Orginal Article

A COLUMNAR & NON-GLOBULAR EQUIAXED MIXED THREE-PHASE MODEL BASED ON THERMOSOLUTAL CONVECTION AND GRAIN MOVEMENT

  • Jun LI ,
  • Honghao GE ,
  • Menghuai WU ,
  • Andreas LUDWIG ,
  • Jianguo LI
Expand
  • 1 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
    2 Simulation and Modeling of Metallurgical Processes, University of Leoben, A-8700, Austria
    3 Christian-Doppler Lab for Advanced Process Simulation of Solidification and Melting, University of Leoben, A-8700, Austria

Received date: 2015-12-07

  Online published: 2016-06-22

Supported by

Support by Christian-Doppler Lab for Advanced Process Simulation of Solidification and Melting (Austria), National Natural Science Foundation of China (No.51404152), National Basic Research Program of China (No.2011CB012900), Shanghai Pujiang Program (No.14PJ1404800) and Shanghai International Cooperation Project (No.14140711-000)

Abstract

The prediction of the macrosegregation in large ingot is a challenging issue due to the size of the ingots and the variety of the phenomena to be accounted for, such as thermal-solutal convection of the liquid, equiaxed grain motion, evolution of grain morphology by suitably considering a coupled grain growth model in the macroscopic solidification model, the columnar-to-equiaxed transition (CET), and shrinkage, etc.. Each of these phenomena is very important to the solidification pattern, while it is impossible for one model to consider all the phenomena together until now due to the computation power limited. Thus, the model capability and computational cost should be counterpoised for the simulation of large ingot. In this work, a mixed three-phase (simplified dendritic-equiaxed, columnar and liquid) solidification model is described based on Eulerian-Eulerian approach and volume average method. The model considers the thermosolutal buoyancy flow, the movement of equiaxed crystal, and the capture of the equiaxed crystals by growing columnar tree trunks. The mechanical interaction and impingement between columnar and equiaxed crystals are considered which give the capability to predict CET. In order to enhance the model capability without increasing the computational cost significantly, a simplified method is proposed to consider the dendritic of equiaxed crystal. This model is employed to simulate the formation process of macrosegregation for two different steel ingots (3.25 and 25 t). The general macrosegregation pattern predicted by this model includes the cone of negative segregation in the bottom of ingot, quasi-A-segregation in the columnar zone, and positive segregation in the top region, which are quite similar to the classic knowledge. The CET zones are also predicted. Although there is still some quantitative discrepancy, the macrosegregation distribution predicted by this model is quite similar to the experimental measurements. The non-globular equiaxed three-phase mixed model results are compared with the globular-equiaxed mixed three-phase model ones, which indicated that for large ingots the equiaxed dendritic structure plays an important role in liquid flow and it affects final characteristic of macrosegregation. It is predicted successfully that a negative segregation zone would be formed in the upper region due to the formation of a local mini-ingot and the subsequent sedimentation and piling up of equiaxed grains within the mini-ingot.

Cite this article

Jun LI , Honghao GE , Menghuai WU , Andreas LUDWIG , Jianguo LI . A COLUMNAR & NON-GLOBULAR EQUIAXED MIXED THREE-PHASE MODEL BASED ON THERMOSOLUTAL CONVECTION AND GRAIN MOVEMENT[J]. Acta Metall Sin, 2016 , 52(9) : 1096 -1104 . DOI: 10.11900/0412.1961.2015.00627

References

[1] Ludwig A, Wu M, Kharicha A.Metall Mater Trans, 2015; 46A: 4856
[2] Pickering E J. ISIJ, 2013; 53: 935
[3] Du Q, Li D Z, Li Y Y.Acta Metall Sin, 2000; 36: 1197
[3] (杜强, 李殿中, 李依依. 金属学报, 2000; 36: 1197)
[4] Han Z Q, Liu B C.Acta Metall Sin, 2003; 39: 140
[4] (韩志强, 柳百成. 金属学报, 2003; 39: 140)
[5] Cao H F, Shen H F, Liu B C.Acta Metall Sin, 2005; 41: 917
[5] (曹海峰, 沈厚发, 柳百成. 金属学报, 2005; 41: 917)
[6] Wang T M, Yao S, Zhang X G, Jin J Z, Wu M, Ludwig A, Pustal B, Polaczek A.Acta Metall Sin, 2006; 42: 584
[6] (王同敏, 姚山, 张兴国, 金俊泽, Wu M, Ludwig A, Pustal B, Polaczek A. 金属学报, 2006; 42: 584)
[7] Flemings M C, Nereo G E.Trans Met Soc AIME, 1967; 239: 1449
[8] Dantzig J A, Rappaz M. Solidification. Switzerland, EPFL Press, 2009: 568
[9] Li X, Noeppel A, Saadi B, Budenkova O, Zaidat K, Ciobanas A, Ren Z, Fautrelle Y.Trans Indian Ins Met, 2009; 62: 465
[10] Li J, Wu M, Hao J, Ludwig A.Comp Mater Sci, 2012; 55: 407
[11] Li J, Wu M, Hao J, Ludwig A.Comp Mater Sci, 2012; 55: 419
[12] Mehrabian R, Keane M, Flemings M C.Metall Trans, 1970; 1: 1209
[13] Flemings M C.Scand J Metall, 1976; 5: 1
[14] Olsson A, West R, Fredriksson H.Scand J Metall, 1986; 15: 104
[15] Schneider M, Beckermann C.Metall Mater Trans, 1995; 26A: 2373
[16] Liu D R, Li D Z, Sang B G.J Mater Sci Technol, 2009; 25: 561
[17] Liu D R, Kang X H, Fu P, Li D Z.Kovove Mater, 2011; 49: 143
[18] Liu D R, Kang X H, Sang B G, Li D Z.Acta Metall Sin (Engl Lett), 2011; 24: 54
[19] Liu D R, Sang B G, Kang X H, Li D Z.Int J Cast Met Res, 2010; 23: 354
[20] Li W S, Shen H F, Liu B C.Steel Res Int, 2010; 81: 994
[21] Tu W T, Shen H F, Liu B C.ISIJ, 2014; 54: 351
[22] Combeau H, Zaloznik M, Hans S, Richy P.Metall Mater Trans, 2009; 40B: 289
[23] Ge H H, Li J, Han X J, Xia M X, Li J G.J Mater Process Technol. 2016; 227: 308
[24] Wu M, Ludwig A.Metall Mater Trans, 2006; 37A: 1613
[25] Wu M, Ludwig A.Metall Mater Trans, 2007; 38A: 1465
[26] Li J, Wu M, Ludwig A, Kharicha A.IOP Conference Series: Mater Sci Eng, 2012; 33: 012091
[27] Li J, Wu M, Ludwig A, Kharicha A.Int J Heat Mass Transfer, 2014; 72: 668
[28] Wu M, Fjeld A, Ludwig A.Comp Mater Sci, 2010; 50: 32
[29] Rappaz M. Int Mater Rev, 1989; 34: 93
[30] Wu M, K?n?zsy L, Ludwig A, Schützenh?fer W, Tanzer R.Steel Res Int, 2008; 79: 637
[31] Wu M, Li J, Ludwig A, Kharicha A.Comp Mater Sci, 2013; 79: 830
[32] Wu M, Ludwig A.Acta Mater, 2009; 57: 5621
[33] Ahmadein M, Wu M, Ludwig A.J Cryst Growth, 2015; 417: 65
[34] Li J, Wu M, Ludwig A, Kharicha A, Schumacher P. Mater Sci Forum, 2014; 790-791: 121
[35] Wang C Y, Ahuja S, Beckermann C, de Groh H C.Metall Mater Trans, 1995; 26B: 111
[36] Heterogeneity Sub-Committee of the British Iron and Steel Institute.J Iron Steel Inst London, 1926; 113: 39
[37] Wu M, Li J, Ludwig A, Kharicha A.Comp Mater Sci, 2014; 92: 267
Outlines

/