EFFECTS OF MICROSTRUCTURE AND STRESS RATIO ON HIGH-CYCLE AND VERY-HIGH-CYCLE FATIGUE BEHAVIOR OF Ti-6Al-4V ALLOY

  • Xiaolong LIU ,
  • Chengqi SUN ,
  • Yantian ZHOU ,
  • Youshi HONG
Expand
  • 1 State Key Laboratory of Nonlinear Mechanics, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100190, China 。
    2 Heat Treatment Plant, Wafangdian Bearing Co. Ltd., Dalian 116300, China

Received date: 2015-11-12

  Online published: 2016-05-04

Supported by

Supported by National Natural Science Foundation of China (Nos.11202210 and 11572325)

Abstract

Titanium alloys have been widely used as superior engineering materials because of their high specific strength, high temperature resistance and high corrosion resistance. In their engineering applications such as used in aircraft engines, titanium alloys may experience even 1010 fatigue cycles. Recently, faceted crack initiation was observed in high-cycle fatigue (HCF) and very-high-cycle fatigue (VHCF) regimes of titanium alloys, which resulted in a sharp decrease in fatigue strength. Therefore, the HCF and VHCF of titanium alloys have both scientific significance and engineering requirement. In this work, the effects of microstructure and stress ratio (R) on HCF and VHCF of a Ti-6Al-4V alloy have been investigated. Fatigue tests were conducted on a rotating-bending fatigue machine and an ultrasonic fatigue machine. All the fatigue fracture surfaces were observed by SEM. The results show that the HCF and VHCF behaviors of the fully-equiaxed and the bimodal Ti-6Al-4V alloy are similar. The observations of fracture surface indicate that two crack initiation mechanisms prevail, i.e. slip mechanism and cleavage mechanism. With the increase of stress ratio, the crack initiation mechanism switches from slip to cleavage. The S-N curves present the single-line type or the bilinear type. For the cases of rotating-bending and ultrasonic axial cycling with R= -1.0, -0.5 and 0.5, the S-N curves are single-line type corresponding to the slip mechanism or cleavage mechanism. For the cases of R= -0.1 and 0.1, the S-N curves are bilinear type corresponding to both slip and cleavage mechanisms. A model based on fatigue life and fatigue limit is proposed to describe the competition between the two mechanisms, which is in agreement with the experimental results.

Cite this article

Xiaolong LIU , Chengqi SUN , Yantian ZHOU , Youshi HONG . EFFECTS OF MICROSTRUCTURE AND STRESS RATIO ON HIGH-CYCLE AND VERY-HIGH-CYCLE FATIGUE BEHAVIOR OF Ti-6Al-4V ALLOY[J]. Acta Metall Sin, 2016 , 52(8) : 923 -930 . DOI: 10.11900/0412.1961.2015.00581

References

[1] Li S X.Int Mater Rev, 2012; 57: 92
[2] Hong Y S, Zhao A G, Qian G A.Acta Metall Sin, 2009; 45: 769
[2] (洪友士, 赵爱国, 钱桂安. 金属学报, 2009; 45: 769)
[3] Liu X L, Sun C Q, Hong Y S.Mater Sci Eng, 2015; A622: 228
[4] Leopold G, Nadot Y, Billaudeau T, Mendez J.Fatigue Fract Eng Mater Struct, 2015; 38: 1026
[5] Ding H S, Shang Z B, Wang Y Z, Chen R R, Guo J J, Fu H Z.Acta Metall Sin, 2015; 51: 569
[5] (丁宏升, 尚子博, 王永喆, 陈瑞润, 郭景杰, 傅恒志. 金属学报, 2015; 51: 569)
[6] Neal F D, Blenkinsop P A.Acta Metall, 1976; 24: 59
[7] Szczepanski C J, Jha S K, Larsen J M, Jones J W.Metall Mater Trans, 2008; 39A: 2841
[8] Chandran K S, Jha S K.Acta Mater, 2005; 53: 1867
[9] Chandran K S, Chang P, Cashman G T.Int J Fatigue, 2010; 32: 482
[10] Oguma H, Nakamura T.Int J Fatigue, 2013; 50: 89
[11] Oguma H, Nakamura T.Scr Mater, 2010; 63: 32
[12] Chandran K S.Nat Mater, 2005; 4: 303
[13] Shanyavskiy A A.Sci China-Phys Mech Astron, 2014; 57: 19
[14] Lei Z Q, Xie J J, Sun C Q, Hong Y S.Sci China-Phys Mech Astron, 2014; 57: 74
[15] Matsunaga H, Sun C, Hong Y, Murakami Y.Fatigue Fract Eng Mater Struct, 2015; 38: 1274
[16] Goodman J.Mechanics Applied Engineering. London: Longman, Green and Co Ltd, 1899: 30
[17] Gerber W. Z Bayer Archit Ing Ver, 1874; 6: 101
[18] Zuo J H, Wang Z G, Han E-H.Mater Sci Eng, 2008; A473: 147
[19] Takeuchi E, Furuya Y, Nagashima N, Matsuoka S.Tetsu Hagané, 2010; 96: 36
[19] (竹内悦男, 古谷佳之, 長島伸夫, 松岡三郎.鉄と鋼, 2010; 96: 36)
[20] Takeuchi E, Furuya Y, Nagashima N, Matsuoka S.Fatigue Fract Eng Mater Struct, 2008; 31: 599
[21] Morrissey R, Nicholas T.Int J Fatigue, 2006; 28: 1577
[22] Basquin O H.Proc Astm, 1910; 10: 625
[23] Sun C, Lei Z, Hong Y.Mech Mater, 2014; 69: 227
[24] Qian G A, Zhou C E, Hong Y S.Acta Mater, 2011; 59: 1321
[25] Hong Y S, Zhao A G, Qian G A, Zhou C E.Metall Mater Trans, 2012; 43A: 2753
Outlines

/

〈 〉