Orginal Article

CORROSION BEHAVIOR OF PIPELINE STEEL UNDER DEPOSIT CORROSION AND THE INHIBITION PERFORMANCE OF ORGANIC PHOSPHINE INHIBITOR

  • Yunze XU ,
  • Yi HUANG ,
  • Liang YING ,
  • Fei YANG ,
  • Bing LI ,
  • Xiaona WANG
Expand
  • 1 School of Naval Architecture Engineering, Dalian University of Technology, Dalian 116024, China
    2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
    3 School of Physics and Optoelectronic Engineering, Dalian University of Technology, Dalian 116024, China

Received date: 2015-06-23

  Online published: 2016-03-17

Supported by

Supported by National Science and Technology Pillar Program During the Twelfth Five-Year Plan Period (No.2011ZX05056), China Postdoctoral Science Foundation (No.2014M561223) and Fundamental Research Funds for the Central Universities (No DUT15YQ36)

Abstract

Localized corrosion such as pitting and mesa attack caused by the presence of solid deposits on a metal surface is defined as under deposit corrosion (UDC). UDC is frequently observed in oil and gas transition pipelines where sand, debris biofilm and carbonate deposit are present. Studies have found that the introduction of oxygen would accelerate the galvanic corrosion behavior between the deposit covered area and the area without deposit. Some experiments have been carried out and demonstrated that high concentration inhibitor should be used for the migration of UDC. However, the inhibition effect of the organic phosphonic inhibitor for UDC is rare in the previous studies. In this work, the evaluation of UDC behavior of X65 pipeline steel and the performance of corrosion inhibitor Ethylene Diamine Tetra (Methylene Phosphonic Acid) Sodium (EDTMPS) in the oxygen contained solutions are studied by using polarization dynamic scan (PDS), electrochemical impedance spectra (EIS) and linear polarization resistance (LPR) methods. The galvanic effect caused by the deposit is studied by using wire beam electrode (WBE). The measurement results show that the corrosion rate of deposit-covered electrode is lower than that of bare electrode, but localized corrosion is observed on the deposit-covered steel surface. After 35 mg/L EDTMPS is introduced into the solution, the corrosion rate of the bare steel decreased from 0.17 mm/a to 0.082 mm/a and the corrosion rate of the deposit covered electrode decreased from 0.051 mm/a to 0.026 mm/a. Protective films are observed on both deposit covered steel surface and bare steel surface after EDTMPS added. In the galvanic corrosion monitoring experiment by using WBE, the under deposit area has a lower potential and performs as the anodic area with serious localized corrosion. After 35 mg/L EDTMPS is injected, the average potential begins to decrease. The maximum anodic current density and the total anodic current respectively decrease from 0.21 mA/cm2 and 0.056 mA to 0.078 mA/cm2 and 0.021 mA. The electrochemical measurement results reveal that EDTMPS has an excellent inhibition effect for the corrosion of both bare electrode and deposit covered electrode. The WBE test illustrates that EDTMPS also has an inhibition effect on the galvanic corrosion caused by the covering deposit. However, EDTMPS cannot completely prevent the localized corrosion behavior on WBE surface.

Cite this article

Yunze XU , Yi HUANG , Liang YING , Fei YANG , Bing LI , Xiaona WANG . CORROSION BEHAVIOR OF PIPELINE STEEL UNDER DEPOSIT CORROSION AND THE INHIBITION PERFORMANCE OF ORGANIC PHOSPHINE INHIBITOR[J]. Acta Metall Sin, 2016 , 52(3) : 320 -330 . DOI: 10.11900/0412.1961.2015.00327

References

[1] Zhang X Y, Di C, Chen Z Y, Wang F P, Du Y L.Corros Sci Prot Technol, 1999; 11: 279
[1] (张学元, 邸超, 陈卓元, 王凤平, 杜元龙. 腐蚀科学与防护技术, 1999; 11: 279)
[2] de Reus J A M, Hendriksen E L J A, Wilms M E, Al-Habsi Y N, Durnie W H, Gough M A. Corrosion 2005, Houston: NACE, 2005: 05288
[3] Xu Y Z, Huang Y, Wang X N, Lin X Q.Sens Actuators, 2016; 224B: 37
[4] Sun C, Sun J B, Wang Y, Wang S J, Liu J X.Acta Metall Sin, 2014; 50: 811
[4] (孙冲, 孙建波, 王勇, 王世杰, 刘建新. 金属学报, 2014; 50: 811)
[5] Gao Q Y, Zhang J J, Yang Z G, Yang D M, Liu J N, Zang H Y, Zhu Y Y, Zhang T.Sci Technol Rev, 2014; 32(24): 35
[5] (高秋英, 张江江, 杨祖国, 羊东明, 刘冀宁, 臧晗宇, 朱原原, 张涛. 科技导报, 2014; 32(24): 35)
[6] Jeannin M, Calonnec D, Sabot R, Refait P.Corros Sci, 2010; 52: 2026
[7] Tan Y, Fwu Y, Bhardwaj K.Corros Sci, 2011; 53: 1254
[8] Pandarinathan V, Lepková K, Bailey S I, Gubner R.Corros Sci, 2013; 72: 108
[9] Pandarinathan V, Lepková K, Bailey S I, Gubner R. J Electrochem Soc, 2013; 160: C432
[10] Cheng H P, Wang D J.Corros Prot Petrochem Ind, 2014; 31(1): 46
[10] (程海鹏, 王东江. 石油化工腐蚀与防护, 2014; 31(1): 46)
[11] Jia H L, Zhao C P, Wang H, Jiang S, Fei X S.Pipe Tech Equip, 2013; (3): 51
[11] (贾恒磊, 赵春平, 汪浩, 姜姝, 费雪松. 管道技术与设备, 2013; (3): 51)
[12] Machuca L L, Murray L, Gubner R, Bailey S I.Mater Corros, 2014; 65: 8
[13] Sawford M K, Ateya B G, Abdullah A M, Pickering H W.J Electrochem Soc, 2002; 149: B198
[14] Ya-Chiao C, Woollam R, Orazem M E.J Electrochem Soc, 2014; 161: C321
[15] Pandarinathan V, Lepková K, Bailey S I, Gubner R.Corrosion 2011, Houston: NACE, 2011: 11261
[16] Zhang G A, Yu N, Yang L Y, Guo X P.Corros Sci, 2014; 86: 202
[17] Pedersen A, Bilkova K, Gulbrandsen E, Kvarekval J.Corrosion 2008, Houston: NACE, 2008: 08632
[18] Huang Y, Xu Y, Li B, Ying L, Yang F, Wang X.Corros Eng Sci Technol, DOI: 10.1179/1743278215Y.0000000047
[19] Dong Z H, Shi W, Guo X P.Acta Phys-Chim Sin, 2011; 27: 127
[19] (董泽华, 石维, 郭兴蓬. 物理化学学报, 2011; 27: 127)
[20] Aung N N, Tan Y J.Corros Sci, 2004; 46: 3057
[21] Tan Y J, Aung N N.Mater Corros, 2014; 65: 457
[22] Varela F, Tan M Y, Forsyth M.Corros Eng Sci Technol, 2015; 50: 226
[23] Belayachi M, Serrar H, Zarrok H, El Assyry A, Zarrouk A, Oudda
[23] H, Boukhris S, Hammouti B, Ebenso E E, Geunbour A.Int J Electrochem Sci, 2015; 10: 3010
[24] Zhang B R, Zhang L, Li F T, Hu W, Hannam P M.Corros Sci, 2010; 52: 3883
[25] Liu L S.Shanxi Chem Ind, 2009; 29(3): 38
[25] (刘丽莎. 山西化工, 2009; 29(3): 38)
[26] Zou Y, Wang J, Zheng Y Y.Corros Sci, 2011; 53: 208
[27] Orlikowski J, Darowicki K, Mikołajski S.Sens Actuators, 2013; 181B: 22
[28] Jiang S H, Xu J W.Shandong Chem Ind, 2013; 42(12): 9
[28] (蒋守红, 徐杰武. 山东化工, 2013; 42(12): 9)
[29] Cao C N.Principles of Electrochemistry of Corrosion. 3rd Ed., Beijing: Chemical Industry Press, 2008: 175
[29] (曹楚南. 腐蚀电化学原理. 第三版, 北京: 化学工业出版社, 2008: 175)
[30] Stern M, Geary A L.J Electrochem Soc, 1957; 104: 56
[31] Peng X, Wang J, Shan C, Wang H J, Liu Z J, Zou Y.Acta Metall Sin, 2012; 48: 1260
[31] (彭欣, 王佳, 山川, 王海杰, 刘在健, 邹妍. 金属学报, 2012; 48: 1260)
[32] Tan Y J.Corros Sci, 2011; 53: 1145
Outlines

/

〈 〉