Orginal Article

EFFECTS OF SECOND PHASES ON MICROARC OXIDATION PROCESS OF MAGNESIUM BASE MATERIALS

  • Yanqiu WANG ,
  • Kun WU ,
  • Fuhui WANG
Expand
  • 1) Education Ministry Key Laboratory of Superlight Materials and Surface Technology, Harbin Engineering University, Harbin 150001, China
    2) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
    3) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-09-25

  Online published: 2016-04-06

Supported by

Supported by National Natural Science Foundation of China (No.51001036) and International S&T Cooperation Program of China (No.2014DFR50560)

Abstract

The effects of second phases on microarc oxidation (MAO, also named plasma electrolytic oxidation-PEO) behavior of Mg base materials were investigated and the related mechanism was discussed. The formation of barrier layer and its influence on sparking discharge behavior were characterized and analyzed on the base of systematic selecting and designing substrate materials. The variation of second phases at the early MAO stage was observed and analyzed by SEM and EDS, and then the effect mechanism of second phases on MAO behaviors was revealed. Voltage evolution trend during MAO were recorded to study the formation state of the barrier layer on the different Mg base materials. According to the growth mechanism of MAO film, the film growth process can be simplistically considered as a repeated breakdown and reconstruction process of a capacitor. Accordingly, the growth process of MAO film on multiphase metal materials and the effects of second phases were discussed. The results show that different second phases in substrate materials have different effects on formation process of MAO films, depending on their own characteristics. For the second phases which have the characteristics of valve metals, although selective sparking discharge occurs at the early stage of MAO, the second phases will not hinder the growth of MAO film since barrier layer can form on the second phases, and they will not induce structural defects into the film-substrate interface. If the second phases have not the characteristics of valve metals, their conductivity property will be an important influencing factor to affect the MAO behaviors. For the elecinsulating second phases which have not the characteristics of valve metals, sparking discharge just occurs on Mg matrix in the substrate, while doesn't occur on the second phases; the second phases exist in the MAO film as heterogeneous phases, do not react in MAO process, and will not hinder the growth of MAO film. For the semi-conductive second phases which have not the characteristics of valve metals, they delay the growth of MAO film because they destroy the integrity of barrier layer. For the electroconductive second phases which have not the characteristics of valve metals, they seriously hinder the growth of MAO film.

Cite this article

Yanqiu WANG , Kun WU , Fuhui WANG . EFFECTS OF SECOND PHASES ON MICROARC OXIDATION PROCESS OF MAGNESIUM BASE MATERIALS[J]. Acta Metall Sin, 2016 , 52(6) : 689 -697 . DOI: 10.11900/0412.1961.2015.00500

References

[1] Van T B, Brown S D, Wirtz G P.Ceram Bull, 1977; 56: 563
[2] Ikonopisov S.Electrochim Acta, 1977; 22: 1077
[3] Srinivasan P B, Liang J, Blawert C, Stormer M, Dietzel W.Appl Surf Sci, 2009; 255: 4212
[4] Li X J, Cheng G A, Xue W B, Zheng R T, Cheng Y J.Mater Chem Phys, 2008; 107: 148
[5] Wang Y M, Lei T Q, Jiang B L, Guo L X.Appl Surf Sci, 2004; 233: 258
[6] Verdier S, Boinet M, Maximovitch S, Dalard F.Corros Sci, 2005; 47: 1429
[7] Krishtal M M.Met Sci Heat Treat, 2004; 46: 378
[8] Khaselev O, Weiss D, Yahalom J.Corros Sci, 2001; 43: 1295
[9] Khaselev O, Yahalom J.Corros Sci, 1998; 40: 1149
[10] Hsiao H Y, Tsai W T.J Mater Res, 2005; 20: 2763
[11] Zhu Q Z, Xue W B, Lu L, Du J C, Liu G J, Li W F.Acta Metall Sin, 2011; 47: 74
[11] (朱庆振, 薛文斌, 鲁亮, 杜建成, 刘贯军, 李文芳. 金属学报, 2011; 47: 74)
[12] Xue W B.Appl Surf Sci, 2006; 252: 6195
[13] Xue W B, Wu X L, Li X J, Tian H.J Alloys Compd, 2006; 425: 302
[14] Xue W B, Jin Q, Zhu Q Z, Hua M, Ma Y Y. J Alloys Compd, 2009; 482: 208
[15] Arrabal R, Matykina E, Skeldon P, Thompson G E.Appl Surf Sci, 2009; 255: 5071
[16] Arrabal R, Pardo A, Merino M C, Mohedano M, Casajús P, Matykina E, Skeldon P, Thompson G E. Corros Sci, 2010; 52: 3738
[17] Hihara L H, Latanision R M.Int Mater Rev, 1994; 39: 245
[18] Trzaskoma P P, McCafferty E, Crowe C R.J Electrochem Soc, 1983; 130: 1804
[19] Pohlman S L.Corrosion, 1978; 34: 156
[20] Turhan M C, Li Q Q, Jha H, Singer R F, Virtanen S.Electrochim Acta, 2011; 56: 7141
[21] Xue W B.Acta Metall Sin, 2006; 42: 350
[21] (薛文斌. 金属学报, 2006; 42: 350)
[22] Wang Y Q, Wang X J, Zhang T, Wu K, Wang F H.J Mater Sci Technol, 2013; 29: 1129
[23] Wang Y Q, Wang X J, Wu K, Wang F H.J Mater Sci Technol, 2013; 29: 267
[24] Wang Y Q, Wang X J, Gong W X, Wu K, Wang F H.Appl Surf Sci, 2013; 283: 906
[25] Liu R, Weng N, Xue W B, Hua M, Liu G J, Li W F. Surf Coat Technol, 2015; 269: 212
Outlines

/

〈 〉