Supported by National Natural Science Foundation of China (Nos.51331005, 51171151 and 51501151), High Technology Research and Development Program of China (No.2012AA03A511), National Basic Research Program of China (No.2011-CB610406), Natural Science Foundation of Shaanxi Province (No.2014JM6227), Foundation Research Foundation of Northwestern Polytechnical University (No.3102014JCQ01022) and Advanced Aero Engine Collaborative Innovation Center of China
Ni-based single crystal superalloy has been widely used in turbine blades due to its excellent high temperature mechanical behavior. In order to completely exhibit high temperature mechanical properties, the seed method has been used to produce Ni-based single crystal components for [001] orientation paralleling to main force direction. Stray crystals, which unexpectedly nucleate in the melt-back region, will competitively grow with seed during directional solidification. It is important to profoundly understand the mechanism of competitive growth to find ways of overgrowing stray crystal during producing Ni-based single crystal components. However, within the published research there are conflicting views on the mechanism of competitive growth at converging case. Bi-crystal converging competitive growth was investigated in Ni-based single crystal superalloy with different pulling rates using seed technology. A series of polishing and imaging quenching interface were done for the positional relationship of dendrites near grain boundary in 3D reference. It was found that solidification microstruc tures were different with different crystal orientations. Unfavorable oriented dendrite tilting to heat flux restrained favorable oriented dendrite aligning to heat flux mainly thought inserting into the favorable oriented dendrites channel, and this resulted in unfavorable oriented dendrite overgrowing favorable oriented dendrite at low pulling rate. However, at high pulling rate the unfavorable oriented dendrites mainly blocked by grain boundary favorable oriented dendrite and the grain boundary grew paralleling to favorable oriented dendrite core. Favorable oriented dendrite being depressed and vanished, owning to that unfavorable oriented dendrite inserting into favorable oriented dendrites channel result in adjusting primary dendrite spacing, is the main factor to favorable oriented grain overgrew by unfavorable oriented grain. According to above mechanism, effect of pulling rate on competitive growth at converging case was interpreted. This could broaden our understanding of competitive growth at converging case in 3D reference.
Key words: Ni-based superalloy; competitive growth; pulling rate
Songsong HU , Lin LIU , Qiangwei CUI , Taiwen HUANG , Jun ZHANG , Hengzhi FU . CONVERGING COMPETITIVE GROWTH IN BI-CRYSTAL OF Ni-BASED SUPERALLOY DURINGDIRECTIONAL SOLIDIFICATION[J]. Acta Metall Sin, 2016 , 52(8) : 897 -904 . DOI: 10.11900/0412.1961.2015.00631
| [1] | Harris K, Erickson G L, Schwer R E. Metals Handbook.10th Ed., Vol.1, Ohio: ASM International, 1990: 995 |
| [2] | D'Souza N, Newell M, Devendra K, Jennings P A, Ardakani M G, Shollock B A.Mater Sci Eng, 2005; A413: 567 |
| [3] | Yang X L, Lee P D, D'Souza N.JOM, 2005; 57(5): 40 |
| [4] | Stanford N, Djakovic A, Shollock B A, Mclean M, D'Souza N, Jennings P A.Scr Mater, 2004; 50: 159 |
| [5] | Aveson J W, Tennant P A, Foss B J, Shollock B A, Stone H J, D'Souza N.Acta Mater, 2013; 61: 5162 |
| [6] | Walton D, Chalmers B.Trans Metall Soc AIME, 1959; 215: 447 |
| [7] | Wagner A, Shollock B A, McLean M.Mater Sci Eng, 2004; A374: 207 |
| [8] | Zhou Y Z, Volek A, Green N R.Acta Mater, 2008; 56: 2631 |
| [9] | Yu H L, Lin X, Li J J, Wang L L, Huang W D.Acta Metall Sin, 2013; 49: 58 |
| [9] | (宇红雷, 林鑫, 李俊杰, 王理林, 黄卫东. 金属学报, 2013; 49: 58) |
| [10] | Liu Z Y, Lin M, Yu D E, Zhou X W, Gu Y X, Fu H Z.Metall Mater Tran, 2013; 44A: 5113 |
| [11] | Zhang H, Xu Q Y, Sun C B, Qi X, Tang N, Liu B C.Acta Metall Sin, 2013; 49: 1521 |
| [11] | (张航, 许庆彦, 孙长波, 戚翔, 唐宁, 刘百成. 金属学报, 2013; 49: 1521) |
| [12] | Rappaz M, Gandin C A, Desbiolles J L, Thevoz P.Metall Mater Trans, 1996; 27A: 695 |
| [13] | Rappaz M, Gandin C A.Acta Metall, 1994; 42: 2233 |
| [14] | Zhou Y Z, Jin T, Sun X F.Acta Metall Sin, 2010; 46: 1327 |
| [14] | (周亦胄, 金涛, 孙晓峰. 金属学报, 2010; 46: 1327) |
| [15] | Li J J, Wang Z J, Wang Y Q, Wang J C.Acta Mater, 2012; 60: 1478 |
| [16] | Yang C B, Liu L, Zhao X B, Wang N, Zhang J, Fu H Z.J Alloys Compd, 2013; 578: 557 |
| [17] | Zhang X L.PhD Dissertation, University of Chinese Academy of Sciences, Beijing, 2013 |
| [17] | (张小丽. 中国科学院大学博士学位论文 ,北京, 2013) |
| [18] | Takaki T, Ohno M, Shibuta Y, Sakane S, Shimokawabe T.J Cryst Growth, 2016; 442: 14 |
| [19] | Takaki T, Ohno M, Shimokawabe T, Aoki T.Acta Mater, 2014; 81: 272 |
| [20] | Yu H L, Li J J, Lin X, Wang L L, Huang W D.J Cryst Growth, 2014; 402: 210 |
| [21] | Zhou Y Z, Sun X F.Sci China Tech Sci, 2012; 55: 1327 |
| [22] | Meng X B, Lu Q, Zhang X L, Li J T, Chen Z Q, Wang Y H, Zhou Y Z, Jin T, Sun X F, Hu Z Q.Acta Mater, 2012; 60: 3965 |
| [23] | Lu Q, Li J G, Jin T, Zhou Y Z, Sun X F, Hu Z Q.Acta Metall Sin, 2011; 47: 641 |
| [23] | (卢琦, 李金国, 金涛, 周亦胄, 孙晓峰, 胡壮麒. 金属学报, 2011; 47: 641) |
| [24] | Sakae S, Takaki T, Ohno M, Shimokawabe T, Aoki T.In: IOP Conference Series: Materials Science and Engineering, 2015; 84: 012063 |
| [25] | Han S H, Trivedi R.Acta Metall Mater, 1994; 42: 25 |
| [26] | Fu H Z, Guo J J, Liu L, Li J S.Directional Solidification and Processing of Advanced Materials. Beijing: Science Press, 2008: 267 |
| [26] | (傅恒志, 郭景杰, 刘林, 李金国. 先进材料定向凝固. 北京: 科学出版社, 2008: 267) |
/
| 〈 |
|
〉 |