EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING
Received date: 2015-11-16
Online published: 2016-03-21
Supported by
Supported by Shanghai Science and Technology Committee (No.13DZ1101500) and Tribology Science Fund of State Key Laboratory of Tribology of Tsinghua University (No.SKLT2015A02)
Elevating steam parameters is the key to enhance the efficiency of fossil power plants, reducing fuel consumption and noxious emission. Therefore, a lot of new creep resistant martensitic stainless steels have been developed, among which FB2 steel (a new 9%Cr martensitic stainless steel) is the most promising candidate for manufacturing steam turbine rotors operated at temperature range from 600 ℃ to 650 ℃. In the present work, the evolution behavior of Laves phase in the as received FB2 steel was studied by thermal simulation technique. Firstly, some sparse micron-sized particles of Laves phase were observed in as received FB2 steel by SEM. It was concluded that the large Laves phase particles formed in casting due to dendritic segregation. Then constitutional liquation resulting from eutectic reaction between Laves phase and γ-Fe in the heating process of welding thermal simulation was found, suggesting a liquation crack tendency in heat affected zone of FB2 steel. In the specimens experiencing thermal simulation, some eutectic microstructures were observed by SEM. Based on the results of EDS analysis and SAED, the two eutectic constituents were identified as χ phase and γ-Fe. At last, the reason for the difference in morphology of eutectic microstructures between specimens experiencing thermal simulation with different peak temperatures was analyzed.
Key words: FB2 steel; Laves phase; constitutional liquation; χ ; phase; hot crack tendency; welding
Kejian LI , Zhipeng CAI , Yifei LI , Jiluan PAN . EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING[J]. Acta Metall Sin, 2016 , 52(6) : 641 -648 . DOI: 10.11900/0412.1961.2015.00590
| [1] | Sun R, Cui Z Z, Tao Y.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 1 |
| [2] | Di Gianfrancesco A, Tizzanini A, Jedamzik M, Stolzenberger C.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 9 |
| [3] | Fukuda M, Saito E, Semba H, Iwasaki J, Izumi S, Takano S, Takahashi T, Sumiyoshi Y.In: Grandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 24 |
| [4] | Jara D R.PhD Dissertation, Ruhr University Bochum, 2011 |
| [5] | Mayr P.PhD Dissertation, Graz University of Technology, 2007 |
| [6] | Di Gianfrancesco A, Budano S, Lombardi P, Paura M, Neri S, Calderini M, Longari N.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 304 |
| [7] | Blaes N, Donth B, Bokelmann D.Energy Mater, 2007; 2(4): 207 |
| [8] | Azuma T, Miki K, Tanaka Y, Isshiguro T.Tetsu Hagané, 2002; 88: 678 |
| [8] | (東司, 三木一宏, 田中泰彦, 石黒徹.鉄と鋼, 2002; 88: 678) |
| [9] | Horiuchi T, Igarashi M, Abe F.ISIJ Int, 2002; 42(suppl): S67 |
| [10] | Shige T, Magoshi R, Itou S, Ichimura T, Kondou Y.Mitsubishi Heavy Industry Tech Rev, 2001; 38(1): 6 |
| [11] | Dzugan J, Novy Z, Konopik P, Podany P.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 924 |
| [12] | Xu Y T, Wang M J, Wang Y, Gu T, Chen L, Zhou X, Ma Q, Liu Y M, Huang J.J Alloys Compd, 2015; 621: 93 |
| [13] | Dimmler G, Weinert P, Kozeschnik E, Cerjak H.Mater Charact, 2003; 51: 341 |
| [14] | Cui H R, Sun F, Chen K, Zhang L T, Wan R C, Shan A D, Wu J S.Mater Sci Eng, 2010; A527: 7505 |
| [15] | Korcakova L, Hald J, Somers M.Mater Charact, 2001; 47: 111 |
| [16] | Jandová D, Kasl J, Chvostová E.Mater Sci Forum, 2014; 782: 311 |
| [17] | Kasl J, Jandová D.Mater Sci Forum, 2014; 782: 179 |
| [18] | Brooks J A.Weld J, 1974; 53(suppl): S517 |
| [19] | Ying H Y, Shi C G, Hao C Y, Yu E J, Qin X D, Zhang Q.Acta Metall Sin, 1997; 33: 995 |
| [19] | (应慧筠, 施成根, 郝传勇, 于尔靖, 秦旭东, 张琪. 金属学报, 1997; 33: 995) |
| [20] | Vagi J J, Martin D C.Weld J, 1956; 35(suppl 3): 137s |
| [21] | Kasper J S.Acta Metall, 1954; 2: 456 |
| [22] | Cieslak M J, Ritter A M, Savage W F.Weld J, 1984; 63: 133 |
| [23] | Kautz H R, Gerlach H.Arch Eisenhuttenw, 1968; 39: 151 |
| [24] | Omsen A, Eliasson L.ISIJ Int, 1971; 209: 830 |
| [25] | Weiss B, Stickler R.Metall Trans, 1972; 3A: 851 |
/
| 〈 |
|
〉 |