength of the sheets increased while the ductility decreased after cryogenic rolling. The strength of the sheets along RD was higher than that along TD.

Cite this article

Yaqiong YAN , Jinru LUO , Jishan ZHANG , Linzhong ZHUANG . Study on the Microstructural Evolution and Mechanical Properties Control of a Strong Textured AZ31 Magnesium Alloy Sheet During Cryorolling[J]. Acta Metall Sin, 2017 , 53(1) : 107 -113 . DOI: 10.11900/0412.1961.2016.00134

References

[1] Easton M, Beer A, Barnett M, et al.Magnesium alloy applications in automotive structures[J]. JOM, 2008, 60(11): 57
[2] Mordike B L, Ebert T.Magnesium: properties-applications-potential[J]. Mater. Sci. Eng., 2001, A302: 37
[3] Bamberger M, Dehm G.Trends in the development of new Mg alloys[J]. Annu. Rev. Mater. Res., 2008, 38: 505
[4] Chino Y, Kimura K, Hakamada M, et al.Mechanical anisotropy due to twinning in an extruded AZ31 Mg alloy[J]. Mater. Sci. Eng., 2008, A485: 311
[5] Al-Samman T.Comparative study of the deformation behavior of hexagonal magnesium-lithium alloys and a conventional magnesium AZ31 alloy[J]. Acta Mater., 2009, 57: 2229
[6] Chino Y, Kimura K, Mabuchi M.Deformation characteristics at room temperature under biaxial tensile stress in textured AZ31 Mg alloy sheets[J]. Acta Mater., 2009, 57: 1476
[7] Jiang L, Jonas J J, Luo A A, et al.[J]. Mater. Sci. Eng., 2007, A445-446: 302
[8] Yi S, Bohlen J, Heinemann F, et al.Mechanical anisotropy and deep drawing behaviour of AZ31 and ZE10 magnesium alloy sheets[J]. Acta Mater., 2010, 58: 592
[9] Wang Y N, Huang J C.The role of twinning and untwinning in yielding behavior in hot-extruded Mg-Al-Zn alloy[J]. Acta Mater., 2007, 55: 897
[10] Barnett M R, Keshavarz Z, Beer A G, et al.Influence of grain size on the compressive deformation of wrought Mg-3Al-1Zn[J]. Acta Mater., 2004, 52: 5093
[11] Lv F, Yang F, Duan Q Q, et al.Fatigue properties of rolled magnesium alloy (AZ31) sheet: influence of specimen orientation[J]. Int. J. Fatigue, 2011, 33: 672
[12] Huang X S, Suzuki K, Chino Y.Influences of initial texture on microstructure and stretch formability of Mg-3Al-1Zn alloy sheet obtained by a combination of high temperature and subsequent warm rolling[J]. Scr. Mater., 2010, 63: 395
[13] Luo J R, Godfrey A, Liu W, et al.Twinning behavior of a strongly basal textured AZ31 Mg alloy during warm rolling[J]. Acta Mater., 2012, 60: 1986
[14] Lee Y B, Shin D H, Park K T, et al.Effect of annealing temperature on microstructures and mechanical properties of a 5083 Al alloy deformed at cryogenic temperature[J]. Scr. Mater., 2004, 51: 355
[15] Rangaraju N, Raghuram T, Krishna B V, et al.Effect of cryo-rolling and annealing on microstructure and properties of commercially pure aluminium[J]. Mater. Sci. Eng., 2005, A398: 246
[16] Lee T R, Chang C P, Kao P W.The tensile behavior and deformation microstructure of cryo-rolled and annealed pure nickel[J]. Mater. Sci. Eng., 2005, A408: 131
[17] Nagarjuna S, Babu U C, Ghosal P.Effect of cryo-rolling on age hardening of Cu-1.5Ti alloy[J]. Mater. Sci. Eng., 2008, A491: 331
[18] Wang Y M, Chen M W, Zhou F H, et al.High tensile ductility in a nanostructured metal[J]. Nature, 2002, 419: 912
[19] Al-Samman T, Gottstein G.Influence of strain path change on the rolling behavior of twin roll cast magnesium alloy[J]. Scr. Mater., 2008, 59: 760
[20] Beausir B, Biswas S, Kim D I, et al.Analysis of microstructure and texture evolution in pure magnesium during symmetric and asymmetric rolling[J]. Acta Mater., 2009, 57: 5061
[21] Pérez-Prado M T, del Valle J A, Contreras J M, et al. Microstructural evolution during large strain hot rolling of an AM60 Mg alloy[J]. Scr. Mater., 2004, 50: 661
[22] Liu Q.Research progress on plastic deformation mechanism of Mg alloys[J]. Acta Metall. Sin., 2010, 46: 1458
[22] (刘庆. 镁合金塑性变形机理研究进展[J]. 金属学报, 2010, 46: 1458)
[23] Chapuis A, Driver J H.Temperature dependency of slip and twinning in plane strain compressed magnesium single crystals[J]. Acta Mater., 2011, 59: 1986
[24] Hutchinson W B, Barnett M R.Effective values of critical resolved shear stress for slip in polycrystalline magnesium and other hcp metals[J]. Scr. Mater., 2010, 63: 737
[25] Luo J R, Liu Q, Liu W, et al.[J]. Acta Metall. Sin., 2012, 48: 717
[25] (罗晋如, 刘庆, 刘伟等. [J]. 金属学报, 2012, 48: 717)
[26] Luo J R, Liu Q, Liu W, et al.[J]. Acta Metall. Sin., 2011, 47: 1567
[26] (罗晋如, 刘庆, 刘伟等. [J]. 金属学报, 2011, 47: 1567)
[27] Yoshinaga H, Obara T, Morozumi S.Twinning deformation in magnesium compressed along the c-axis[J]. Mater. Sci. Eng., 1973, 12: 255
[28] Read-Hill R E, Robertson W D. Additional modes of deformation twinning in magnesium[J]. Acta Metall., 1957, 5: 717
[29] Luo J R, Chen X P, Xin R L, et al.Comparison of microstructure and properties of AZ31 Mg alloy sheet produced through different routes[J]. Trans. Nonferrous Met. Soc. China, 2008, 18: s194
[30] Barnett M R.Twinning and the ductility of magnesium alloys: Part I: “Tension” twins[J]. Mater. Sci. Eng., 2007, A464: 1
[31] Barnett M R.Twinning and the ductility of magnesium alloys: Part II. “Contraction” twins[J]. Mater. Sci. Eng., 2007, A464: 8
[32] Jiang J, Godfrey A, Liu W, et al.Identification and analysis of twinning variants during compression of a Mg-Al-Zn alloy[J]. Scr. Mater., 2008, 58: 122
Outlines

/