COMPOSITION DESIGN AND OPTIMIZATION OF Fe-B-Si-Nb BULK AMORPHOUS ALLOYS
Received date: 2016-01-20
Online published: 2016-08-19
Supported by
Supported by National Natural Science Foundation of China (No.51131002), Fundamental Research Funds for the Central Universities (Nos.DUT16ZD209 and DUT13ZD102), Scientific and Technological Development Foundation of China Academy of Engineering Physics (No.2013A03010115), National Magnetic Confinement Fusion Science Program (No.2013GB107003) and the Fund of the State Key Laboratory of Solidification Processing in NWPU (No.SKLSP201607)
Fe-based amorphous alloys are well known for their good magnetic properties including ultrahigh saturation magnetization, low coercive force, high magnetic permeability and low core loss. But these alloys were only prepared into ribbon form in early times due to their insufficient glass-forming abilities (GFAs). The present work focuses on the design of Fe-B-Si-Nb bulk metallic glasses with good soft magnetic properties and high glass-forming ability. Glass formation in Fe-B system is first considered with cluster-plus-glue-atom model. A basic composition formula [B-B2Fe8]Fe is proposed as the framework for multi-component alloy design. Considering the structural stability of the model glass, Si and Nb are introduced to the [B-B2Fe8] cluster to replace the center B and shell Fe atoms, from which a series of Fe-B-Si-Nb alloys with composition formulas [Si-B2Fe8-xNbx]Fe (x=0.1~1.2) are derived. Copper mold casting experiments revealed that bulk glass alloys with a critical diameter (dc) exceeding 1.0 mm are readily obtained with the Nb content range of x=0.2~1.2, the largest dc (about 2.5 mm) appears in the vicinity of x=0.4~0.5. Considering the local packing efficiency of Fe-B-Si-Nb glass model structure, another series alloy compositions, namely, [(Si1-yBy)-B2Fe8-xNbx]Fe is reached by increasing Nb and decreasing Si simultaneously in [Si-B2Fe7.6Nb0.4]Fe basal glass alloys. The experimental results show that bulk glass alloys with dc=2.5 mm are available over a wide range of compositions from (x=0.5, y=0.05) to (x=0.9, y=0.25). Excellent magnetic softness with high saturation magnetizations (Bs=1.14~1.46 T) and low coercive forces (Hc=1.6~6.7 A/m) is found in the [Si-B2Fe8-xNbx]Fe (x=0.2~0.6) series glass alloys. A high fracture strength of 4220 MPa with a plasticity of 0.5% is observed in the [(Si0.95B0.05)-B2Fe7.5Nb0.5]Fe bulk glass alloy.
Key words: cluster-plus-glue-atom; model,; Fe-B-Si-Nb; bulk; glass; alloy,; mechanical; property,; soft; magnetic; property
Yaoxiang GENG , Yingmin WANG , Jianbing QIANG , Chuang DONG , Haibin WANG , Ojied TEGUS . COMPOSITION DESIGN AND OPTIMIZATION OF Fe-B-Si-Nb BULK AMORPHOUS ALLOYS[J]. Acta Metall Sin, 2016 , 52(11) : 1459 -1466 . DOI: 10.11900/0412.1961.2016.00033
| [1] | Inoue A, Shinohara Y, Gook J S.Mater Trans JIM, 1995; 36: 1427 |
| [2] | Suryanarayana C, Inoue A.Int Mater Rev, 2013; 58: 131 |
| [3] | Inoue A.Acta Mater, 2000; 48: 279 |
| [4] | Davies H A, Lewis B G.Scr Metall, 1975; 9: 1107 |
| [5] | Shen B L, Chang C T, Inoue A.Intermetallics, 2007; 15: 9 |
| [6] | Wang W H.Prog Mater Sci, 2007; 52: 540 |
| [7] | Lu Z P, Liu C T.J Mater Sci, 2004; 39: 3965 |
| [8] | Shen B L, Inoue A, Chang C T.Appl Phys Lett, 2004; 85: 4911 |
| [9] | Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H.J Phys, 2007; 40D: R273 |
| [10] | Miracle D B.Nat Mater, 2004; 3: 697 |
| [11] | Han G, Qiang J B, Li F W, Yuan L, Quan S G, Wang Q, Wang Y M, Dong C, H?ussler P.Acta Mater, 2011; 59: 5917 |
| [12] | Luo L J, Chen H, Wang Y M, Qiang J B, Wang Q, Dong C, H?ussler P.Philos Mag, 2014; 94: 2520 |
| [13] | Wu J, Wang Q, Qiang J B, Chen F, Dong C, Wang Y M, Shek C H.J Mater Res, 2007; 22: 573 |
| [14] | Xia J H, Qiang J B, Wang Y M, Wang Q, Dong C. Appl Phys Lett, 2006; 88: 101907 |
| [15] | Wang Y M, Wang Q, Zhao J J, Dong C.Scr Mater, 2010; 63: 178 |
| [16] | Yuan L, Pang C, Wang Y M, Wang Q, Dong C.Intermetallics, 2010; 18: 1800 |
| [17] | Gaskell P H.In: Beck H, Güntherodt H J eds., Models for the Structure of Amorphous Metals. Belin, Heidelberg, New York, Tokyo: Springer-Verlag, 1983: 5 |
| [18] | Inoue A, Shen B L.Mater Trans, 2002; 43: 766 |
| [19] | Amiya K, Urata A, Nishiyama N, Inoue A.Mater Trans, 2004; 45: 1214 |
| [20] | Shen B L, Inoue A, Chang C T.Appl Phys Lett, 2004; 85: 4911 |
| [21] | Shen B L, Inoue A.J Mater Res, 2005; 20: 1 |
| [22] | Geng Y X, Han K M, Wang Y M, Qiang J B, Wang Q, Dong C, Zhang G F, Tegus O, H?ussler P.Acta Metall Sin, 2015; 51: 1017 |
| [22] | (耿遥祥, 韩凯明, 王英敏, 羌建兵, 王清, 董闯, 张贵锋, 特古斯, H?ussler P. 金属学报, 2015; 51: 1017) |
| [23] | Geng Y X, Wang Y M, Qiang J B, Zhang G F, Dong C, Tegus O, Sun J Z.Intermetallics, 2015; 67: 138 |
| [24] | Geng Y X, Wang Y M, Wang Z Y, Wang H B, Qiang J B, Dong C, Tegus O.Mater Des, 2016; 106: 67 |
| [25] | Geng Y X, Wang Y M, Qiang J B, Zhang G F, Dong C, H?ussler P.J Non-Cryst Solids, 2016; 432: 453 |
| [26] | Takeuchi A, Inoue A.Mater Trans, 2005; 46: 2817 |
| [27] | Inoue A, Shen B L, Chang C T.Acta Mater, 2004; 52: 4093 |
| [28] | Inoue A, Shen B L, Chang C T.Intermetallics, 2006; 14: 936 |
| [29] | Park J M, Park J S, Na J H, Kim D H, Kim D H. Mater Sci Eng#/magtechI#, 2006; A435-436: 425 |
| [30] | Chen H S.Rep Prog Phys, 1980; 43: 353 |
| [31] | Li F S, Shen B L, Makino A, Inoue A.Appl Phys Lett, 2007; 91: 234101 |
| [32] | Ling H B, Li Q, Li H X, Zhang J J, Dong Y Q, Chang C T, Seonghoon Y. J Appl Phys, 2014; 115: 204901 |
/
| 〈 |
|
〉 |