MICROSTRUCTURES AND PROPERTIES OF Ni-BASEDWEAR RESISTANT LAYERS REINFORCED BYTiC GENERATED FROM IN SITU PLASMASPRAY WELDING
Received date: 2016-03-11
Online published: 2016-06-21
Supported by
Supported by Science and Technology Department of Jilin Province (No.20100328)
Generally, wear is one of the main failure mechanisms for mold steel. The heavy financial loss will often occur if molds are out of service due to their hard manufacturing process and high cost of metal materials. Therefore, mold repairing is urgent and critical if they fail to function. Ni-matrix wear resistant composited layers reinforced by TiC generated from in situ plasma spray welding NiCrBSi+Ti powders were prepared. The analysis instruments of OM, SEM, XRD and EDS were used to study the microstructural characterization, phase identification and chemical compositions of the layers. And the microhardness and wear resistance were tested using Vickers hardness tester and abrasion tester, respectively. The investigations demonstrated that the layers were mainly composed of basic phases (γ-Ni+β1-Ni3Si) with eutectic features and hypereutectoid (α-Fe+FeNi3) structures, in which hard phases M7C3 and M23C6 were embedded in the matrix. The phase CrB was distributed uniformly in the layers. One part of TiC generated from in situ reaction acted as the nucleation of the chromium compounds precipitates M7C3 and M23C6. The other part of TiC was also distributed in the base with the fine particles (<1 μm) and even bigger size (>1 μm). Ti percentage rising, the microstructures of plasma spray welding layers were refined and the phase M23C6 increased while M7C3 decreased. When the Ti addition reached 6%, the layers had better performance with microhardness of 800 HV0.5. The wear mass loss of layers was 14.5 mg, which were more than 2 times of NiCrBSi layer.
Key words: TiC,; plasma; spray; welding,; in; situ; generation,; microstructure; and; property
Hongyong XU , Wenquan WANG , Shiming HUANG , Xiangxia CHENG , Meixuan REN . MICROSTRUCTURES AND PROPERTIES OF Ni-BASEDWEAR RESISTANT LAYERS REINFORCED BYTiC GENERATED FROM IN SITU PLASMASPRAY WELDING[J]. Acta Metall Sin, 2016 , 52(11) : 1423 -1431 . DOI: 10.11900/0412.1961.2016.00084
| [1] | Kulkarni K, Srivastava A, Shivpuri R, Bhattacharya R, Dixit S, Bhat D.Surf Coat Technol, 2002; 149: 171 |
| [2] | Srivastava A, Joshi V, Shivpuri R.Wear, 2004; 256: 38 |
| [3] | Jacobsen S D, Hinrichs R, Baumvol I J R, Castellano G, Vasconcellos M A Z.Surf Coat Technol, 2015; 270: 266 |
| [4] | Lei Y W, Sun R L, Tang Y, Niu W.Opt Laser Eng, 2015; 66: 181 |
| [5] | Wang D, Li H, Yang H, Ma J, Li G.Chin J Aeronaut, 2014; 27: 1002 |
| [6] | Telasang G, Majumdar J D, Padmanabham G, Manna I.Surf Coat Technol, 2015; 261: 69 |
| [7] | Hou Q Y, Gao J S, Zhou F.Surf Coat Technol, 2005; 194: 238 |
| [8] | Cho T Y, Yoon J H, Cho J Y, Joo Y K, Kang J H, Zhang S H, Chun H G, Hwang S Y, Kwon S C.Surf Coat Technol, 2009; 203: 3250 |
| [9] | Xu H Y, Wang W Q, Huang S M, Fang L Q.Trans Mater Heat Treat, 2015; 36: 221 |
| [9] | (徐红勇, 王文权, 黄诗铭, 方丽琴. 材料热处理学报, 2015; 36: 221) |
| [10] | Ingo G M, Kaciulis S, Mezzi A, Valente T, Casadei F, Gusmano G. Electrochim Acta, 2005; 50: 4531 |
| [11] | Xiao L S, Yan D R, He J N, Lin Z, Dong Y C, Zhang J X, Li X Z.Appl Surf Sci, 2007; 253: 7535 |
| [12] | Mao Z P, Wang J, Sun B D, Yao C W.J Therm Spray Technol, 2009; 18: 563 |
| [13] | Borgioli F, Galvanetto E, Galliano F P, Bacci T.Wear, 2006; 260: 832 |
| [14] | Rosu R A, Serban V A, Bucur A I, Dragos U.Appl Surf Sci, 2012; 258: 3871 |
| [15] | Shahien M, Yamada M, Yasui T, Fukumoto M.J Therm Spray Technol, 2011; 20: 580 |
| [16] | Liu H Y, Huang J H, Yin C F, Zhang J G, Lin G B.Ceram Int, 2007; 33: 827 |
| [17] | Shanmugavelayutham G, Yano S, Kobayashi A.Vacuum, 2006; 80: 1336 |
| [18] | Ye F X, Tsumura T, Nakata K, Ohmori A.Mater Sci Eng, 2008; B148: 154 |
| [19] | Culha O, Tekmen C, Toparli M, Tsunekawa Y.Mater Des, 2010; 31: 533 |
| [20] | Tekmen C, Ozdemir I, Fritsche G, Tsunekawa Y.Surf Coat Technol, 2009; 203: 2046 |
| [21] | Sahu J K, Sahoo C K, Masanta M.Mater Manuf Process, 2015; 30: 736 |
| [22] | Isalgue A, Fernandez J, Cinca N, Villa M, Guilemany J M.J Alloys Compd, 2013; 577: S277 |
| [23] | Wang W F, Wang M C, Sun F J.Heat Treat Met, 2009; 34(2): 65 |
| [23] | (王维夫, 王茂才, 孙凤久. 金属热处理, 2009; 34(2): 65) |
| [24] | Liu L, Fu H Z, Shi Z X.Acta Metall Sin, 1989; 25: 48 |
| [24] | (刘林, 傅恒志, 史正兴. 金属学报, 1989; 25: 48) |
/
| 〈 |
|
〉 |