Orginal Article

RESEARCH ON THE CARBIDE PRECIPITATION AND CHROMIUM DEPLETION IN THE GRAIN BOUNDARY OF ALLOY 690 CONTAINING DIFFERENT CONTENTS OF NITROGEN

  • Yingche MA ,
  • Shuo LI ,
  • Xianchao HAO ,
  • Xiangdong ZHA ,
  • Ming GAO ,
  • Kui LIU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-12-09

  Online published: 2016-05-13

Supported by

Supported by Chinese Academy of Scicences Innovation Foundation (No;CXJJ-14-M44)

Abstract

Nickel-based alloy Inconel 690 (hereinafter called alloy 690) is currently replacing alloy 600 as steam generator tubes in pressurized water nuclear reactors, owing to its excellent resistance to intergranular stress corrosion cracking (IGSCC) and good mechanical properties. The carbide precipitation is a major microstructural characteristic during heat treatment of stainless steels and nickel-based alloys. The carbide precipitation and chromium depletion in the grain boundary of alloy 690 were investigated. The grain size and carbide of alloy 690 with 0.001% and 0.03% (mass fraction) nitrogen contents were observed and analyzed. The extent of chromium depletion in the vicinity of grain boundaries was quantitatively determined as a function of thermal treatment time. The solution treatment of the samples was at 1080 ℃ for 10 min, and then the samples were thermally treated at 715 ℃ for 1~25 h. The results show that the nitrogen addition decreases the intergranular carbide density and the average carbide length but increases its distance. The level of chromium in the depleted regions in alloy 690 with 0.03%N is higher than that with 0.001%N. This is attributed to the beneficial role of nitrogen addition against grain growth and sensitization.

Cite this article

Yingche MA , Shuo LI , Xianchao HAO , Xiangdong ZHA , Ming GAO , Kui LIU . RESEARCH ON THE CARBIDE PRECIPITATION AND CHROMIUM DEPLETION IN THE GRAIN BOUNDARY OF ALLOY 690 CONTAINING DIFFERENT CONTENTS OF NITROGEN[J]. Acta Metall Sin, 2016 , 52(8) : 980 -986 . DOI: 10.11900/0412.1961.2015.00636

References

[1] Was G S..Corrosion, 1988; 46: 319
[2] Briant C L, Toole C S O, Hall E L.Corrosion, 1986; 42: 15
[3] Was G S, Tischner H H, Latanision R M.Metall Trans, 1981; 12A: 1397
[4] Yu G P, Yao H C.Corrosion, 1990; 46: 391
[5] Kai J J, Tsai C H, Huang T A, Liu M N.Metall Trans, 1989; 20A:1077
[6] Simmons J W.Mater Sci Eng, 1996; A207: 159
[7] Mozhi T A, Betrabet H S, Jagannathan V, Wilde B E, Clark W A T.Scr Metall, 1986; 20: 723
[8] Mozhi T A, Clark W A T, Nishimoto K, Johson W B, MacDonald D D.Corrosion, 1985; 41: 555
[9] Speidel M O, Pedrazzoli R M.Mater Perform, 1992; 31(9): 59
[10] Fuchs G E, Hayden S Z.Scr Mater, 1991; 25: 1483
[11] Jiang R, Chen B, Hao X C, Ma Y C, Li S, Liu K.J Mater Sci Technol, 2012; 28: 446
[12] Thuvander M, Miller M K, Stiller K.Mater Sci Eng, 1999; A270: 38
[13] Thuvander M, Stiller K, Olsson E.Mater Sci Technol, 1999; 15: 237
[14] Li S, Chen B, Ma Y C, Liu K.Acta Metall Sin, 2011; 47: 816
[14] (李硕, 陈波, 马颖澈, 刘奎. 金属学报, 2011; 47: 816)
[15] Betrabet H S, Nishimoto K, Wilde B E, Clark W A T.Corrosion, 1987; 43: 77
[16] Rios P R..Scr Mater, 1998; 39: 1725
[17] Rios P R, Fonseca G S.Scr Mater, 2004; 50: 1373
[18] Su Z Y, Liu C M.Diffusion and Phase Transformation in Alloys. Shenyang: Northeastern University Press, 2002: 39
[18] (孙振岩, 刘春明. 合金中的扩散与相变. 沈阳: 东北大学出版社, 2002: 39)
[19] Zener C.J Appl Phys, 1949; 20: 950
[20] Sahlaoui H, Sidhom H, Philibert J.Acta Mater, 2002; 50: 1383
[21] Mayo W E.Mater Sci Eng, 1997; A232: 129
[22] Sarver J M, Crum J R, Mankins W L.Corrosion NACE, 1988; 44: 288
[23] Nagano H, Yamanaka K, Kobayashi K, Inoue M.Sumitomo Search, 1989; 40: 57
Outlines

/

〈 〉