Orginal Article

EFFECTS OF IN718 GRAIN SIZE ON ULTRASONICBACKSCATTING SIGNALS AND ITS NONDE-STRUCTIVE EVALUATION METHOD

  • Yongfeng SONG ,
  • Xiongbing LI ,
  • Haiping WU ,
  • Jiayong SI ,
  • Xiaoqin HAN
Expand
  • 1 School of Traffic & Transportation Engineering, Central South University, Changsha 410075, China
    2 State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China

Received date: 2015-07-10

  Online published: 2016-03-17

Supported by

Supported by National Natural Science Foundation of China (Nos.61271356 and 51575541), High Technology Research and Development Program of China (No.2012AA03A514), Fundamental Research Funds for the Central Universities (No.2014zzts203) and State Key Laboratory of Powder Metallurgy Foundation (No.2014M562126)

Abstract

Superalloy In718 enjoys wide application in such crucial parts as turbine engine disks due to high strength, great toughness and corrosion resistance in different temperature environment. Since the mechanical properties of superalloy In718 are greatly influenced by the grain size, a nondestructive detection method is studied in order to determine the grain size quickly and effectively. In this work, superalloy In718 samples of different grain sizes were produced and the empirical mode decomposition (EMD) method was employed to find the characteristics of the time-frequency domain of the ultrasonic backscattering signals. Then the effects of the grain size over the intrinsic mode function (IMF) of different frequency bands were analyzed to seek the relations between the grain size and the power of the IMF signals. The original backscattering signals and IMF1 (the first IMF) signals barely respond to the change of the grain size because of their wide frequency bandwidths; the distribution of the frequency domain of the IMF2 signals is centralized and the amplitude of the peak frequency increases with the grain size, and the correlation coefficient between the power and the grain size is 0.995, much higher than that of other modes. This method eliminates the components irrelative to the grain size and takes the IMF2 components which fully reflect the intensity of the grain scattering as the characteristic signals of the grain size evaluation to build an ultrasonic backscattering EMD model evaluating the grain size of superalloy In718. The actual measurement results of the grain size show that the sensitivity of this method is 3.7 times over the traditional backscattering method; the evaluation errors over the two verification test samples are -3.72% and 2.87%, apparently more accurate than the ultrasonic velocity method; compared with the attenuation method, this method requires no information of the thickness so that the evaluation results are independent of the thickness measuring error; compared with the metallographic method, this method is more efficient and requires no damage on the components to be evaluated.

Cite this article

Yongfeng SONG , Xiongbing LI , Haiping WU , Jiayong SI , Xiaoqin HAN . EFFECTS OF IN718 GRAIN SIZE ON ULTRASONICBACKSCATTING SIGNALS AND ITS NONDE-STRUCTIVE EVALUATION METHOD[J]. Acta Metall Sin, 2016 , 52(3) : 378 -384 . DOI: 10.11900/0412.1961.2015.00367

References

[1] Shi C X, Zhong Z Y.Acta Metall Sin, 2010; 11: 1281
[1] (师昌绪, 仲增墉. 金属学报, 2010; 11: 1281)
[2] Zhuang J Y, Du J H, Deng Q, Qu J L, lv X D. The Wrought Superalloys GH4169. Beijing: Metallurgy Industry Press, 2006: 96
[2] (庄景云, 杜金辉, 邓群, 曲敬龙, 吕旭东. 变形高温合金GH4169. 北京: 冶金工业出版社, 2006: 96)
[3] Liu L, Huang T W, Xiong Y H, Yang A M, Zhao Z L, Zhang R, Li J S.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004 Tenth International Symposium. Iowa: AIP Publishing, 2004: 493
[4] Chen L Q, Sui F L, Liu X H.Acta Metall Sin, 2009; 10: 1242
[4] (陈礼清, 隋凤利, 刘相华. 金属学报, 2009; 10: 1242)
[5] Badidi B A, Lebaili S, Benchaala A.NDT&E Int, 2003; 36: 1
[6] Palanichamy P, Joseph A, Jayakumar T, Raj B.NDT&E Int, 1995; 28: 179
[7] Chen Y, Luo Z B, Zhou Q, Zou L J, Lin L.Ultrasonics, 2015; 59: 31
[8] Lynnworth L C.Ultrasonic Measurements for Process Control: Theory, Techniques, Applications. San Diego: Academic Press, 2013: 75
[9] ünal R, Sarpün I H, Yal?m H A, Erol A, ?zdemir T, Tuncel S. Mater Charact, 2006; 56: 241
[10] Aghaie-Khafri M, Honarvar F, Zanganeh S.J Nondestruct Eval, 2012; 31: 191
[11] Li X B, Song Y F, Ni P J, Liu F.Acta Metall Sin, 2015; 51: 121
[11] (李雄兵, 宋永锋, 倪培君, 刘锋. 金属学报, 2015; 51: 121)
[12] Fay B, Brendel K, Ludwig G.Ultrasound Med Biol, 1976; 2(3): 195
[13] Margetan F J.In: Thompson D O, Chimenti D E eds., Review of Progress in Quantitative Nondestructive Evaluation. Iowa: AIP Publishing, 2012: 1430
[14] Panetta P D, Bland L G, Tracy M, Hassan W.In: The Minerals, Metals & Materials Society (TMS) ed., TMS 2014 Annual Meeting Supplemental Proceedings. Hoboken: John Wiley & Sons Inc, 2014: 721
[15] Thompson R B, Gray T A. J Acoust Soc Am, 1983; 74: 1279
[16] Margetan F, Nieters E, Haldipur P, Chiou T.Fundamental Studies of Nickel Billet Materials-Engine Titanium Consortium Phase Ⅱ. Atlantic City: Federal Aviation Administration William J, Hughes Technical Center Press, 2005: 16
[17] Ma S W, Yuan K.J Shanghai Univ (Nat Sci Ed), 2010; 16: 125
[17] (马世伟, 袁康. 上海大学学报(自然科学版), 2010; 16: 125)
[18] Huang N E, Shen S S.Hilbert-Huang Transform and Its Applications. Washington: World Scientific, 2005: 1
[19] Qi H, Azer M, Ritter A.Metall Mater Trans, 2009; 40A: 2410
[20] Du H, Turner J A.Ultrasonics, 2014; 54: 882
Outlines

/

〈 〉