Orginal Article

COMPUTATIONAL STUDY ON MICROSTRUCTURE-SENSITIVE HIGH CYCLE FATIGUE DISPERSIVITY

  • Shiwei HAN ,
  • Duoqi SHI ,
  • Xiaoguang YANG ,
  • Guolei MIAO
Expand
  • 1) School of Energy and Power Engineering, Beihang University, Beijing 100191, China
    2) the Collaborative Innovation Center for Advanced Aero-Engine (CICAAE), Beijing 100191, China;

Received date: 2015-06-23

  Online published: 2016-03-17

Abstract

Empirical approaches to characterize the variability of high cycle fatigue have been widely used. However, little is understood about the intrinsic relationship of randomness of microstructure attributes on the overall variability in high cycle fatigue. The ability of quantifying the dispersivity of high cycle fatigue with physics based computational methods has great potential in design of minimum life and can aid in the improvement of fatigue resistance. To investigate the effects between microstructure attributes and high cycle fatigue dispersivity, the microstructure-sensitive extreme value probabilistic framework is introduced. First, the Voronoi algorithm is used to construct random polycrystalline microstructure representative volume elements. Different kinds of periodic boundary conditions are proposed to simulate the interior and surface constraints in polycrystalline microstructure representative volume elements. Then mechanical responses of both interior and surface microstructure representative volume elements under different strain amplitudes are simulated by internal state variable based crystal plasticity. The fatigue indicator parameter is introduced to characterize the driving force for fatigue crack formation dominated by maximum shear plastic strain amplitude. By computing a limited number of random polycrystalline microstructure representative volume elements, the distributions of fatigue indicator parameter under different strain amplitudes are obtained and analyzed with extreme value probability theory. The study with a kind of titanium alloy with material grade TC4 supports that the high cycle fatigue dispersivity increases with the decrease of the strain amplitude, especially under elastic limit. The extreme value of fatigue indicator parameter from random polycrystalline microstructure representative volume elements correlates well with the Gumbel extreme value distribution. Besides, the lower the average stress under different strain amplitudes, the fewer grains in polycrystalline microstructure representative volume element yield. Moreover, the grains on surface tend to have higher probability to initiate fatigue cracks and lower dispersivity in fatigue crack formation.

Cite this article

Shiwei HAN , Duoqi SHI , Xiaoguang YANG , Guolei MIAO . COMPUTATIONAL STUDY ON MICROSTRUCTURE-SENSITIVE HIGH CYCLE FATIGUE DISPERSIVITY[J]. Acta Metall Sin, 2016 , 52(3) : 289 -297 . DOI: 10.11900/0412.1961.2015.00322

References

[1] Cowles B A. Int J Fracture, 1989; 80: 147
[2] Przybyla C P.PhD Dissertation, Georgia Institute of Technology, USA, 2010
[3] Tucker J C, Cerrone A R III, Ingraffea A R, Rollett A D.Modell Simul Mater Sci Eng, 2015; 23: 1
[4] McDowell D L, Dunne F P E.Int J Fatigue, 2010; 32: 1521
[5] McDowell D L.Int J Plast, 2010; 26: 1280
[6] Przybyla C P, McDowell D L.Int J Plast, 2010; 26: 372
[7] Przybyla C P, McDowell D L.Acta Mater, 2012; 60: 293
[8] Przybyla C, Prasannavenkatesan R, Salajegheh N, McDowell D L.Int J Fatigue, 2010; 32: 512
[9] Bridier F, McDowell D L, Villechaise P, Mendez J.Int J Plast, 2009; 25: 1066
[10] Castelluccio G M.PhD Dissertation, Georgia Institute of Technology, USA, 2012
[11] Musinski W D.PhD Dissertation, Georgia Institute of Technology, USA, 2014
[12] Zhang M, Zhang J, McDowell D L.Int J Plast, 2007; 23: 1328
[13] Zhang M.PhD Dissertation, Georgia Institute of Technology, USA, 2018
[14] Mu Y W, Lu S.Acta Aeroet Astro Sin, 2013; 34: 282
[14] (牟园伟, 陆山. 航空学报, 2013; 34: 282)
[15] Tanaka K, Mura T.J Appl Mech, 1981; 48: 97
[16] Sharaf M, Kucharczyk P, Vajragupta N, Munstermann S, Hartmaier A, Blech W.Comput Mater Sci, 2014; 94: 258
[17] China Aeronatical Material Manual Editorial Board. China Aeronautical Material Manual. Vol.4, Beijing: China Standard Press, 2002: 104
[17] (中国航空材料手册编委会. 中国航空材料手册. 第4卷, 北京: 中国标准出版社, 2002: 104)
[18] Quey R, Dawson P R, Barbe F.Comput Methods Appl Mech Eng, 2011; 20: 1729
[19] Peirce D, Asaro R J, Needleman A.Acta Metall, 1982; 30: 1087
[20] Asaro R J.Adv Appl Mech, 1983; 23: 1
[21] Peirce D, Asaro R J, Needleman A.Acta Metall, 1983; 31: 1951
[22] Lee E H.J Appl Mech, 1969; 36: 1
[23] Rice J R.J Mech Phys Solids, 1971; 19: 433
[24] Roters F, Eisenlohr P, Hantcherli L, Tjahjanto D D, Bieler T R, Raabe D.Acta Mater, 2010; 58: 1152
[25] Fatemi A, Socie D F.Fatigue Fract Engng Mater Struct, 1988; 11: 146
[26] Bennett V P, McDowell D L. Mixed-Mode Crack Behavior. Pennsylvania: American Society for Testing and Materials, 1999: 203
[27] Gumbel E J.Statistics of Extremes. New York: Columbia University Press, 1958: 1
[28] Lütjering G, Williams J C.Titanium. Verlag Berlin Heidelberg: Springer, 2003: 202
Outlines

/