Orginal Article

INFLUENCE OF NECKLACE-TYPE M-A CONSTITU-ENT ON IMPACT TOUGHNESS AND FRACTUREMECHANISM IN THE HEAT AFFECTED ZONE OF X100 PIPELINE STEEL

  • Xueda LI ,
  • Chengjia SHANG ,
  • Changchai HAN ,
  • Yuran FAN ,
  • Jianbo SUN
Expand
  • 1 College of Mechanical and Electronic Engineering, China University of Petroleum, Qingdao 266580, China
    2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
    3 Petroleum China West East Gas Pipeline Company, Shanghai 200120, China
    4 China Petroleum Pipeline Research Institute, Langfang 065000, China

Received date: 2015-11-27

  Online published: 2016-04-12

Supported by

Supported by National Basic Research Program of China (No.2010CB630801), China Postdoctoral Science Foundation (No.2015M582159) and Qingdao Postdoctoral Application Research Foundation (No.2015240)

Abstract

After decades of development, mechanical properties of pipeline steels have a good combination of strength and toughness. But after welding, in the heat affected zone (HAZ), microstructure of the base plate was erased by the welding thermal cycle. Several subzones with different microstructures were formed in the HAZ due to different thermal histories they went through. Toughness of the HAZ varies due to the heterogeneous microstructure. In this work, toughness of the HAZ of X100 pipeline steel was examined with two notch locations. Low toughness of 51 J was obtained when the notch encountered intercritically reheated coarsen-grained (ICCG) HAZ and high toughness of 183 J when the notch did not contain ICCGHAZ. Meanwhile, different sub-zones in the HAZ were simulated using Gleeble thermal simulation machine. Simulated coarsen-grained (CG) HAZ, fine-grained (FG) HAZ and intercritically reheated (IC) HAZ with uniform microstructure had good toughness of 244, 164 and 196 J, respectively. In contrast, toughness of simulated ICCGHAZ was only 32 J. Therefore, ICCGHAZ consisting of coarse granular/upper bainite and necklace-type martensite-austenite (M-A) constituent along grain boundaries was proved to be the primary reason for low toughness. Instrumented Charpy impact test results showed that ICCGHAZ could notably embrittle the sample and lower the crack initiation energy. Characterization on the fracture surfaces of the as-fractured Charpy impact specimens showed that ICCGHAZ was found to be the crack initiation site of the whole fracture, and M-A constituent in the ICCGHAZ was characterized as cleavage facet initiation. Fracture mechanisms in the CGHAZ and ICCGHAZ were separately investigated using EBSD. The results showed that necklace-type M-A constituent in the ICCGHAZ notably increased the frequency of cleavage microcracks nucleation. Fracture mechanism changed from nucleation controlled in the CGHAZ to propagation controlled in the ICCGHAZ due to the existence of necklace-type M-A constituent. Therefore, the formation of necklace-type M-A constituent in the ICCGHAZ could not only cause notable drop of toughness in the HAZ, but also change the fracture behavior/mechanism. Hence, research on how to control the distribution status of M-A constituent in the ICCGHAZ is the key to improve the toughness of a weld joint.

Cite this article

Xueda LI , Chengjia SHANG , Changchai HAN , Yuran FAN , Jianbo SUN . INFLUENCE OF NECKLACE-TYPE M-A CONSTITU-ENT ON IMPACT TOUGHNESS AND FRACTUREMECHANISM IN THE HEAT AFFECTED ZONE OF X100 PIPELINE STEEL[J]. Acta Metall Sin, 2016 , 52(9) : 1025 -1035 . DOI: 10.11900/0412.1961.2015.00610

References

[1] Shang C J, Wang X X, Liu Q Y, Fu J Y.In: Gray J M ed., Proceedings of the International Seminar on Welding of High Strength Pipeline Steel, Araxa, Brazil: TMS, 2011: 435
[2] Shang C J, Li X D, Nie W J, Wu S J.In: Deardo A ed., Proceedings of Recent Developments in High Strength Steels for Energy Applications, Pittsburgh, USA: MS&T, 2012: 892
[3] Matsuda F, Fukada Y, Okada H, Shiga C, Ikeuchi K, Horii Y, Shiwaku T, Suzuki S.Welding World, 1996; 37: 134
[4] Fairchild D P.In Koo J Y ed., Proceedings of Welding Metallurgy of Structural Steels, Warrendale, Pennsylvania, USA: TMS-AIME, 1987: 303
[5] Lambert A, Drillet J, Gourgues A F, Sturel T, Pineau A.Sci Technol Welding Joining, 2000; 5: 168
[6] You Y, Shang C J, Nie W J, Subramanian S.Mater Sci Eng, 2012; A558: 692
[7] Davis C L, King J E.Metall Mater Trans, 1994; 25A: 563.
[8] Mohseni P, Solberg J K, Karlsen M, Akselsen O M, ?stby E.Metall Mater Trans, 2014; 45A: 384
[9] Li Y, Baker T N.Mater Sci Technol, 2010; 26: 1029
[10] Chen J H, Kikuta Y, Araki T, Yoneda M, Matsuda Y.Acta Metall, 1984; 32: 1779
[11] Lambert-Perlade A, Gourgues A F, Besson J, Sturel T, Pineau A.Metall Mater Trans, 2004; 35A: 1039
[12] Thompson A W, Knott J F.Metall Trans, 1993; 24A: 523
[13] Curry D A.Met Sci, 1980; 14: 319
[14] Fairchild D P, Howden D G, Clark W A T.Metall Mater Trans, 2000; 31A: 641
[14] Fairchild D P, Howden D G, Clark W A T.Metall Mater Trans, 2000; 31A: 641
[15] Ritchie R O, Knott J F, Rice J R.J Mech Phys Solids, 1973; 21: 395
[16] Griffiths J R, Owen D R J.J Mech Phys Solids, 1971; 19: 419
[17] Bouyne E, Flower H M, Lindley T C, Pineau A.Scr Mater, 1998; 39: 295
[18] Lin T, Evans A G, Ritchie R O.Acta Metall, 1986; 34: 2205
[19] Guo A M,Misra R D K, Liu J B, Chen L, He X L, Jansto S J.Mater Sci Eng, 2010; A527: 6440
[20] Nohava J, Hausild P, Karlik M, Bompard P.Mater Charact, 2003; 49: 211
[21] Venegas V, Caleyo F, Gonzalez J L, Baudin T, Hallen J M, Penelle R.Scr Mater, 2005; 52: 147
[22] Jian H G, Jiang F, Wei L L, Zheng X Y, Wen K.Mater Sci Eng, 2010; A527: 5879
[23] Li X D, Fan Y R, Ma X P, Subramanian S V, Shang C J.Mater Des, 2015; 67: 457
[24] Li X D, Ma X P, Subramanian S V, Shang C J, Misra R D K.Mater Sci Eng, 2014; A616: 141
[25] You Y, Shang C J, Chen L, Subramanian S.Mater Des, 2013; 43: 485
[26] Pineau A.Int J Fract, 2006; 138: 139
Outlines

/

〈 〉