A First-Principles Study on Crystal Structure, Phase Stability and Magnetic Properties of Ni-Mn-Ga-Cu Ferromagnetic Shape Memory Alloys
Received date: 2016-04-18
Online published: 2016-10-25
Supported by
Supported by National Natural Science Foundation of China (Nos.51301036 and 51431005), High Technology Research and Development Program of China (No.2015AA034101), Fundamental Research Funds for the Central Universities (No.N130523001) and Natural Science Foundation of Hebei Province (No.E2013501089)
Ni-Mn-Ga ferromagnetic shape memory alloys (FSMAs) have attracted great attention for more than two decades, due to their large magnetic shape memory effect that originates from the rearrangement of martensitic variants under an external magnetic field. Over the past decade, accumulated knowledge on the properties of Ni-Mn-Ga Heusler alloys has allowed people to foresee the possibility of employing these alloys in device applications. However, the low operating temperatures and high brittleness remain the major drawbacks for the industrial application. Consequently, there has been growing interest in the modification of Ni-Mn-Ga alloys by adding a fourth element to increase transformation temperatures and to improve ductility. A recent study shows that the ductility has been effectively improved in Cu-doped Ni-Mn-Ga alloy under the situation of single phase via strengthening grain boundaries. In addition, the crystal structure, martensitic transformation, magnetic properties, high temperature magnetoplasticity and magnetocaloric effect have been reported in Ni-Mn-Ga-Cu alloys. Experimental results have shown that the martensitic transformation temperature (Tm) is drastically increased and the Curie temperature (TC) slightly decreased with Cu addition. As already known, the alloying elements affect both the crystal and electronic structures and hence the stability of austenite and martensite phases. Therefore, knowledge of the effects of Cu addition is of great importance to understand the composition dependence of Tm and TC. First-principles calculation results on Ni8Mn4-xGa4Cux (x=0, 0.5, 1, 1.5 and 2) ferromagnetic shape memory alloys of this research draw following conclusions. The added Cu atom preferentially occupies the Mn site. The formation energy results indicate that ferromagnetic austenite is more stable than the paramagnetic one. The ferromagnetic state becomes instable and paramagnetic state becomes more stable when Mn is gradual substituted by Cu. The evaluated TC decreases with increasing Cu content that is derived from the decrease of total energy difference between the paramagnetic and the ferromagnetic austenite. The experimentally observed decrease of Tm is originated from the decrease of total energy difference between the austenite and the non-modulated martensite. The difference between the up and down DOS is reduced with the increasing Cu content that gives rise to the decrease of the total magnetic moments. The purpose of this work is to explore the influence of Cu addition on crystal structure, Tm, TC and electronic structures of Ni8Mn4-xGa4Cux (x=0, 0.5, 1, 1.5 and 2) alloys by first-principles calculations, aiming at providing theoretical data and directions for developing high performance FSMAs.
Jing BAI , Ze LI , Zhen WAN , Xiang ZHAO . A First-Principles Study on Crystal Structure, Phase Stability and Magnetic Properties of Ni-Mn-Ga-Cu Ferromagnetic Shape Memory Alloys[J]. Acta Metall Sin, 2017 , 53(1) : 83 -89 . DOI: 10.11900/0412.1961.2016.00142
| [1] | Sozinov A, Likhachev A A, Lanska N, et al.Giant magnetic-field-induced strain in NiMnGa seven-layered martensitic phase[J]. Appl. Phys. Lett., 2002, 80: 1746 |
| [2] | Henry C P, Bono D, Feuchtwanger J, et al.AC field-induced actuation of single crystal Ni-Mn-Ga[J]. J. Appl. Phys., 2002, 91: 7810 |
| [3] | Gao L, Cai W, Liu A L, et al.Martensitic transformation and mechanical properties of polycrystalline Ni50Mn29Ga21-xGdx ferromagnetic shape memory alloys[J]. J. Alloys Compd., 2006, 425: 314 |
| [4] | Guo S H, Zhang Y H, Zhao Z Q, et al.Effects of Sm on phase transformation in Ni-Mn-Ga alloys[J]. J. Rare Earth, 2004, 22: 875 |
| [5] | Tsuchiya K, Tsutsumi A, Ohtsuka H, et al.Modification of Ni-Mn-Ga ferromagnetic shape memory alloy by addition of rare earth elements[J]. Mater. Sci. Eng., 2004, A378: 370 |
| [6] | Wang H B, Chen F, Gao Z Y, et al. Effect of Fe content on fracture behavior of Ni-Mn-Fe-Ga ferromagnetic shape memory alloys [J]. Mater. Sci. Eng., 2006, A438-440: 990 |
| [7] | Yang S Y, Liu Y, Wang C P, et al.The mechanism clarification of Ni-Mn-Fe-Ga alloys with excellent and stable functional properties[J]. J. Alloys Compd., 2013, 560: 84 |
| [8] | Cong D Y, Wang S, Wang Y D, et al.Martensitic and magnetic transformation in Ni-Mn-Ga-Co ferromagnetic shape memory alloys[J]. Mater. Sci. Eng., 2008, A473: 213 |
| [9] | Li Y Y, Wang J M, Jiang C B.Study of Ni-Mn-Ga-Cu as single-phase wide-hysteresis shape memory alloys[J]. Mater. Sci. Eng., 2011, A528: 6907 |
| [10] | Stadler S, Khan M, Mitchell J, et al.Magnetocaloric properties of Ni2Mn1-xCuxGa[J]. Appl. Phys. Lett., 2006, 88: 192511 |
| [11] | Glavatskyy I, Glavatska N, Dobrinsky A, et al.Crystal structure and high-temperature magnetoplasticity in the new Ni-Mn-Ga-Cu magnetic shape memory alloys[J]. Scr. Mater., 2007, 56: 565 |
| [12] | Duan J F, Long Y, Bao B, et al.Experimental and theoretical investigations of the magnetocaloric effect of Ni2.15Mn0.85-xCuxGa (x=0.05, 0.07) alloys[J]. J. App. Phys., 2008, 103: 063911 |
| [13] | Jiang C B, Wang J M, Li P P, et al.Search for transformation from paramagnetic martensite to ferromagnetic austenite: NiMnGaCu alloys[J]. Appl. Phys. Lett., 2009, 95: 012501 |
| [14] | Roy S, Blackburn E, Valvidares S M, et al.Delocalization and hybridization enhance the magnetocaloric effect in Cu-doped Ni2MnGa[J]. Phys. Rev., 2009, 79B: 235127 |
| [15] | Li C M, Luo H B, Hu Q M, et al.Site preference and elastic properties of Fe-, Co-, and Cu-doped Ni2MnGa shape memory alloys from first principles[J]. Phys. Rev., 2011, 84B: 024206 |
| [16] | Sokolovskiy V, Buchelnikov V, Skokov K, et al.Magnetocaloric and magnetic properties of Ni2Mn1-xCuxGa Heusler alloys: an insight from the direct measurements and ab initio and Monte Carlo calculations[J]. J. Appl. Phys., 2013, 114: 183913 |
| [17] | Li G J, Liu E K, Zhang H G, et al.Role of covalent hybridization in the martensitic structure and magnetic properties of shape-memory alloys: the case of Ni50Mn5+xGa35-xCu10[J]. Appl. Phys. Lett., 2013, 102: 062407 |
| [18] | Zeleny M, Sozinov A, Straka L, et al.First-principles study of Co- and Cu-doped Ni2MnGa along the tetragonal deformation path[J]. Phys. Rev., 2014, 89B: 184103 |
| [19] | Li Z B, Zou N F, Sánchez-Valdés C F, et al. Thermal and magnetic field-induced martensitic transformation in Ni50Mn25-xGa25Cux (0≤x≤7) melt-spun ribbons[J]. J. Phys., 2016, 49D: 025002 |
| [20] | Hafner J.Atomic-scale computational materials science[J]. Acta Mater., 2000, 48: 71 |
| [21] | Kresse G, Furthmüller J.Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set[J]. Phys. Rev., 1996, 54B: 11169 |
| [22] | Bl?chl P E.Projector augmented-wave method[J]. Phys. Rev., 1994, 50B: 17953 |
| [23] | Kresse G, Joubert D.From ultrasoft pseudopotentials to the projector augmented-wave method[J]. Phys. Rev., 1999, 59B: 1758 |
| [24] | Perdew J P, Wang Y.Accurate and simple analytic representation of the electron-gas correlation energy[J]. Phys. Rev., 1992, 45B: 13244 |
| [25] | Monkhorst H J, Pack J D.Special points for Brillouin-zone integrations[J]. Phys. Rev., 1976, 13B: 5188 |
| [26] | Cong D Y, Zetterstr?m P, Wang Y D, et al.Crystal structure and phase transformation in Ni53Mn25Ga22 shape memory alloy from 20 K to 473 K[J]. Appl. Phys. Lett., 2005, 87: 111906 |
| [27] | Wu S K, Yang S T.Effect of composition on transformation temperatures of N-Mn-Ga shape memory alloys[J]. Mater. Lett., 2003, 57: 4291 |
| [28] | Bai J, Raulot J M, Zhang Y D, et al.Crystallographic, magnetic, and electronic structures of ferromagnetic shape memory alloys Ni2XGa (X=Mn, Fe, Co) from first-principles calculations[J]. J. Appl. Phys., 2011, 109: 014908 |
| [29] | Bai J, Raulot J M, Zhang Y D, et al.Defect formation energy and magnetic structure of shape memory alloys Ni-X-Ga (X=Mn, Fe, Co) by first principle calculation[J]. J. Appl. Phys., 2010, 108: 064904 |
| [30] | Brown P J, Crangle J, Kanomata T, et al.The crystal structure and phase transitions of the magnetic shape memory compound Ni2MnGa[J]. J. Phys.: Condens. Matter, 2002, 14: 10159 |
| [31] | Ayuela A, Enkovaara J, Nieminen R M.Ab initio study of tetragonal variants in Ni2MnGa alloy[J]. J. Phys.: Condens. Matter, 2002, 14: 5325 |
| [32] | Bungaro C, Rabe K M, Corso A D.First-principles study of lattice instabilities in ferromagnetic Ni2MnGa[J]. Phys. Rev., 2003, 68B: 134104 |
| [33] | Chakrabarti A, Biswas C, Banik S, et al.Influence of Ni doping on the electronic structure of Ni2MnGa[J]. Phys. Rev., 2005, 72B: 073103 |
| [34] | Fujii S, Ishida S, Asano S.Electronic structure and lattice transformation in Ni2MnGa and Co2NbSn[J]. J. Phys. Soc. Jpn., 1989, 58: 3657 |
| [35] | Velikokhatnyi O I, Nuamov I I.Electronic structure and instability of Ni2MnGa[J]. Phys. Solid State, 1999, 41: 617 |
| [36] | Chen J, Li Y, Shang J X, et al.First principles calculations on martensitic transformation and phase instability of Ni-Mn-Ga high temperature shape memory alloys[J]. Appl. Phys. Lett., 2006, 89: 231921 |
| [37] | Bl?chl P E, Jepsen O, Andersen O K.Improved tetrahedron method for Brillouin-zone integrations[J]. Phys. Rev., 1994, 49B: 16223 |
/
| 〈 |
|
〉 |