EFFECTS OF N ON CREEP PROPERTIES OF AUSTENI-TIC HEAT-RESISTANT CAST STEELS DEVELOPEDFOR EXHAUST COMPONENT APPLICATIONSAT 1000 ℃
Received date: 2015-12-03
Online published: 2016-03-22
To comply with more stringent environmental and fuel consumption regulations in recent years, automotive gasoline engines equipped with turbochargers are increasingly used to improve fuel efficiency. As a result, exhaust gas temperatures are now reaching 1050 ℃, about 200 ℃ higher than the conventional temperature. Hence, there is an urgent demand in automobile industries to develop novel and economic austenitic heat-resistant steels that are durable against these increased temperatures. In this study, the effects of N addition on creep behavior at 1000 ℃ and 50 MPa are investigated in a series of Nb-bearing austenitic heat-resistant cast steels, which are developed for exhaust component applications. Microstructures before and after creep rupture tests are carefully characterized to illustrate the microstructural evolution during creep deformation. The results of creep tests show approximately an order of magnitude increase in the minimum creep rate among the experimental alloys with variations of N addition. Microstructural analyses indicate that the morphology of NbC and Nb(C, N) is changed from “Chinese-script” to mixed flake-blocks, and then to faceted blocks as N additions increase. The best creep property occurs in an alloy with “Chinese-script” NbC, which could effectively strengthen the grain boundaries and interdendritic regions. The Cr-rich phases are adverse to creep properties, in particular those coarsened and coalesced phases along grain boundaries. They act as crack sources and accelerate the propagation of creep cracks. Moreover, the secondary precipitation of Cr-rich phase results in a significant decrease of C concentration in the matrix and thus reduces the solution strengthening ability during creep deformation. This study suggests that the strengthening of these austenitic cast steels can be achieved through the exploit of primary NbC and Nb(C, N) and the elimination of Cr-rich phases, and therefore, N additions should be strictly controlled.
Yinhui ZHANG , Mei LI , Larry A GODLEWSKI , Jacob W ZINDEL , Qiang FENG . EFFECTS OF N ON CREEP PROPERTIES OF AUSTENI-TIC HEAT-RESISTANT CAST STEELS DEVELOPEDFOR EXHAUST COMPONENT APPLICATIONSAT 1000 ℃[J]. Acta Metall Sin, 2016 , 52(6) : 661 -671 . DOI: 10.11900/0412.1961.2015.00618
| [1] | Takabayashi H, Ueta S, Shimizu T, Noda T.SAE Int J Mater Manuf, 2009; 2: 147 |
| [2] | Wang J X, Shuai S J. Automotive Engine Fundamentals.Beijing: Tsinghua University Press, 2011: 1(王建昕, 帅石金. 汽车发动机原理. 北京: 清华大学出版社, 2011: 1) |
| [3] | Itoh K, Hayashi K, Souda T.Hitachi Met Tech Rev, 2006; 22: 51 |
| [4] | Matsumoto K, Tojo M, Jinnai Y, Hayashi N, Ibaraki S.Mitsubishi Heavy Ind Tech Rev, 2008; 45(3): 1 |
| [5] | Shingledecker J P, Maziasz P J, Evans N D, Pollard M J.Int J Pressure Vessels Piping, 2007; 84: 21 |
| [6] | Maziasz P J, Shingledecker J P, Evans N D, Pollard M J.J Pressure Vessel Technol, 2009; 131: 0514041 |
| [7] | Evans N D, Maziasz P J, Shingledecker J P, Pollard M J.Metall Mater Trans, 2010; 41A: 3032 |
| [8] | Sourmail T.Mater Sci Technol Lond, 2001; 17: 1 |
| [9] | Lo K H, Shek C H, Lai J K L.Mater Sci Eng, 2009; R65: 39 |
| [10] | Yu Y N, Yang P, Qiang W J, Chen L.Foundations of Materials Science. Beijing: High Education Press, 2006: 412(余永宁, 杨平, 强文江, 陈冷. 材料科学基础. 北京: 高等教育出版社, 2006: 412) |
| [11] | Reed R.JOM, 1989; 41(3): 16 |
| [12] | Mujica Roncery L, Weber S, Theisen W.Acta Mater, 2011; 59: 6275 |
| [13] | Knutsen R D, Lang C I, Basson J A.Acta Mater, 2004; 52: 2407 |
| [14] | Hsiao C M. Acta Metall Sin, 1958; 3: 138(萧纪美. 金属学报, 1958; 3: 138) |
| [15] | Yamamoto Y, Brady M P, Santella M L, Bei H, Maziasz P J, Pint B A.Metall Mater Trans, 2011; 42A: 922 |
| [16] | Cutler E R, Wasson A J, Fuchs G E.Scr Mater, 2008; 58: 146 |
| [17] | Elmer J, Allen S, Eagar T.Metall Mater Trans, 1989; 20A: 2117 |
| [18] | Fu H Z, Guo J J, Liu L, Li J S.Directional Solidification and Processing of Advanced Materials. Beijing: Science Press, 2008: 223 |
| [18] | (傅恒志, 郭景杰, 刘林, 李金山. 先进材料定向凝固. 北京: 科学出版社, 2008: 223) |
| [19] | Yong Q L.Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 59 |
| [19] | (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 59) |
| [20] | Lee K M, Cho H S, Choi D C.J Alloys Compd, 1999; 285: 156 |
| [21] | Smith W F, Hashemi J.Foundations of Materials Science and Engineering. 4th Ed., New York: McGraw-Hill Education, 2005: 3 |
| [22] | Zhu S J, Zhao J, Wang F G.Metall Trans, 1990; 21A: 2237 |
| [23] | Ribeiro E A A G, Papaléo R, Guimar?es J R C.Metall Trans, 1986; 17A: 691 |
| [24] | Larson J M, Floreen S.Metall Trans, 1977; 8A: 51 |
| [25] | Zhang J S.High Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 3(张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 3) |
| [26] | Zhang J S, Li P E, Jin J Z.Acta Metall, 1991; 39: 3063 |
| [27] | Rettberg L H, Pollock T M.Acta Mater, 2014; 73: 287 |
| [28] | Min K S, Nam S W.J Nucl Mater, 2003; 322: 91 |
| [29] | Cutler E R, Wasson A J, Fuchs G E.J Cryst Growth, 2009; 311: 3753 |
| [30] | Piekarski B.Mater Charact, 2010; 61: 899 |
| [31] | Zhang Y H, Li M, Godlewski L A, Zindel J W, Feng Q.Metall Mater Trans, 2016; DOI: 10.1007/s11661-016-3544-1, in press |
| [32] | Buchanan K, Kral M.Metall Mater Trans, 2012; 43A: 1760 |
/
| 〈 |
|
〉 |