Abstract

Thermo-mechanical control process (TMCP) plays a key role in the manufacturing of hot-rolled low-alloy steels, as well as the optimization of microstructures and properties. However, the various phase transformations involved in the TMCP of steels and its impact on the microstructures/properties are still not fully understood. In the present work, on the basis of classical theories of phase transformations and previous experimental results, the key parameters controlling the phase transformation processes are analyzed, from which the correlation between thermodynamics and kinetics of the phase transformations are proposed; then, this correlation in the phase transformations of low-alloy steels and its effect on the competing mechanisms of transformations are analyzed; based on well-established theories (i.e. the first-principles calculations and the double well potential in phase field methods), the energetics of the Bain path of Na and the fcc/bcc transformation of Fe are calculated to demonstrate the correlation between thermodynamics and kinetics. Eventually, the current work is summarized and the potential applications of the correlation between thermodynamics and kinetics of phase transformations are proposed.

Cite this article

Feng LIU , Kang WANG . DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. Acta Metall Sin, 2016 , 52(10) : 1326 -1332 . DOI: 10.11900/0412.1961.2016.00341

References

[1] Herlach D M.Mater Sci Eng Rep, 1994; 12: 172
[2] Zhao J C, Notis M R.Mater Sci Eng Rep, 1995; 15: 135
[3] Willnecker R, Herlach D M, Feuerbacher B.Phys Rev Lett, 1989; 62: 2707
[4] Liu Y C, Sommer F, Mittemeijer E J.Acta Mater, 2006; 54: 3383
[5] Bhadeshia H K D H.Mater Sci Eng, 1999; A273: 58
[6] Nishiyama Z. Martensitic Transformation.New York: Academic Press, 1978: 211
[7] Xu Z Y.Phase Transformation in Materials. Beijing: Higher Education Press, 2013: 43
[7] (徐祖耀. 材料相变. 北京:高等教育出版社, 2013: 43)
[8] Hillert M. Phase Equilibria, Phase Diagrams and Phase Transformations-Their Thermodynamic Basis. Cambridge: Cambridge University Press, 1998: 80
[9] Liu F, Sommer F, Bos C, Mittemeijer E J.Int Mater Rev, 2007; 52: 193
[10] Liu F, Wang H F, Song S J, Zhang K, Yang G C, Zhou Y H.Prog Phys, 2012, 32: 1
[11] Christian J W.The Theory of Transfomation in Metals and Alloys, Part 1: Equilibrium and General Kinetics Theory. Oxford: Pergamon Press, 2002: 422, 1015
[12] Kelton F.Solid State Phys, 1991; 45: 75
[13] Weeks J D, Gilmer G H.Adv Chem Phys, 1979; 40: 157
[14] Turnbull D.J Phys Chem, 1962; 66: 609
[15] Aziz M J, Boettinger W J.Acta Metall Mater, 1994; 42: 527
[16] Eyring H.J Chem Phys, 1995; 3: 107
[17] Liu F, Sommer F, Mittemeijer E J.Acta Mater, 2004; 52: 3207
[18] Zhang J M.J Phys, 1984; F14: 769
[19] Zhao Y T, Shang C J, Yang S W, Wang X M, He X L.Mater Sci Eng, 2006; A433: 169
[20] Madariaga I, Gutiérrez I, García-de A C, Capdevila C.Scr Mater, 1999; 41: 229
[21] Zhao Y T, Shang C J, He X L, Guo H.Acta Metall Sin, 2006; 42: 54
[21] (赵运堂, 尚成嘉, 贺信莱, 郭晖. 金属学报, 2006; 42: 54)
[22] Tang W J, Zheng L, Wang Z Q, Zheng F.Baosteel Technol, 2010; (2): 45
[22] (唐文军, 郑磊, 王自强, 郑芳. 宝钢技术, 2010; (2): 45)
[23] Delaey L.In: Kostorz G ed., Phase Transformations in Materials, Weinheim: Wiley-Vch, 2001: 630
[24] Hong M, Wang K, Chen Y Z, Liu F.J Alloys Compd, 2015; 647: 763
[25] Zhao M C, Yang K, Xiao F R, Shan Y Y.Mater Sci Eng, 2003; A355: 126
[26] Smith Y E, Siebert C A.Metall Trans, 1971; 2: 1711
[27] Wang Z D, Qu J B, Liu X H, Wang G D.Acta Metall Sin, 1998; 11: 121
[27] (王昭东, 曲锦波, 刘相华, 王国栋. 金属学报, 1998; 11: 121)
[28] Weng Y Q.Ultra-Fine Grained Steels. Beijing: Metallurgical Industry Press, and Berlin: Springer-Verlag GmbH, 2009: 86
[29] Matsumura Y, Yada H.Trans ISIJ, 1987; 27: 492
[30] Yada H, Li C M, Yamagata H.ISIJ Int, 2000; 40: 200
[31] Yu W, Chen Y L, Chen Y L, Liao D J.J Univ Sci Technol Beijing, 2002; 24: 643
[31] (余伟, 陈银莉, 陈雨来, 廖东骏. 北京科技大学学报, 2002; 24: 643)
[32] Wang X D, Huang B X, Wang L, Rong Y H.Metall Mater Trans, 2008; 39A: 1
[33] Kelly M J.J Phys, 1979; 9F: 1921
[34] Henkelman G, Uberuaga B P, Jónsson H.J Chem Phys, 2000; 113: 9901
[35] Okatov S V, Kuznetsov A R, Gornostyrev Y N, Urtsev V N, Katsnelson M I.Phys Rev, 2009; 79B: 094111
[36] Kresse G, Furthmuller J.Phys Rev, 1996; 54B: 11169
[37] Methfessel M, Paxton A T.Phys Rev, 1989; 40B: 3616
[38] Perdew J P, Burke K, Ernzerhof M.Phys Rev Lett, 1996; 77: 3865
[39] Boettinger W J, Warren J A, Beckermann C, Karma A.Annu Rev Mater Res, 2002; 32: 163
[40] Peter G B, Christoph D, Chandler D.PNAS, 2000; 97: 5877
[41] Radhakrishnan R, Trout B L.In: Yip S ed., Handbook of Materials Modeling, Netherlands: Springer, 2005: 1613
[42] Heo T W, Chen L Q.Acta Mater, 2014; 76: 68
[43] Dinsdale A T.Calphad, 1991; 15: 317
Outlines

/