Orginal Article

EFFECTS OF DEUTERIUM CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Zr-4 ALLOY

  • Cheng ZHANG ,
  • Xiping SONG ,
  • Jingru LIU ,
  • Yun YANG ,
  • Li YOU
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2015-05-17

  Online published: 2016-09-28

Supported by

Supported by National Natural Science Foundation of China (Nos.21171018 and 51271021)

Abstract

Zirconium alloy has been employed widely in nuclear industry, yet the absorption of deuterium in zircaloy is considered to play a critical role in mechanical properties especially in high temperature under a loss of coolant accident (LOCA) and application for deuterium storage. However, little is known about the microstructure evolution of zircaloy during deuterium absorption. In this work, deuterium was charged into the sample at 900oC and different pressures, and the effects of deuterium content on microstructure and mechanical properties of Zr-4 alloy have been studied by means of OM, BSE, SEM, XRD, and hardness and compressive tests. The results showed that the amount of deuteride increased with the increase of deuterium content from 1.35% to 2.21%, accompanying with the morphology variations from intragranular deuteride needles to intergranular deuteride blocks, which formed an interlinked deuteride configuration and grew into equiaxed α-Zr grains. Deuteride layer was observed on the surface of sample at higher deuterium content with the micro-crack appeared within it. The mostly deuteride was δ-deuteride, and ε-deuteride was observed on sample surface with high deuterium content. There existed a hardness gradient from surface to center. With the increase of deuterium content, the hardness increased and hardness gradient became evident. With increasing deuterium content, the compressive yield strength of samples in creased slightly, but the compressive ultimate strength decreased greatly from 1176 MPa (1.35%) to 856 MPa (2.21%). The deceasing of compressive ultimate strength was probably related to the formation of micro-crack. The cracks nucleated and propagated within the intergranular deuteride blocks, which leads to the degradation of compressive ultimate strength.

Cite this article

Cheng ZHANG , Xiping SONG , Jingru LIU , Yun YANG , Li YOU . EFFECTS OF DEUTERIUM CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Zr-4 ALLOY[J]. Acta Metall Sin, 2016 , 52(12) : 1572 -1578 . DOI: 10.11900/0412.1961.2016.00193

References

[1] Zinkle S J, Was G S.Acta Mater, 2013; 61: 735
[2] Li Z K, Liu J Z, Xue X Y.Mat-China, 2007; 26(1): 6
[2] (李中奎, 刘建章, 薛祥义. 中国材料进展, 2007; 26(1): 6)
[3] Northwood D O.Mater Des, 1985; 6: 58
[4] Motta A T, Yilmazbayhan A, Da Silva M J G, Comstock R J, Was G S, Busby J T, Gartner E, Peng Q, Jeong Y H, Park J Y.J Nucl Mater, 2007; 371: 61
[5] Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y.Acta Metall Sin, 2011; 47: 865
[5] (姚美意, 李士炉, 张欣, 彭剑超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865)
[6] Sun G C, Zhou B X, Yao M Y, Xie S J, Li Q.Acta Metall Sin, 2012; 48: 1103
[6] (孙国成, 周邦新, 姚美意, 谢世敬, 李强. 金属学报, 2012; 48: 1103)
[7] Allen T R, Konings R J M, Motta A T. Comprehensive Nuclear Materials. Oxford: Elsevier, 2012: 49
[8] Forgeron T, Brachet J C, Barcelo F, Castaing A, Hivroz J, Mardon J P, Bernaudat C.In: Sabol G P, Moan G D eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, West Conshohocken, PA: ASTM International, 2000: 256
[9] Zinkle S J, Terrani K A, Gehin J C, Ott L J, Snead L L.J Nucl Mater, 2014; 448: 374
[10] Yang Y, Song X P, Zhang C.J Nucl Mater, 2015; 465: 97
[11] Zhao C, Song X P, Yang Y, Zhang B.Int J Hydrogen Energy, 2013; 38: 10903
[12] Yang Y, Song X P.Acta Metall Sin, 2016; 52: 100
[12] (杨云, 宋西平. 金属学报, 2016; 52: 100)
[13] Sidhu S S, Murthy N S, Campos F P.Adv Chem Ser, 1963; 39: 87
[14] Zuzek E, Abriata J P, San-Martin A, Manchester F D.Bull Alloy Phase Diagrams, 1990; 11: 385
[15] Qin W, Kiran Kumar N A P, Szpunar J A, Kozinski J.Acta Mater, 2011; 59: 7010
[16] Carpenter G J C.J Nucl Mater, 1973; 48: 264
[17] Pshenichnikov A, Stuckert J, Walter M.Nucl Eng Des, 2015; 283: 33
[18] Yamanaka S, Yoshioka K, Uno M, Katsura M, Anada H, Matsuda T, Kobayashi S. J Alloys Compd#/magtechI#, 1999; 293-295: 23
[19] Kuroda M, Setoyama D, Uno M, Yamanaka S.J Alloys Compd, 2004; 368: 211
[20] Wang Z Y, Garbe U, Li H J, Studer A J, Harrison R P, Callaghan M D, Wang Y B, Liao X Z.Scr Mater, 2012; 67: 752
[21] Wang ZY, Garbe U, Li HJ, Harrison R P, Kaestner A, Lehmann E.Metall Mater Trans, 2014; 45B: 532
[22] Simpson L A, Cann C D.J Nucl Mater, 1979; 87: 303
[23] Kim Y S, Ahn S B, Cheong Y M.J Alloys Compd, 2007; 429: 221
[24] Shi S Q, Puls M P.J Nucl Mater, 1994; 208: 232
[25] Puls M P.Metall Trans, 1988; 19A: 1507
[26] Bai J B, Fran?ois D. J Nucl Mater, 1992; 187: 186
[27] Bai J B, Prioul C, Francois D.Metall Mater Trans, 1994; 25A: 1185
[28] Grange M, Besson J, Andrieu E.Metall Mater Trans, 2000; 31A: 679
Outlines

/