OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS
Received date: 2015-08-21
Online published: 2016-03-17
MnCo2O4 spinel was coated on the surface of SUS 430 alloy by using the sol-gel method. The oxidation kinetics behavior and electrical property of coated SUS 430 alloy in solid oxide fuel cells (SOFCs) cathode atmosphere were investigated. XRD, EDS and SEM were used to characterize the phase structure, surface and cross-section morphology, and composition of the surface oxides; the area specific resistance (ASR) of the surface oxides was measured by using the four-probe direct current technique. The result shows that a 2 μm thick oxide scale, mainly consisting of an inner layer of Mn-Cr spinel and an outer layer of doped Mn-Co spinel, was formed during cyclic oxidation at 750 ℃ in air for 1000 h. The growth of Cr2O3 and Fe2O3 was depressed. The oxidation kinetics obeys the parabolic law with two rate constants 3.74×10-15 g2/(cm4s)(0~200 h) and 7.06×10-15 g2/(cm4s) (200~1000 h), respectively, which is 1 order of magnitude lower than that of the SUS 430 alloy without coating. The ASR is in the range of 5.21~22.65 mΩcm2 at 600~800 ℃. MnCo2O4 coating was proved to be effective in enhancing the oxidation resistance and electrical property of SUS 430 alloy.
Wenying ZHANG , Jun LI , Bo ZHOU . OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS[J]. Acta Metall Sin, 2016 , 52(3) : 355 -360 . DOI: 10.11900/0412.1961.2015.00449
| [1] | Yang Z G.Int Mater Rev, 2008; 53: 39 |
| [2] | Zhu W Z, Deevi S C.Mater Res Bull, 2003; 38: 957 |
| [3] | Fergus J W.Mater Sci Eng, 2005; A397: 271 |
| [4] | Toji A, Uehara T.ECS Trans, 2007; 7: 2117 |
| [5] | Han M F, Peng S P, Wang Z L, Yang Z B, Chen X.J Power Sources, 2007; 164: 278 |
| [6] | Pu J, Li J, Hua B, Xie G Y.J Power Sources, 2006; 158: 354 |
| [7] | Stanislowski M, Wessel E, Hilpert K, Markus T, Singheiser L.J Electrochem Soc, 2007; 154: A295 |
| [8] | Tucker M C, Kurokawa H, Jacobson C P, De Jonghe L C, Visco S J.J Power Sources, 2006; 160: 130 |
| [9] | Shaigan N, Qu W, Ivey D G, Chen W.J Power Sources, 2010; 195: 1529 |
| [10] | Qu W, Li J, Ivey D G, Hill J M.J Power Sources, 2006; 157: 335 |
| [11] | Oishi N, Namikawa T, Yamazaki Y.Surf Coat Technol, 2000; 132(1): 58 |
| [12] | Roure S, Czerwinski F, Petric A.Oxid Met, 1994; 42(1~2): 75 |
| [13] | Johnson C, Gemmen R, Orlovskaya N.Compos Part Eng, 2004; 35B: 167 |
| [14] | Chu C, Wang J, Lee S.Int J Hydrogen Energy, 2008; 33: 2536 |
| [15] | Yang Z, Xia G, Maupin G D, Stevenson J W.J Electrochem Soc, 2006; 153: A1852 |
| [16] | Shaigan N, Ivey D G, Chen W.J Power Sources, 2008; 183: 651 |
| [17] | Qu W, Jian L, Hill J W, Ivey D G.J Power Sources, 2006; 153: 114 |
| [18] | Wei W, Chen W, Ivey D G.J Power Sources, 2009; 186: 428 |
| [19] | Hua B, Pu J, Gong W, Zhang J F, Lu F S, Jian L.J Power Sources, 2008; 185: 419 |
| [20] | Bateni M R, Wei P, Deng X, Petric A.Surf Coat Technol, 2007; 201: 4677 |
| [21] | Hua B, Zhang J F, Lu F S, Kong Y H, Pu J, Li J.Acta Metall Sin, 2009; 45: 605 |
| [21] | (华斌, 张建福, 卢凤双, 孔永红, 蒲健, 李箭. 金属学报, 2009; 45: 605) |
| [22] | Shannon R D. Acta Cryst, 1976; 32A: 751 |
| [23] | Li J, Pu J, Hua B, Xie G Y.J Power Sources, 2006; 159: 641 |
| [24] | Quadakkers W J, Piron-Abellan J, Shemet V.Mater High Temp, 2003; 20: 115 |
/
| 〈 |
|
〉 |