Orginal Article

EFFECT OF COILING TEMPERATURE ON MICRO-STRUCTURE AND MECHANICAL PROPERTIES OF Ti-V-Mo COMPLEX MICROALLOYED ULTRA-HIGH STRENGTH STEEL

  • Ke ZHANG ,
  • Qilong YONG ,
  • Xinjun SUN ,
  • Zhaodong LI ,
  • Peilin ZHAO
Expand
  • 1 School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
    2 Department of Structural Steels, Central Iron and Steel Research Institute, Beijing 100081, China
    3 R&D Center, Laiwu Iron and Steel Group Co. Ltd., Laiwu 271104, China

Received date: 2015-07-23

  Online published: 2016-05-25

Supported by

Supported by National Basic Research Program of China (No.2015CB654803), National Natural Science Foundation of China (No.51201036) and National Science and Technology Pillar Program (No.2013BAE07B05)

Abstract

Among various hardening factors of steels, precipitation hardening has the least embrittlement vector value except grain refinement hardening. Giving full play to the precipitation hardening of microalloyed carbonitrides is an important aspect in the development of microalloyed high strength steels. Recently, the research on behaviors of precipitation and development of microalloyed high strength steels is mainly focused on these relatively simple microalloyed steels including single V, single Ti, Ti-V and Ti-Mo microalloyed steels, while paid less attention on complex microalloyed steels such as Ti-V-Mo steels. Therefore, it is expected to provide a theoretical basis and a practical significance for the development of Ti-V-Mo microalloyed high strength steel. Various hardening increments at different coiling temperatures were calculated. Meanwhile, the effect of coiling temperatures on yield strength and the influence of MC particles on uniform elongation were discussed by means of OM, EBSD, TEM, XRD and physical-chemical phase analysis. The results show that Ti-V-Mo steel has the best mechanical properties with ultimate tensile strength of 1134 MPa, yield strength of 1080 MPa, elongation of 13.2% and uniform elongation of 6.8% at coiling temperature of 600 ℃. The precipitation hardening increment was high to about 444~487 MPa due to the mass fraction of about 72.6% of total precipitates with a size of ?10 nm. In addition, precipitation hardening and grain refinement hardening are the main mechanisms to improve the strength of Ti-V-Mo steel, while the variation in precipitation hardening increment causes a significent difference in yield strength. With the coiling temperature increases from 500 ℃ to 600 ℃, the ultimate tensile strength and yield strength increase continuously, but the uniform elongation increases slowly instead of decreasing, which is mainly attributed to an increase of precipitation hardening increment.

Cite this article

Ke ZHANG , Qilong YONG , Xinjun SUN , Zhaodong LI , Peilin ZHAO . EFFECT OF COILING TEMPERATURE ON MICRO-STRUCTURE AND MECHANICAL PROPERTIES OF Ti-V-Mo COMPLEX MICROALLOYED ULTRA-HIGH STRENGTH STEEL[J]. Acta Metall Sin, 2016 , 52(5) : 529 -537 . DOI: 10.11900/0412.1961.2015.00411

References

[1] Xu Z Y.Shanghai Met, 2009; 31(2): 1
[1] (徐祖耀. 上海金属, 2009; 31(2): 1)
[2] Gan Y, Dong H.China Metall, 2004; (8): 1
[2] (干勇, 董翰.中国冶金, 2004; (8): 1)
[3] Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Yamamoto T, Maeda E.ISIJ Int, 2004; 44: 1945
[4] Chen C Y, Yen H W, Kao F H, Li W C, Huang C Y, Yang J R, Wang S H.Mater Sci Eng, 2009; A499: 162
[5] Jang J H, Lee C H, Heo Y U, Suh D W.Acta Mater, 2012; 60: 208
[6] Kazuhiro S, Yoshimasa F, Shinjiro K.JFE Tech Rep, 2007; 10: 19
[7] Kang J Y. Master Thesis, Central Iron and Steel Research Institute, Beijing, 2015
[7] (康俊雨. 钢铁研究总院硕士学位论文, 北京, 2015)
[8] Kim Y W, Song S W, Seo S J, Hong S G, Lee C S.Mater Sci Eng, 2013; A565: 430
[9] Kim Y W, Kim J H, Hong S G, Lee C S.Mater Sci Eng, 2014; A605: 244
[10] Park D B, Huh M Y, Shim J H, Suh J Y, Lee K H, Jung W S.Mater Sci Eng, 2013; A560: 528
[11] Shen Y F, Wang C M, Sun X.Mater Sci Eng, 2011; A528: 8150
[12] Jha G, Das S, Sinha S, Lodh A, Haldar A.Mater Sci Eng, 2013; A561: 394
[13] Xu M, Sun X J, Liu Q Y, Dong H, Yong Q L, Huang J L.Iron Steel Vanadium Titanium, 2005; 26(3): 7
[13] (徐曼, 孙新军, 刘清友, 董瀚, 雍岐龙, 黄金亮. 钢铁钒钛, 2005; 26(3): 7)
[14] Wang Z Q.PhD Dissertation, Tsinghua University, Beijing, 2013
[14] (王振强. 清华大学博士学位论文, 北京, 2013)
[15] Zhang K, Sun X J, Yong Q L, Li Z D, Yang G W, Li Y M.Acta Metall Sin, 2015; 51: 553
[15] (张可, 孙新军, 雍岐龙, 李昭东, 杨庚蔚, 李员妹. 金属学报, 2015; 51: 553)
[16] Xu Y, Sun M X, Zhou Y L, Liu Z Y.Acta Metall Sin, 2015; 51: 31
[16] (徐洋, 孙明雪, 周砚磊, 刘振宇. 金属学报, 2015; 51: 31)
[17] Sun C F, Cai Q W, Wu H B, Mao H Y, Chen H Z.Acta Metall Sin, 2012; 48: 1415
[17] (孙超凡, 蔡庆伍, 武会宾, 毛红艳, 陈宏振. 金属学报, 2012; 48: 1415)
[18] Duan X G, Cai Q W, Wu H B, Tang D.J Univ Sci Technol Beijing, 2012; 34: 644
[18] (段修刚, 蔡庆伍, 武会宾, 唐狄. 北京科技大学学报, 2012; 34: 644)
[19] Iza-Mendia A, Gutiérrez I.Mater Sci Eng, 2013; A561: 40
[20] Yong Q L, Ma M T, Wu B R.Microalloyed Steel-Physical and Mechanical Metallurgy. Beijing: China Machine Press, 1989: 65
[20] (雍岐龙, 马鸣图, 吴宝榕. 微合金钢─物理和力学冶金. 北京: 机械工业出版社, 1989: 65)
[21] Gladman T, McLvor I D, Pickering F B.J Iron Steel Int, 1972; 210: 916
[22] Zhang K, Li Z D, Sun X J, Yong Q L, Yang J W, Li Y M, Zhao P L.Acta Metall Sin (Engl Lett), 2015; 28: 641
[23] Petch N J.J Iron Steel Inst, 1953; 174: 25
[24] Petch N J.Philos Mag, 1958; 3: 1089
[25] Bailey J E, Hirsch P B.Philos Mag, 1960; 5: 485
[26] Chin G Y, Mammel W L.Trans Metall Soc AIME, 1967; 239: 1400
[27] Keh A S.Philos Mag, 1965; 12: 9
[28] Yong Q L.Secondary Phases in Steel. Beijing: Metallurgical Industry Press, 2006: 20
[28] (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 20)
[29] Ashby M F.Philos Mag, 1970; 21: 399
[30] Ashby M F.Strengthening Methods in Crystals. London: Applied Science Publishers Ltd, 1971: 137
[31] Jha G, Das S, Lodh A, Haldar A.Mater Sci Eng, 2012; A552: 457
Outlines

/