Orginal Article

INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT

  • Wei FU ,
  • Xiaoguo SONG ,
  • Long LONG ,
  • Jianhang CHAI ,
  • Jicai FENG ,
  • Guodong WANG
Expand
  • 1 State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China
    2 Shandong Provincial Key Lab of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264209, China

Received date: 2015-09-25

  Online published: 2016-04-06

Supported by

Supported by National Natural Science Foundation of China (No.51405099) and Aerospace Science and Technology Innovation Foundation of Shanghai (No.SAST2015045)

Abstract

Graphite and metal composite structures were widely used in aerospace, electrical engineering and electronics. Because of its conveniences and less cost, brazing was widely used to bond graphite and metals. Due to the differences in microstructure, graphite was difficult to be wetted by traditional braze alloys. To improve the wettability of traditional brazing alloys on graphite, active brazing process and indirect brazing process were developed to braze graphite to metals. As to active brazing process, active elements (such as Ti, Cr, Zr) were added into traditional brazing alloys, a high brazing temperature, was essential to guarantee the reaction of active elements with graphite. However, the mechanical properties of metals will degrade under high temperature. Electroplating and chemical plating were the general techniques for indirect brazing process. The covered coating had a mechanical combination which decreased the joint strength, rather than metallurgical bonding with graphite. Therefore, in this work, a new metallization method was proposed. On the one hand, a metallurgical bonding was formed between metallization layer and graphite substrate. On the other hand, graphite could be brazed to metal at a relatively low temperature. Firstly, graphite was metalized by Ti-containing Sn0.3Ag0.7Cu metallization powder at 950 ℃ for 30 min. Then metalized graphite was brazed with copper by Sn0.3Ag0.7Cu successfully. The typical interfacial structure of brazed joint was copper/Cu3Sn/Cu6Sn5/β-Sn/TiC/graphite. Element Ti of metallization powder played an important role in metallization process for a reaction layer TiC was formed on the interface of graphite and metallization layer. Nevertheless, Ti contents had no effect on interfacial structure and shear strength of brazed joint. With the increase of brazing temperature, more and more element Cu dissolved into molten solder and formed Cu-Sn compounds by reacting with Sn. Furthermore, shear strength was improved slightly. Fracture analysis reveals that cracks extended along β-Sn layer and presented ductile fracture. When Cu-Sn compounds occupied the entire brazing seam (joint brazed at 600 ℃), shear strength improved remarkably and reached 30 MPa. Additionally, the joint was fractured in graphite entirely.

Cite this article

Wei FU , Xiaoguo SONG , Long LONG , Jianhang CHAI , Jicai FENG , Guodong WANG . INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. Acta Metall Sin, 2016 , 52(6) : 734 -740 . DOI: 10.11900/0412.1961.2015.00502

References

[1] Zhong Z H, Zhou Z J, Ge C.J Mater Process Technol, 2009; 209: 2662
[2] Sueyoshi H, Fukudome H.Mater Trans, 2008; 49: 2063
[3] Xiong H P, Wan C G, Zhou Z F.Acta Metall Sin, 1999; 35: 527
[3] (熊华平, 万传庚, 周振丰. 金属学报, 1999; 35: 527)
[4] Chen B, Xiong H P, Mao W, Guo W L, Cheng Y Y, Li X H.Acta Metall Sin, 2007; 43: 1181
[4] (陈波, 熊华平, 毛唯, 郭万林, 程耀永, 李晓红. 金属学报, 2007; 43: 1181)
[5] Liu Y, Jiang G F, Xu K, Luo X M, Chen D Q, Li W.Acta Metall Sin, 2015; 51: 209
[5] (刘毅, 江国锋, 许昆, 罗锡明, 陈登权, 李伟. 金属学报, 2015; 51: 209)
[6] Ray A K, Kar A, Kori S A, Pathak L C, Sonnad A N.J Mater Eng Perform, 2013; 22: 258
[7] Makimura S, Ozaki H, Okamura H, Futakawa M, Naoe T, Miyake Y, Kawamura N, Nishiyama K, Kawai M.J Nucl Mater, 2008; 377: 28
[8] Caturla F, Molina F, Molina-Sabio M, Rodriguez-Reinoso F, Esteban A.J Electrochem Soc, 1995; 142: 4084
[9] Moutis N, Jimenez C, Azpiroz X, Speliotis T, Wilhelmi C, Messoloras S, Mergia K.J Mater Sci, 2010; 45: 74
[10] Wang Y Y, Li S J, Yan L S.Rare Met Mater Eng, 2005; 34: 970
[10] (王艳艳, 李树杰, 闫联生. 稀有金属材料与工程, 2005; 34: 970)
[11] Li Y Q, Zhang Z D, Den C Q, Su Y S.Mater Charact, 2000; 44: 425
[12] Zhang Z H, Zhou Z J, Song S X, Du J, Ge C C.Rare Met Mater Eng, 2006; 35: 117
[12] (钟志宏, 周张健, 宋书香, 都娟, 葛昌纯. 稀有金属材料与工程, 2006; 35: 117)
[13] Singh M, Smith C, Asthana R, Gyekenyesi A.Int J Appl Ceram Technol, 2013; 10: 790
[14] Song X G, Cao J, Liu J K, Wang Y F, Feng J C. Chin Pat, 10094289.8, 2014(宋晓国, 曹健, 刘甲坤, 王义峰, 冯吉才. 中国专利,10094289.8, 2014)
[15] Okamoto H. J Phase Equilib Diff, 2010; 31: 202
[16] Singh M, Shpargel T P, Morscher G N, Asthana R.Mater Sci Eng, 2005; A412: 123
[17] Wang B Y. Mater Thesis, China University of Petroleum, Dong- ying, 2009
[17] (王宝阳. 中国石油大学硕士学位论文, 东营, 2009)
[18] Naidich Y.Curr Opin Solid State Mater Sci, 2005; 9: 161
[19] Standing R, Nicholas M.J Mater Sci, 1978; 13: 1509
[20] Singh M, Smith C, Asthana R, Gyekenyesi A.Int J Appl Ceram Technol, 2013; 10: 790
[21] Yu W Y, Liu S H, Liu X Y, Liu M P, Shi W G.J Mater Process Technol, 2015; 221: 285
[22] Zhu W J, Wang J, Liu L B, Liu H S, Jin Z P, Leinenbach C.Comput Mater Sci, 2013; 78: 74
[23] Laurila T, Vuorinen V, Kivilahti J K.Mater Sci Eng, 2005; R49: 1
[24] Hwang C W, Kim K S, Suganuma K.J Electron Mater, 2003; 32: 1249
[25] Gong J, Liu C, Conway P P, Silberschmidt V V.Acta Mater, 2008; 56: 4291
Outlines

/

〈 〉