Orginal Article

AGE-HARDENING RESPONSE FOR Mg96.17Zn3.15Y0.5Zr0.18 SOLID SOLUTION ALLOY UNDER HIGH PRESSURE

  • Zhibin FAN ,
  • Xiaoping LIN ,
  • Yun DONG ,
  • Jie YE ,
  • Chan LI ,
  • Bo LI
Expand
  • School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China

Received date: 2016-03-24

  Online published: 2016-06-23

Supported by

Supported by National Natural Science Foundation of China (Nos.51675092 and 51475486) and Natural Science Foundation of Hebei Province (No.E2014501123)

Abstract

Rare-earth (RE) element addition can remarkably improve the mechanical properties of magnesium alloys through solid solution and age-hardening. Increasing the solubility in the Mg matrix and enhancing the precipitation density are effective measures to improve ageing strengthening of magnesium alloys. In this work, solid solution treatment at 600~800 ℃ under 4 GPa, and then isothermal ageing at 200 ℃ for Mg96.17Zn3.15Y0.5Zr0.18 alloy was carried out. The microstructures of the high pressure solution treatment Mg96.17Zn3.15Y0.5Zr0.18 alloy before and after ageing were investigated by TEM, HRTEM, SEM and XRD, and age-hardening curves of Mg96.17Zn3.15Y0.5Zr0.18 alloy after solution treatment under the high pressure of 4 GPa have been tested. The results show that, as the rise of the solution treatment temperature, I-Mg3Zn6Y and W-Mg3Zn3Y2 continually dissolved into the Mg matrix, and the solubility of Zn in the Mg matrix drastically improved after solution treatment under the high pressure of 4 GPa. The solubility of Zn in the Mg matrix reached up to 6.60% (mass fraction) after solution treatment at 700~800 ℃ under the high pressure of 4 GPa than 2.11% after solution treatment at 400 ℃ under the atmosphere, and the supersaturated solid solution α-Mg has been attained. After ageing treatment at 200 ℃, the peak hardness of Mg96.17Zn3.15Y0.5Zr0.18 alloy after solution treatment under the high pressure of 4 GPa could been reached in short ageing time, the peak hardness of the Mg96.17Zn3.15Y0.5Zr0.18 alloy after solution treatment at 800 ℃ under 4 GPa was 105 HV, which was increased by 30% than 81 HV of the alloy after solution treatment at 400 ℃ under the atmosphere. HRTEM analysis results indicated that the high precipitation density was found in the Mg96.17Zn3.15Y0.5Zr0.18 alloy after solution treatment under the high pressure of 4 GPa, and some of precipitation were particle quasicrystal I-Mg3Zn6Y phases.

Cite this article

Zhibin FAN , Xiaoping LIN , Yun DONG , Jie YE , Chan LI , Bo LI . AGE-HARDENING RESPONSE FOR Mg96.17Zn3.15Y0.5Zr0.18 SOLID SOLUTION ALLOY UNDER HIGH PRESSURE[J]. Acta Metall Sin, 2016 , 52(12) : 1491 -1496 . DOI: 10.11900/0412.1961.2016.00098

References

[1] Ding W J.Science and Technology of Magnesium Alloys. Beijing: Science Press, 2007: 98
[1] (丁文江. 镁合金科学与技术. 北京: 科学出版社, 2007: 98)
[2] Song W X.Metallography. Beijing: Metallurgical Industry Press, 1989: 60
[2] (宋维锡. 金属学. 北京:冶金工业出版社, 1989: 60)
[3] Liang Y, Huang X F, Wang T, Cao X J, Zhu K.China Foundry Machine Technol, 2009; (1): 8
[3] (梁艳, 黄晓锋, 王韬, 曹喜娟, 朱凯. 中国铸造装备与技术, 2009; (1): 8)
[4] Gao X, Nie J F.Scr Mater, 2007; 56: 645
[5] Buha J.Mater Sci Eng, 2008; A492: 11
[6] Clark J B.Aata Metall, 1965; 13: 1281
[7] Sturkey L, Clark J B.Inst Met, 1959; 88: 177
[8] Chen J Q, Liu J W.Mater Rev, 2008; 22: 342
[8] (陈敬区, 刘江文. 材料导报, 2008; 22: 342)
[9] Wang X L, Li C R, Guo C P, Du Z M, He W.Acta Metall Sin, 2010; 46: 575
[9] (王晓亮, 李长荣, 郭翠萍, 杜振民, 何维. 金属学报, 2010; 46: 575)
[10] Dong Y, Lin X P, Ye J, Zhao T B, Fan Z B.Mater Sci Eng, 2015; A636: 600
[11] Buha J.Mater Sci Eng, 2008; A491: 70
[12] Chen J G, Sun Y, Zhang J S, Cheng W L, Niu X F, Xu C X.J Magn Alloy, 2015; 3: 121
[13] Li X M, Starink M J.J Alloys Compd, 2011; 509: 471
[14] Jiang T J, Xiao W Q, Yang L, Shao W Z, Yuan S J, Zhen L.Mater Sci Eng, 2014; A605: 167
[15] Shi G L, Zhang D F, Zhang H J, Zhao X B, Qi F G, Zhang K.Trans Nonferrous Met Soc China, 2013; 23: 586
[16] Zhao J, Li J M, Zhao L M, Yin S, Chen J C, Wen Q X.Rare Met, 2015; 39: 97
[16] (赵军, 李冀蒙, 赵陆民, 尹硕, 陈久川, 文全兴. 稀有金属, 2015; 39: 97)
[17] Wang H Y, Lu W, Liu J H.Chin J High Pressure Phys, 2010; 24: 300
[17] (王海燕, 陆伟, 刘建华. 高压物理学报, 2010; 24: 300)
[18] Zhao S S, Peng Q P, Li H, Liu B Z.J Alloys Compd, 2014; 584: 56
[19] Jie J C, Zou C M, Wang H W, Li B, Wei Z J.J Alloys Compd, 2012; 510: 11
[20] Zhang G Z, Yu X F, Zhang Y J, Jia G L.J Mater Metall, 2006; 5(1): 61
[20] (张国志, 于溪凤, 张雅静, 贾光霖. 材料与冶金学报, 2006; 5(1): 61)
[21] Luo Z P, Zhang S Q, Tang Y L, Zhao D S.Scr Mater, 1993; 28: 1513
[22] Kim I J, Bae D H, Kim D H.Mater Sci Eng, 2003; A359: 313
[23] Zhang S J, Bian X F, Jing Y G, Li Z K, Wang C D.Spec Cast Nonferrous Alloys, 2007; 27: 698
[23] (张士佼, 边秀房, 景元高, 李贞宽, 王才东. 特种铸造及有色合金, 2007; 27: 698)
[24] Lin X P, Dong Y, Xu R, Sun G F, Jiao S H.Acta Metall Sin, 2011; 47: 1550
[24] (林小娉, 董允, 徐瑞, 孙桂芳, 焦世辉. 金属学报, 2011; 47: 1550)
[25] Lin X P, Dong Y, Xu R, Zheng R G, Jiao S H.Rare Met Mater Eng, 2013; 42: 2309
[25] (林小娉, 董允, 徐瑞, 郑润国, 焦世辉. 稀有金属材料与工程, 2013; 42: 2309 )
[26] Батншeв А И, translated by Zhang J S. Crystallization of Metal and Alloys Under Pressure. Harbin: Harbin University of Techonology Press, 1987: 23
[26] (Батншeв А И 著, 张锦升译. 金属和合金在压力下结晶. 哈尔滨: 哈尔滨工业大学出版社, 1987: 23)
[27] Jie J C, Zou C M, Wang H W, Wei Z J.Acta Metall Sin, 2014; 50: 971
[27] (接金川, 邹鹑鸣, 王宏伟, 魏尊杰. 金属学报, 2014; 50: 971)
Outlines

/