Orginal Article

STUDY ON SHAPE CORRECTION OF THE THIN PLATE OF TA15 TITANIUM ALLOY BY POST WELD HEAT TREATMENT

  • Yongkui LI ,
  • Chunyi QUAN ,
  • Shanping LU ,
  • Qingyang JIAO ,
  • Shijian LI ,
  • Zhonghai SUN
Expand
  • 1 Shenyang National Laboratory of Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 AVIC Shenyang Aircraft Corporation, Shenyang 110034, China

Received date: 2015-06-15

  Online published: 2016-03-17

Abstract

Weld deformation of the thin-wall weldment used in fighter aircraft not only hinders its subsequent procedure of fabrication and assembling, but also reduces its fatigue strength. As a result, weld deformation shortens its service life essentially. Dustpan deformation is always produced in the thin-wall weldment after multiple-pass weld. In this work, combining with the experiment, the finite element method was adopted to analysis the deformation of the thin-wall weldment by multiple-pass weld and its shape correction by post weld heat treatment. For obtaining the fundamental properties such as thermal parameters and mechanical parameters of TA15 titanium alloy, a series of experiments were conducted at room temperature and high temperatures. Additionally, creep behaviors of TA15 titanium alloy were studied at the temperatures of 500, 550, 600, 650, 700 and 750 ℃, and the parameters of creep constitutive equations of the alloy were obtained with considering the analysis of post weld heat treatment. A thermal coupled temperature-displacement analysis for welding and post weld heat treatment was performed on a three dimensional shell model of protective grille. Experiments of multiple-pass weld and post weld heat treatment were used to testify the reliability of the finite element model of welding and post weld heat treatment. With using the reliable finite element model, the parameters of heat treatment were studied. The study indicates that, the fabrication on the crossing of structure section and fillet after fillet-wallboard weld leads the compression deformation release along the fillet, after that, the shrinkage distortion produced during spot welding of fillet-structural section mainly contributes the large dustpan deformation of the thin-wall weldment; increasing temperatures, enlarging loads and prolonging the hold time can improve the shape correction of the thin-wall weldment during post weld heat treatment, hence the guide maps of the post weld heat treatment for shape correction of the thin-wall weldment under 700 and 750 ℃ are worked out.

Cite this article

Yongkui LI , Chunyi QUAN , Shanping LU , Qingyang JIAO , Shijian LI , Zhonghai SUN . STUDY ON SHAPE CORRECTION OF THE THIN PLATE OF TA15 TITANIUM ALLOY BY POST WELD HEAT TREATMENT[J]. Acta Metall Sin, 2016 , 52(3) : 281 -288 . DOI: 10.11900/0412.1961.2015.00314

References

[1] Li X W, Sha A X, Zhang W F, Chu J P, Ma J M.Titanium Ind Prog, 2003; 20(4-5): 90
[1] (李兴无, 沙爱学, 张旺峰, 储俊鹏, 马济民. 钛工业进展, 2003; 20(4-5): 90)
[2] Chen L, Gong S L, Yao W, Hu J L.China Weld, 2004; 13: 1
[3] Wang L F, Liu J Z, Hu B R.Trans China Weld Inst, 2007; 28(1): 97
[3] (王利发, 刘建中, 胡本润. 焊接学报, 2007; 28(1): 97)
[4] McClung R C.Fatigue Frat Eng Mater Struct, 2007; 30: 173
[5] Wang Y H, Li Y, Zhang W F, Ma J M.Chin J Nonferrous Met, 2010; 20: 641
[5] (王玉会, 李艳, 张旺峰, 马济民. 中国有色金属学报, 2010; 20: 641)
[6] Li J.PhD Dissertation, Beijing University of Technology, 2004
[6] (李菊. 北京工业大学博士学位论文, 2004)
[7] Guo S Q, Xu W L, Liu X S, Tian X T.Trans China Weld Inst, 1999; 20(1): 34
[7] (郭绍庆, 徐文立, 刘雪松, 田锡唐. 焊接学报, 1999; 20(1): 34)
[8] Li J, Yang J G, Weng L L, Fang H Y.Trans China Weld Inst, 2008; 29(11): 25)
[8] (李军, 杨建国, 翁路露, 方洪渊. 焊接学报, 2008; 29(11): 25)
[9] Liu X S, Xu W L, Fang H Y.Trans China Weld Inst, 2004; 25(2): 84
[9] (刘雪松, 徐文立, 方洪渊. 焊接学报, 2004; 25(2): 84)
[10] Adamus K, Kucharczyk Z, Wojsyk K, Kudla K.Comput Mater Sci, 2013; 77: 286
[11] Zhang Y, Yang J G, Liu X S, Fang H Y. Niu J, Zhou G T Eds., Physical and Numerical Simulation of Material Processing. Stafa-Zurich: Trans Tech Publications Ltd, 2012: 739
[12] Liu X S, Ji S D, Fang H Y.Trans Nonferrous Met Soc China, 2005; 15: 101
[13] Li J, Guan Q, Guo D L, Sun Y C, Du Y X, Shi Y W.J Mech Strength, 2003; 25: 637
[14] Li Y.Mach Des Manuf, 2002; (1): 86
[14] (李友. 机械设计与制造, 2002; (1): 86)
[15] Yan X J, Ge Y L.J Mater Eng Perform, 2014; 23: 3474
[16] Wanjara P, Dalgaard E, Gholipour J, Cao X J, Cuddy J, Jonas J J.Metall Mater Trans, 2014; 45A: 5138
[17] Hao C Y, Li Z L, Mao X F.Acta Metall Sin, 2001; 37: 709
[17] (郝传勇, 李正林, 毛先锋. 金属学报, 2001; 37: 709)
[18] Hu G, Li J W, Fu G, Mao Z Y.Aerospe Manuf Technol, 2005; (4): 1
[18] (胡刚, 李晋炜, 付纲, 毛智勇. 航天制造技术, 2005; (4): 1)
[19] Zhang W F, Wang Y H, Li Y, Ma J M.Chin J Nonferrous Met, 2010; 20: 523
[19] (张旺峰, 王玉会, 李艳, 马济民. 中国有色金属学报, 2010; 20: 523)
[20] Li Y K, Hongo H, Tabuchi M, Takahashi Y, Monma Y.Int J Press Vessels Pip, 2009; 86: 585
[21] Li Y K, Kaji Y, Igarashi T.Nucl Eng Des, 2012; 242: 100
[22] Pavelic V, Tanbakuchi R, Uyehara O, Myers P.Weld J, 1969; 48: 295
[23] Li Y K, Chen J D, Lu S P.Acta Metall Sin, 2014; 50: 121
[23] (李永奎, 陈俊丹, 陆善平. 金属学报, 2014; 50: 121)
[24] Wang Z C.Trans China Weld Inst, 2000; 21(2): 55
[24] (王者昌. 焊接学报, 2000; 21(2): 55)
[25] Wang J H, Lu H.Trans China Weld Inst, 2002; 23(3): 75
[25] (汪建华, 陆皓. 焊接学报, 2002; 23(3): 75)
[26] Cao J X, Fang B, Huang X, Li Z X.Chin J Rare Met, 2004; 28: 362
[26] (曹京霞, 方波, 黄旭, 李臻熙. 稀有金属, 2004; 28: 362)
Outlines

/