EFFECT OF BOBBIN TOOL FRICTION STIR WELDING ON MICROSTRUCTURE AND CORROSION BEHAVIOR OF 6061-T6 ALUMINUM ALLOY JOINT IN 3.5%NaCl SOLUTION
Received date: 2016-01-13
Online published: 2016-08-18
Supported by
Supported by National Natural Science Foundation of China (Nos.51401092, 51575252 and 51205175)
Friction stir welding (FSW) is a new solid-state joining method which offers several advantages compared with conventional welding methods, including better mechanical properties, lower residual stress and reduced occurrence of defects. It has already been used for joining Al alloys in the aerospace and automotive industries. In spite of the advantages, FSW also has drawbacks, such as the risk of root flaws in single-side welds. Using a bobbin tool instead is a promising way to solve this problem since the root region is avoided. Compared with standard (single-side) FSW techniques, the bobbin tool FSW has an extra shoulder attached to the tip of the probe, namely the lower shoulder. This setup makes BTFSW capable of joining closed profiles like hollow extrusions. Furthermore, root flaws, such as lack of penetration, which occasionally occurred in standard FSWtechiques, can be completely avoided. In this work, 6061-T6 aluminum alloy was welded by using bobbin tool friction stir weld (BTFSW). The influence of BTFSW on the microstructure development and hardness distribution in the weldment has been investigated. The corrosion behaviors of the base metal and weld nugget in 3.5%NaCl (mass fraction) solution were investigated using SEM, XRD and electrochemical measurements. The results showed that the weld surface of 6061-T6 welded by BTFSW is of good quality. No welding defect was detected in the joints. Three microstructural zones, i.e., nugget zone, thermo-mechanically affected zone, and heat affected zone were discernible. The microstructural analysis indicates that the weld nugget region exhibited fine and equiaxed grain structure with an average grain size of ~8 μm, indicating the occurrence of dynamic recrystallization due to severe plastic deformation and thermal exposure. The thermo-mechanically affected zone underwent plastic deformation and recrystallization occured in this zone due to deformation strain and thermal input. The low hardness zone, determined by constructing the hardness distribution profile on cross-section of joint, located at thermo-mechanically affected zone of advancing side. Although 6061-T6 alloys are readily weldable, they suffered from severe softening in the heat affected zone because of the dissolution of Mg2Si precipitates during the weld thermal cycle. BTFSW can improve the corrosion resistance of 6061-T6 aluminum alloy in 3.5%NaCl solution. The corrosion behavior results showed that both anodic dissolution and pitting were observed after the immersion test due to the inhomogeneous microstructure of 6061-T6 aluminum alloy. The corrosion products mainly composed of Al(OH)3 and Al2O3. Furthermore, the corrosion process and mechanism were also discussed.
Key words: corrosion,; aluminum; alloy,; bobbin; tool; friction; stir; welding,; microstructure
Yanxin QIAO , Yang ZHOU , Shujin CHEN , Qining SONG . EFFECT OF BOBBIN TOOL FRICTION STIR WELDING ON MICROSTRUCTURE AND CORROSION BEHAVIOR OF 6061-T6 ALUMINUM ALLOY JOINT IN 3.5%NaCl SOLUTION[J]. Acta Metall Sin, 2016 , 52(11) : 1395 -1402 . DOI: 10.11900/0412.1961.2016.00026
| [1] | Marzoli L M, Strombeck A V, Santos J F D, Gambaro C, Volpone L M.Compos Sci Technol, 2006; 66: 363 |
| [2] | Hong S J, Kim S S, Lee C G, Kim S J.Scr Mater, 2006; 55: 1007 |
| [3] | Zhao Y, Fu J, Zhang P L, Yan K, Jiang C Y.J Jiangsu Univ Sci Technol (Nat Sci Ed), 2006; 20(1): 90 |
| [3] | (赵勇, 付娟, 张培磊, 严铿, 蒋成禹. 江苏科技大学学报(自然科学版), 2006; 20(1): 90) |
| [4] | Tong J H, Li L, Deng D, Wan F R.J Univ Sci Technol Beijing, 2008; 30: 1011 |
| [4] | (佟建华, 李炼, 邓冬, 万发荣. 北京科技大学学报, 2008; 30: 1011) |
| [5] | Wang D, Wang Q Z, Xiao B L, Ni D R, Ma Z Y.Acta Metall Sin, 2014; 50: 489 |
| [5] | (王东, 王全兆, 肖伯律, 倪丁瑞, 马宗义. 金属学报, 2014; 50: 489) |
| [6] | Liu F J, Fu L, Zhang W Y, Meng Q, Dong C L, Luan G H.Acta Metall Sin, 2015; 51: 281 |
| [6] | (刘奋军, 傅莉, 张纹源, 孟强, 董春林, 栾国红. 金属学报, 2015; 51: 281) |
| [7] | Somasekharan A C, Murr L E.Mater Charact, 2004; 53: 19 |
| [8] | Xu W F, Liu J H, Chen D L.Acta Metall Sin, 2015; 51: 587 |
| [8] | (徐韦锋, 刘金合, CHEN Daolun. 金属学报, 2015; 51: 587) |
| [9] | Ren S R, Ma Z Y, Chen L Q, Zhang Y Z.Acta Metall Sin, 2007; 43: 225 |
| [9] | (任淑荣, 马宗义, 陈礼清, 张玉政. 金属学报, 2007; 43: 225) |
| [10] | Yan D Y, Shi Q Y, Wu A P, Juergen S, Liu Y, Zhang Z L.Acta Metall Sin, 2009; 45: 183 |
| [10] | (鄢东洋, 史清宇, 吴爱萍, Juergen Silvanus, 刘园, 张增磊. 金属学报, 2009; 45: 183) |
| [11] | Xu W F, Liu J H, Luan G H, Dong C L.Acta Metall Sin, 2009; 45: 490 |
| [11] | (徐韦锋, 刘金合, 栾国红, 董春林. 金属学报, 2009; 45: 490) |
| [12] | Liu H J, Fujii H, Maeda M, Nogi K.J Mater Sci Lett, 2003; 22: 1061 |
| [13] | Hilgert J, Schmidt H N B, dos Santos J F, Huber N.J Mater Process Technol, 2011; 211: 197 |
| [14] | Sued M K, Pons D, Lavroff J, Wong E H.D.Mater Des, 2014; 54: 632 |
| [15] | Paglia C S, Buchheit R G.Scr Mater, 2008; 58: 383 |
| [16] | Lafly A-L, Allehaux D, Marie F, Donne C D, Doker H.J Int Inst Weld, 2005; 49: 444 |
| [17] | Chen Y C, Nakata K.Mater Des, 2009; 30: 469 |
| [18] | Kumbhar N T, Sahoo S K, Samajdar I, Dey G K,Mater Des, 2011; 32: 1657 |
| [19] | Thomas W M, Wiesner C S, Marks D J, Staines D G.Sci Technol Weld Joining, 2009; 14: 247 |
| [20] | Corral J, Trillo E A, Li Y, Murr L E.J Mater Sci Lett, 2002; 19: 2117 |
| [21] | Gharavi F, Matoria K, Yunus R, Othman N, Fadaeifard F.J Mater Res Technol, 2015; 4: 314 |
| [22] | Emilie B, Angéline P Q, Monique P, Olivier D, Marie T.Corros Sci, 2011; 53: 3026 |
| [23] | Kang J, Fu R D, Luan G H, Dong C L, He M.Corros Sci, 2010; 52: 620 |
| [24] | Gupta R K, Das H, Pal T K.J Mater Eng Perform, 2012; 21: 1645 |
| [25] | Feng A H, Chen D L, Ma Z Y.Metall Mater Trans, 2010; 41A: 2626 |
| [26] | Yutaka S S, Mitsunori U, Hiroyuki Ka, Keisuke I.Mater Sci Eng, 2003; A354: 298 |
| [27] | Elangovan K, Balasubramanian V.Mater Des, 2008; 29: 362 |
| [28] | Liu F C, Ma Z Y.Metall Mater Trans, 2008; 39A: 2378 |
| [29] | Rajesh K G, Hrishikesh D, Tapan K P.J Mater Eng Perform, 2012; 21: 1645 |
| [30] | Zhou K, Wang B, Zhao Y, Liu J.Trans Nonferrous Met Soc China, 2015; 25: 2509 |
| [31] | Wang X H, Wang J H, Fu C W.Trans Nonferrous Met Soc China, 2014; 24: 3907 |
| [32] | Singh A K, Quraishi M A.Corros Sci, 2010; 52: 152 |
| [33] | Pardo A, Merino M C, Coy A E, Viejo F, Jr Arrabal R S F.Electrochim Acta, 2008; 53: 7890 |
| [34] | He J G, Wen J B, Li X D.Corros Sci, 2011; 53: 1948 |
| [35] | Ghods P, Isgor O B, McRae G A, Li J, Gu G P.Corros Sci, 2011; 53: 946 |
| [36] | Chen J, Wang J Q, Han E-H, Dong J H, Ke W.Electrochim Acta, 2007; 52: 3299 |
| [37] | Tan L, Allen T R.Corros Sci, 2010; 52: 548 |
| [38] | Yasakau K A.Electrochim Acta, 2007; 52: 7651 |
| [39] | Zhang J, Zhang T, Shao Y W, Meng G Z, Wang F H.Corros Sci Prot Technol, 2014; 26: 125 |
| [39] | (张晋, 张涛, 邵亚薇, 孟国哲, 王福会. 腐蚀科学与防护技术, 2014; 26: 125) |
| [40] | Sun F L, Li X G, Lu L, Cheng X Q, Dong C F, Gao J.Acta Metall Sin, 2013; 49: 1219 |
| [40] | (孙飞龙, 李晓刚, 卢琳, 程学群, 董超芳, 高瑾. 金属学报, 2013; 49: 1219) |
| [41] | Seetharaman R, Ravisankar V, Balasubramanian V.Trans Nonferrous Met Soc China, 2015; 25: 1427 |
| [42] | Voskov A L, Voronin G F.Russ J Phys Chem, 2010; 80A: 6105 |
| [43] | Nady H, Helal N H, El-Rabiee M M, Badawy W A.Mater Chem Phys, 2012; 134: 945 |
/
| 〈 |
|
〉 |