STRESS CORROSION CRACKING OF X80 PIPELINE STEEL AT COATING DEFECT IN ACIDIC SOIL
Received date: 2015-12-15
Online published: 2016-06-12
Supported by
Supported by National Natural Science Foundation of China (No.51131001) and National Research and Development Infrastructure and Facility Development Program of China (No.2005DKA10400)
The three-layer polyethylene (3PE or 3LPE) coatings have been widely used on long-distance high pressure transmission pipelines in China. The 3PE coating tends to remain high insulating after disbonding from pipelines, and block the function of cathoidc protection (CP), similar to PE tape coatings that caused stress corrosion cracking (SCC) failure of pipeline. Disbondment 3PE coatings have been reported worldwide. Because of the high integrity and dielectric strength of 3PE coatings, SCC under disbonded 3PE coating becomes an important issue for integrity management and operation of high pressure pipelines. A great deal of researches have been conducting over the past 20 years to reproduce SCC of high strength low alloy (HSLA) pipeline in laboratory. Most of these studies were conducted in bulk solution condition. The methodology neglects particularity of the thin-layer electrolyte under disbonded coating which has been identified as one of the primary environmental factors related to SCC. In this context, a research project has been initiated on this subject. The overall goal is to systematically investigate corrosion scenarios and mechanochemical interaction of HSLA pipeline steels under disbonded 3PE coating in different soil environments, particularly to further mechanistic understanding the initiation of SCC on pipelines under disbonded coating. In this work, SCC behavior of API X80 pipeline steel under disbonded coating with defect was investigated in acidic soil solution by a crevice cell specially designed for simulating coating disbondment. The crevice cell was equipped with a multi-sample loading frame, through which multi specimens in the crevice cell can be loaded simultaneously. Electrochemical impedance spectroscopy (EIS) was applied to characterize local electrochemical process of the tensile specimens. Local environment parameters (potential and pH) were monitored by microelectrodes. Surface morphology of the corrosion specimens indicate that corrosion intensity of X80 steel decreased over the distance from the opening. Intensive anodic dissolution and microcrack initiation were preferential at the opening defect, whereas corrosion was markedly mitigated under disbonded coating. CO2 content gradient is proposed for the special corrosion scenarios under coating disbondment.
Maocheng YAN , Shuang YANG , Jin XU , Cheng SUN , Tangqing WU , Changkun YU , Wei KE . STRESS CORROSION CRACKING OF X80 PIPELINE STEEL AT COATING DEFECT IN ACIDIC SOIL[J]. Acta Metall Sin, 2016 , 52(9) : 1133 -1141 . DOI: 10.11900/0412.1961.2015.00641
| [1] | Shen G J, Chen H Y, Xue Z Y, Zhao J.Corros Sci Prot Technol, 2013; 25: 246 |
| [1] | (沈光霁, 陈洪源, 薛致远, 赵君. 腐蚀科学与防护技术, 2013; 25: 246) |
| [2] | Tang Y P, Yan R J, Huang Z Y, Li J X, Wang L.Mater Prot, 2011; 44: 45 |
| [2] | (唐谊平, 晏荣军, 黄子阳, 李建新, 王琍. 材料保护, 2011; 44: 45) |
| [3] | Xue Z Y, Bi W X, Chen Z H, Zhang F, Chen H Y.Oil Gas Storage Transp, 2014; 33: 938 |
| [3] | (薛致远, 毕武喜, 陈振华, 张丰, 陈洪源. 油气储运, 2014; 33: 938) |
| [4] | Argent C, Norman .D Corrosion2005, Houston, TX: NACE, 2005:Paper 05034 (CD) |
| [5] | Yan M C, Wang J Q, Ke W, Han E-H.J Chin Soc Corros Prot, 2007; 27: 257 |
| [5] | (闫茂成, 王俭秋, 柯伟, 韩恩厚. 中国腐蚀与防护学报, 2007; 27: 257) |
| [6] | Yan M C, Wang J Q, Han E-H, Ke W.Corros Sci, 2008; 50: 1331 |
| [7] | Chen X, Li X G, Du C W, Cheng Y F.Corros Sci, 2009; 51: 2242 |
| [8] | Chang B T, Jiang H, Sue H J, Wong D, Kehr A, Mallozzi M.Proc 17th Int Conf on Pipeline Protection, Edinburgh, UK (CD) |
| [9] | Nazarbeygi A E, Moeini A R.Mater Perform, 2009; 48: 32 |
| [10] | Lagos F F, Maga?a C S, Lopez M A, Padilla J, Canto J, Villamizar W, Martinez-de la-Escalera L M, Ascencio J A, Martínez L. Corrosion2010, Houston, TX: NACE, 2010:Paper 10003 (CD) |
| [11] | Song F M, Kirk D W, Graydon J W, Cormack D E, Wong D. Mater Perform, 2003; 42: 24 |
| [12] | Parkins R N. Corrosion2000, Houston, TX: NACE, 2005:Paper 363 (CD) |
| [13] | National Energy Board.Report of Public Inquiry Concerning Stress Corrosion Cracking on Canadian Oil and Gas Pipelines. MH-2-95, 1996 |
| [14] | Yan M C, Wang J Q, Han E-H, Ke W.Corros Eng Sci Technol, 2007; 42: 42 |
| [15] | Charles E A, Parkins R N.Corrosion, 1995; 51: 518 |
| [16] | Yan M, Sun C, Xu J, Wu T Q, Yang S, Ke W. Corros Sci, 2015; 93: 27 |
| [17] | Eslami A, Fang B, Kania R, Worthingham B, Been J, Eadie R, Chen W.Corros Sci, 2010; 52: 3750 |
| [18] | Liu Z Y, Li X G, Du C W, Zhai G L, Cheng Y F.Corros Sci, 2008; 50: 2251 |
| [19] | Yan M C, Sun C, Xu J, Dong J H, Ke W.Corros Sci, 2014; 80: 309 |
| [20] | Zhao B, Du C W, Liu Z Y, Li X G, Yang J K, Li Y Q.Acta Metall Sin, 2012; 48: 1530 |
| [20] | (赵博, 杜翠薇, 刘智勇, 李晓刚, 杨吉可, 李月强. 金属学报, 2012; 48: 1530) |
| [21] | Yan M C, Sun C, Dong J H, Xu J, Ke W.Corros Sci, 2015; 97: 62 |
| [22] | Paolinelli L D, Perez T, Simison S N.Corros Sci, 2008; 50: 2456 |
| [23] | Fang B Y, Eadie R L, Chen W X, Elboujdaini M.Corros Eng Sci Technol, 2010; 45: 302 |
| [24] | Chechirlian S, Eichner P, Keddam M, Takenouti H, Mazille H.Electrochim Acta, 1990; 35: 1125 |
| [25] | Rosborg B, Kosec T, Kranjc A, Pan J, Legat A.Electrochim Acta, 2011; 56: 7862 |
| [26] | Sridhar N, Dunn D S, Seth M.Corrosion, 2001; 57: 598 |
| [27] | Egbewande A, Chen W, Eadie R, Kania R, Van Boven G, Worthingham R, Been J.Corros Sci, 2014; 83: 343 |
| [28] | Egbewande A, Chen W, Eadie R, Kania R, Van Boven G, Worthingham R, Been J.Metall Mater Trans, 2014; 45A: 4946 |
| [29] | Fu A Q, Cheng Y F.Corros Sci, 2010; 52: 2511 |
| [30] | Yan M C, Weng Y J.J Chin Soc Corros Prot, 2005; 25: 34 |
| [30] | (闫茂成, 翁永基. 中国腐蚀与防护学报, 2005; 25: 34) |
| [31] | Eslami A, Kania R, Worthingham B, Boven G V, Eadie R, Chen W.Corrosion, 2013; 69: 1103 |
| [32] | Chen W, Kania R, Worthingham R, Boven G V.Acta Mater, 2009; 57: 6200 |
| [33] | Wang Z Y, Wang J Q, Han E-H, Ke W, Yan M C, Zhang J W, Liu C W.Acta Metall Sin, 2012; 48: 1267 |
| [33] | (王志英, 王俭秋, 韩恩厚, 柯伟, 闫茂成, 张峻巍, 刘楚威. 金属学报, 2012; 48: 1267) |
/
| 〈 |
|
〉 |