Orginal Article

RECENT PROGRESS ON EVOLUTION OF PRECIPI-TATES IN INCONEL 718 SUPERALLOY

  • Yongchang LIU ,
  • Qianying GUO ,
  • Chong LI ,
  • Yunpeng MEI ,
  • Xiaosheng ZHOU ,
  • Yuan HUANG ,
  • Huijun LI
Expand
  • State Key Lab of Hydraulic Engineering Simulation and Safety, School of Materials Science & Engineering, Tianjin University, Tianjin 300354, China

Received date: 2016-07-07

  Online published: 2016-09-05

Supported by

Supported by National High Technology Research and Development Program of China (No.2015-AA042504), National Natural Science Foundation of China (No.51474156) and China National Funds for Distinguished Young Scientists (No.51325401)

Abstract

For the manufacture of complicated metallic structural components in power plants, aerospace and defense industry, Inconel 718 superalloy has been widely employed. High-temperature fatigue resistance and creep rupture strength of Inconel 718 superalloy are susceptible to the microstructure evolution in manufacture processing. Previous research work is generally focused on the parameter optimization of hot working processes (directional solidification, heat treatment, forging and welding). Relationships between the cold deformation, hot working, welding and the high-temperature mechanical performance, are seldom discussed, especially in the light of precipitate control . In this work, various types of secondary phases in Inconel 718 alloy are reviewed, including the primary strengthening phase (γ'' phase), secondary strengthening phase (γ' phase), equilibrium phase of γ'' phase (δ phase), MX-type carbonitride and Laves phase. Precipitation mechanisms of secondary phases in Inconel 718 alloy are also reviewed, as well as the effects of different types of precipitates on high-temperature performance of the Inconel 718 alloy. With respect to the high-energy electron beam welding of Inconel 718 alloys, factors contributing to the cracking in heat affected zone are indicated.

Cite this article

Yongchang LIU , Qianying GUO , Chong LI , Yunpeng MEI , Xiaosheng ZHOU , Yuan HUANG , Huijun LI . RECENT PROGRESS ON EVOLUTION OF PRECIPI-TATES IN INCONEL 718 SUPERALLOY[J]. Acta Metall Sin, 2016 , 52(10) : 1259 -1266 . DOI: 10.11900/0412.1961.2016.00290

References

[1] Guan Y S, Liu E Z, Guan X R, Liu Z.J Mater Sci Technol, 2016; 32: 271
[2] Dong J X, Liu X B, Tang B, Hu Y H, Xu Z C, Xie X S.Acta Metall Sin, 1996; 32: 241
[2] (董建新, 刘兴博, 唐宾, 胡尧和, 徐志超, 谢锡善. 金属学报, 1996; 32: 241)
[3] Zhang Y W, Hu B F.Acta Metall Sin, 2015; 51: 967
[3] (张义文, 胡本芙. 金属学报, 2015; 51: 967)
[4] Rao G A, Kumar M, Srinivas M, Sarma D S.Mater Sci Eng, 2003; A355: 114
[5] Dong X M, Zhang X L, Du K, Zhou Y Z, Jin T, Ye H Q.J Mater Sci Technol, 2012; 28: 1031
[6] Tiley J, Viswanathan G B, Srinivasan R, Banerjee R, Dimiduk D M, Fraser H L.Acta Mater, 2009; 57: 2538
[7] Li X W, Wang L, Dong J S, Lou L H.J Mater Sci Technol, 2014; 30: 1296
[8] Ma D X.Acta Metall Sin, 2015; 51: 1179
[8] (马德新. 金属学报, 2015; 51: 1179)
[9] Liu T, Dong J S, Wang L, Li Z J, Zhou X T, Lou L H, Zhang J.J Mater Sci Technol, 2015; 31: 269
[10] Xu Z H, Wang Z K, Niu J, Dai J W, He L M, Mu R D.J Alloys Compd, 2016; 676: 231
[11] Bai M W, Jiang H B, Chen Y, Chen Y Q, Grovenor C, Zhao X F, Xiao P.Mater Des, 2016; 97: 364
[12] Song K, Yu K, Lin X, Yang J, Hu H O, Huang W D.Acta Metall Sin, 2015; 51: 935
[12] (宋衎, 喻恺, 林鑫, 杨静, 胡海鸥, 黄卫东. 金属学报, 2015; 51: 935)
[13] Kirman I, Warrington D H.Metall Trans, 1970; 1A: 2667
[14] Zhao X B, Gu Y F, Lu J T, Yan J B, Yin H F.Rare Met Mater Eng, 2015; 44: 768
[14] (赵新宝, 谷月峰, 鲁金涛, 严靖博, 尹宏飞. 稀有金属材料与工程, 2015; 44: 768)
[15] Wlodek S T, Field R D.In: Loria E A ed., 3rd Int Symp on Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 659
[16] Sundararaman M, Mukhopadhyay P, Banerjee S.Metall Trans, 1988; 19A: 453
[17] Damodaram R, Raman S G S, Satyanarayana D V V, Madhusudhan R G, Prasad R K.Mater Sci Eng, 2014; A612: 414
[18] Sundararaman M, Banerjee S.Metall Mater Trans, 1992; 23A: 2015
[19] Sundararaman M, Mukhopadhyay P, Banerjee S.In: Loria E A ed., 3rd Int Symp on Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 419
[20] Asadian S, Wei L Y, Warren R.Mater Charact, 2004; 53: 7
[21] Wang W Q.Aviat Manuf Eng, 1995; (7): 15
[21] (汪文迁. 航空制造工程, 1995; (7): 15)
[22] Zhou X H.Forging Technol, 2004; 29(5): 9
[22] (周晓虎. 锻压技术, 2004; 29(5): 9)
[23] Cai D Y, Zhang W H, Liu W C.Trans Nonferrous Met Soc China, 2003; 13: 1338
[24] Sellars C M, Tegart W J.Met Sci Rev Methods, 1996; 63: 731
[25] Biswas S, Reddy G M, Mohandas T, Murthy V S.J Mater Sci, 2004; 39: 6813
[26] Zhou N, Lv D C, Zhang H L, McAllister D, Zhang F.Acta Mater, 2014; 65: 270
[27] Lin Y C, Wen D X, Deng J, Chen J.Mater Des, 2014; 59: 115
[28] Findley K O, Evans J L, Saxena A.Int Mater Rev, 2011; 56: 49
[29] Garcia C I, Wang G D, Camus D E, Loria E A, De Ardo A J. In: Loria E A ed., 3rd Int Symp on Superalloys 718, 626, 706, and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 293
[30] Ning Y Q, Fu M W, Chen X.Mater Sci Eng, 2012; A540: 164
[31] Wen D X, Lin Y C, Li H B, Chen X M, Deng J, Li L T.Mater Sci Eng, 2014; A591: 183
[32] Wen D X, Lin Y C, Chen J, Chen X M, Zhang J L, He M.Mater Sci Eng, 2015; A620: 319
[33] Thomas A, El-Wahabi M, Cabrera J M, Prad J M.J Mater Process Technol, 2006; 177: 469
[34] Zhang H Y, Zhang S H, Cheng M, Li Z X.Mater Charact, 2010; 61: 49
[35] Cheng M, Zhang H Y, Zhang S H.J Mater Sci, 2012; 47: 251
[36] Wang Y, Zhen L, Shao W Z, Yang L, Zhang X M.J Alloys Compd, 2009; 474: 341
[37] Nalawade S A, Sundararaman M, Singh J B, Verma A, Kishore R.Mater Sci Eng, 2010; A527: 2906
[38] Lin Y C, Li K K, Li H B, Wen D X.Mater Des, 2015; 74: 108
[39] Chen X M, Lin Y C, Wen D X, Zhang J L, He M.Mater Des, 2014; 57: 568
[40] Lin Y C, Chen X M, Wen D X, Chen M S.Comp Mater Sci, 2014; 83: 282
[41] Feng Y J.Master Thesis, Harbin Institute of Technology, 2012
[41] (冯莹娟. 哈尔滨工业大学硕士学位论文, 2012)
[42] Liu W C, Xiao F R, Yao M.Scr Mater, 1997; 37: 53
[43] Wei X P, Zheng W J, Song Z G, Lei T, Yong Q L, Xie Q C.J Iron Steel Res Int, 2014; 21: 375
[44] Mei Y P, Liu Y C, Liu C X, Li C, Yu L M, Guo Q Y, Li H J.J Alloys Compd, 2015; 649: 949
[45] Wang Y.Master Thesis, Harbin Institute of Technology, 2008
[45] (王岩. 哈尔滨工业大学硕士学位论文, 2008)
[46] Lin Y C, Deng J, Jiang Y Q, Liu G.Mater Des, 2014; 55: 949
[47] Kashyap B P, Chaturvedi M C. Mater Sci Eng, 2007; A445-446: 364
[48] Huang Y, Langdon T G.J Mater Sci, 2007; 42: 421
[49] Ning Y Q, Huang S B, Fu M W, Dong J.Mater Charact, 2015; 109: 36
[50] Deng G J, Tu S T, Zhang X C, Wang J, Zhang C C, Qian X Y, Wang Y N.Eng Fract Mech, 2016; 153: 35
[51] Hu D Y, Mao J X, Song J, Meng F C, Shan X M, Wang R Q.Mater Sci Eng, 2016; A669: 318
[52] Ding T S, Zhang X C, Tu S D, Xuan F Z.Trans Mater Heat Treat, 2016; 37(4): 69
[52] (丁天胜, 张显程, 涂善东, 轩福贞. 材料热处理学报, 2016; 37(4): 69)
[53] Wang R Z, Zhang X C, Liu F, Yao L L, Tu S T.Procedia Eng, 2015; 130: 1088
[54] Chen G, Zhang Y, Xu D K, Chen X.Mater Sci Eng, 2016; A655: 175
[55] Xiao L, Chen D L, Chaturvedi M C.Mater Sci Eng, 2008; A483: 369
[56] Xiao L, Chen D L, Chaturvedi M C.Scr Mater, 2005; 52: 603
[57] Tian S G, Li Z R, Zhao Z G, Chen L Q, Sun W R, Liu X H.Rare Met Mater Eng, 2012; 41: 1651
[57] (田素贵, 李振荣, 赵中刚, 陈礼清, 孙文儒, 刘相华. 稀有金属材料与工程, 2012; 41: 1651)
[58] Tian S G, Li Z R, Zhao Z G, Chen L Q, Sun W R, Liu X F.Mater Sci Eng, 2012; A550: 235
[59] Caliari F R, Candioto K C G, Couto A A, Nunes C ?, Reis D A P.J Mater Eng Perform, 2016; 25: 2307
[60] Kuo C M, Yang Y T, Bor H Y, Wei C N, Tai C C. Mater Sci Eng, 2009; A510-511: 289
[61] Song H W, Guo S R, Hu Z Q.Scr Mater, 1999; 41: 215
[62] Yeh A C, Lu K W, Kuo C M, Borc H Y, Wei C N.Mater Sci Eng, 2011; A530: 525
[63] Richards N L, Chaturvedi M C.Int Mater Rev, 2000; 45: 109
[64] Damodaram R, Raman S G S, Rao K P.Mater Sci Eng, 2013; A560: 781
[65] Damodaram R, Raman S G S, Rao K P.Mater Des, 2014; 53: 954
[66] Idowu O A, Ojo O A, Chaturvedi M C.Mater Sci Eng, 2007; A454: 389
[67] Manikandan S G K, Sivakumar D, Kamaraj M, Prasad K.Mater Sci Forum, 2012; 710: 614
[68] Ramkumar K D, Sridhar R, Periwal S, Oza S, Saxena V.Mater Des, 2015; 68: 158
[69] Koleva E G, Mladenov G M, Trushnikov D N, Belenkiy V Y.J Mater Process Technol, 2014; 214: 1812
[70] Khodir S, Shibayanagi T, Takahashi M, Abdel-Aleem H, Ikeuchi K, Hidad P, Arivazhagan N.Mater Des, 2014; 60: 391
[71] Mei Y P, Liu Y C, Liu C X, Li C, Yu L M, Guo Q Y, Li H J.Mater Des, 2016; 89: 964
Outlines

/