EVALUATING SERVICE TEMPERATURE FIELD OF HIGH PRESSURE TURBINE BLADES MADE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY BASED ON MICRO-STRUCTURAL EVOLUTION
Received date: 2016-05-03
Online published: 2016-10-18
Supported by
Supported by National High Technology Research and Development Program of China (No. 2012AA03A513) and Science Foundation of Ministry of Education of China (No. 625010337)
To get the actual service temperature distribution of turbine blades in aeroengines is very important for the design and maintenance. However, the acquisition of service temperature distribution has always been a challenge due to the complex and severe working condition of turbine blades. In this work, one turbine blade made of directionally solidified DZ125 superalloy was investigated after the service in air for 900 h. The microstructural evolution of DZ125 superalloy after thermal exposure at 900~1100 ℃ without the stress in different time period was also investigated, for comparison. According to microstructural degradation behaviors in the dendritic region, interdendritic region, carbides and grain boundary of DZ125 superalloy before and after service, the volume fraction of γ precipitates in the dendritic region was determined as the quantitative characterization parameter. A method to evaluate the service temperature of turbine blades was developed, based on the quantitative characterization of microstructural evolution, such as the relationship between the thermally exposured temperature and volume fraction of γ precipitates. The equivalent average service temperature (Tave) and the equivalent maximum service temperature (Tmax) were proposed based on the assumption of the constant temperature during service and the nearly service condition with variable temperature of blades, respectively. The results indicate that the service temperature was higher in the middle of the blade, and became lower at the locations closer to the tip or the root. For each cross-section, the service temperatures of the serviced blade in the descending order were leading edge, pressure side, trailing edge and suction side. The highest service temperature of 1050~1100 ℃ appeared at the leading edge in the middle of the blade. The distribution trend of Tave agreed well with that of Tmax, but Tmax was higher than Tave in some locations of the blade. This work suggests that the evaluation results of Tmax were more reasonable than those of Tave. This method would be helpful to establish the assessment method of the service-induced microstructural damage in turbine blades made of directionally solidified superalloys.
Yadong CHEN , Yunrong ZHENG , Qiang FENG . EVALUATING SERVICE TEMPERATURE FIELD OF HIGH PRESSURE TURBINE BLADES MADE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY BASED ON MICRO-STRUCTURAL EVOLUTION[J]. Acta Metall Sin, 2016 , 52(12) : 1545 -1556 . DOI: 10.11900/0412.1961.2016.00170
| [1] | Dong Z G, Wang M, Li X X, Teng B Q. J Steel Res, 2011; 23: 455 |
| [1] | (董志国, 王鸣, 李晓欣, 滕佰秋. 钢铁研究学报, 2011; 23: 455) |
| [2] | Ali A R A, Janajreh I.Energy Procedia, 2015; 75: 3220 |
| [3] | Dye D, Anxin M, Reed R C.In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloys 2008, Warrendale: Minerals, Metals & Materials Soc, 2008: 911 |
| [4] | Cheng W F, Wen Z T, Guang C B.Aerosp Sci Technol, 2014; 39: 588 |
| [5] | Wen Z X, Hou N, Wang B.Multi Model Mater Str, 2010; 6: 508 |
| [6] | Carter T J.Eng Fail Anal, 2005; 12: 237 |
| [7] | Kim S G, Hwang Y H, Kim T G, Shu C M.Eng Fail Anal, 2008; 15: 394 |
| [8] | Tong J Y, Ding X F, Wang M L, Zheng Y R, Yagi K, Feng Q.Mater Sci Eng, 2014; A618: 605 |
| [9] | Yang J X, Zheng Q, Sun X F, Guan H R, Hu Z Q.Mater Sci Eng, 2007; A457: 148 |
| [10] | Miura N, Nakata K, Miyazaki M, Hayashi Y, Kondo Y.In: Chandra T, Reimers W, Wanderka N, Ionescu M eds., 6th Int Conf on Processing and Manufacturing of Advanced Materials, Berlin: Materials Science Forum, 2010: 2291 |
| [11] | Wu X, Beres W, Zhang Z, Reed P.In: Badyda K, Bujalski W, Milewski J, Warchol M, Nowowiejska U eds., ASME Turbo Expo 2010 Power for Land, Sea and Air, Glasgow: ASME Press, 2010: 499 |
| [12] | Xu X, Yu Z.Eng Fail Anal, 2007; 14: 1322 |
| [13] | Feng Q, Tong J Y, Zheng Y R, Wang M L, Wei W J, Zhao H L, Yuan X F, Ding X F.Mater China, 2012; 31(12): 21 |
| [13] | (冯强, 童锦艳, 郑运荣, 王美玲, 魏文娟, 赵海龙, 袁晓飞, 丁贤飞. 中国材料进展, 2012; 31(12): 21) |
| [14] | Cai Y L, Zheng Y R.Metallographic Research of Superalloys. Beijing: National Defense Industry Press, 1986: 228 |
| [14] | (蔡玉林, 郑运荣. 高温合金的金相研究. 北京: 国防工业出版社, 1986: 228) |
| [15] | Yuan X F, Song J X, Zheng Y R, Huang Q, Yagi K, Xiao C B, Feng Q.J Alloys Compd, 2016; 662: 583 |
| [16] | Yuan X F, Song J X, Zheng Y R, Huang Q, Yagi K, Xiao C B, Feng Q.Mater Sci Eng, 2016; A651: 734 |
| [17] | Wang C S, Zhang J, Liu L, Fu H Z.J Alloys Compd, 2010; 508: 440 |
| [18] | Miura N, Kondo Y.J ASTM Int, 2011; 9: 1 |
| [19] | Murakumo T, Kobayashi T, Koizumi Y, Harada H.Acta Mater, 2004; 52: 3737 |
| [20] | Yu Y N, Yang P, Qiang W J, Chen L.Foundations of Materials Science. Beijing: High Education Press, 2006: 26 |
| [20] | (余永宁, 杨平, 强文江, 陈冷. 材料科学基础. 北京: 高等教育出版社, 2006: 266) |
| [21] | Giraud R, Hervier Z, Cormier J, Staint-Martin G, Hamon F, Mihet X, Mendez J.Metall Mater Trans, 2012; 44: 131 |
| [22] | Roebuck B, Cox D, Reed R.Scr Mater, 2001; 44: 917 |
| [23] | Liu P C, Zhang X N, Ge L, Li X.J Chin Electron Microsc Soc, 2015; 34: 298 |
| [23] | (刘程鹏, 张晓娜, 葛麟, 李宪. 电子显微学报, 2015; 34: 298) |
| [24] | Pierret S, Etter T, Evans A, Swygenhoven H V.Acta Mater, 2013; 61: 1478 |
| [25] | Reyhani M R, Alizadeh M, Fathi A, Khaledi H.Propul Power Res, 2013; 2: 148 |
/
| 〈 |
|
〉 |