EFFECT OF Fe-RICH PHASE PARTICLES WITH DIFFER-ENT CONCENTRATIONS ON THE BENDABILITYOF Al-Mg-Si-Cu SERIES ALLOYS
Received date: 2015-04-14
Online published: 2016-03-17
Supported by
Supported by National High Technology Research and Development Program of China (No.2013-AA032403), National Natural Science Foundation of China (Nos.51571023 and 51301016), Fundamental Research Funds for the Central Universities (NoFRF-TP-15-051A3) and Constructed Project for Key Laboratory of Beijing (No FRF-SD-B-005B)
The influence of Fe-rich phase particle with different contents on the bendability of the Al-Mg-Si-Cu alloys was investigated by means of bending and tensile tests, OM, SEM and TEM characterization. The results reveal that, with the increase of Fe-rich phase particle content, the bendability of the alloy sheets in the longitudinal and transverse directions was quite different, and the outer surface of the alloy sheets after bending of 180° along the two directions became much rough, especially along the transverse direction. When the Fe-rich phase concentration increased to the medium level (0.2%Fe), the quality of outer surface after bending was very good. With further increasing Fe-rich phase to the high level (0.5%Fe), micro cracks were produced after bending along the transverse direction. Although increasing Fe-rich phase concentration did not give a great effect on the elongation of the alloys in the two directions, according to the tensile fracture and microstructure in the slid surface of the specimen after bending or tension test, the roughening of outer surface of the alloy sheet without Fe-rich phase was closely related with the formation of shear bands, while for the alloy sheet with high concentration of Fe-rich phases, the formation of micro cracks after bending was mainly related with the size, morphology and distribution of coarse Fe-rich phases. In addition, based on the quantitative relationship between Fe-rich phase concentration and bendability of the alloy sheets, the models of outer surface roughening and micro cracks forming during bendingare proposed.
Key words: Al-Mg-Si-Cu alloy; Fe-rich phase; bendability; shear band; modelling
Hui XING , Mingxing GUO , Xiaofeng WANG , Yan ZHANG , Jishan ZHANG , Linzhong ZHUANG . EFFECT OF Fe-RICH PHASE PARTICLES WITH DIFFER-ENT CONCENTRATIONS ON THE BENDABILITYOF Al-Mg-Si-Cu SERIES ALLOYS[J]. Acta Metall Sin, 2016 , 52(3) : 271 -280 . DOI: 10.11900/0412.1961.2015.00220
| [1] | Miller W S, Zhuang L, Bottema J, Wittebrood A J, De Smet P, Haszler A, Vieregge A.Mater Sci Eng, 2000; A280: 37 |
| [2] | Wang D.Shanghai Nonferrous Met, 2013; 34(3): 130 |
| [2] | (王丹. 上海有色金属, 2013; 34(3): 130) |
| [3] | Wang M J, Huang D Y, Jiang H T.Heat Treatment Met, 2006; (09): 34 |
| [3] | (王孟君, 黄电源, 姜海涛. 金属热处理, 2006; (09): 34) |
| [4] | Sun J.Tech Educ, 2010; (02): 26 |
| [4] | (孙静. 技术与教育, 2010; (02): 26) |
| [5] | Liu Y W, Wang S W.Auto Engineer, 2011; (02): 50 |
| [5] | (刘伟燕, 王书伟. 汽车工程师, 2011; (02): 50) |
| [6] | Zhang Q X, Guo M X, Hu X Q, Cao L Y, Zhuang L Z, Zhang J S.Acta Metall Sin, 2013; 49: 1604 |
| [6] | (张巧霞, 郭明星, 胡晓倩, 曹零勇, 庄林忠, 张济山. 金属学报, 2013; 49: 1604) |
| [7] | Cui L, Guo M X, Peng X Y, Zhang Y, Zhang J S, Zhuang L Z.Acta Metall Sin, 2015; 51: 289 |
| [7] | (崔莉, 郭明星, 彭祥阳, 张艳, 张济山, 庄林忠. 金属学报, 2015; 51: 289) |
| [8] | Wang A D. Master Thesis, Dalian University of Technology, 2011 |
| [8] | (王安东. 大连理工大学硕士学位论文, 2011) |
| [9] | Wang X F, Guo M X, Cao L Y, Luo J R, Zhang J S, Zhuang L Z.Mater Sci Eng, 2015; A621: 8 |
| [10] | Sarkar J, Kutty T R G, Wilkinson D S, Embury J D, Lloyd D J.Mater Sci Eng, 2004; A369: 258 |
| [11] | Itoh G, Suzuki T, Horikawa K. Mater Sci Forum, 2002; 396-402: 1193 |
| [12] | Hirth S M, Marshall G J, Court S A, Lloyd D J. Mater Sci Eng, 2001; A319-321: 452 |
| [13] | Datsko J, Yang C T.J Eng Ind, 1960; 82: 309 |
| [14] | Davidkov A, Petrov R H, Smet P D, Schepers B, Kestens L A I.Mater Sci Eng, 2011; A528: 7068 |
| [15] | Castany P, Diologent F, Rossoll A, Despois J F, Bezen?on C, Mortensen A.Mater Sci Eng, 2013; A559: 558 |
| [16] | Mulazimoglu M, Zaluska A, Gruzleski J, Paray F.Metall Mater Trans, 1996; 27A: 929 |
| [17] | Allen C M, O'Reilly K A Q, Cantor B, Evans P V.Prog Mater Sci, 1998; 43: 89 |
| [18] | Tanihata H, Sugawara T, Matsuda K, Ikeno S.J Mater Sci, 1999; 34: 1205 |
| [19] | Couper M J, Rinderer B, Yao J Y. Mater Sci Forum, 2006; 519-521: 303 |
| [20] | Peng X Y, Guo M X, Wang X F, Cui L, Zhang J S, Zhuang L Z.Acta Metall Sin, 2015; 51: 169 |
| [20] | (彭祥阳, 郭明星, 汪小锋, 崔莉, 张济山, 庄林忠. 金属学报, 2015; 51: 169) |
| [21] | Wang X F, Guo M X, Chapuis A, Luo J R, Zhang J S, Zhuang L Z.Mater Sci Eng, 2015; A644: 137 |
| [22] | Lievers W B, Pilkey A K, Worswick M J.Mech Mater, 2003; 35: 661 |
| [23] | Lloyd D J, Weatherly G C, Perovic D D.In: Subodh K Das ed., Proceedings of Symposium: Automotive Alloys 1999, San Diego: TMS, 2000: 211 |
| [24] | Lv D. Master Thesis, Lanzhou University of Technology, 2009 |
| [24] | (吕丹. 兰州理工大学硕士学位论文, 2009) |
| [25] | Fan X G.PhD Dissertation, Harbin Institute of Technology, 2007 |
| [25] | (樊喜刚. 哈尔滨工业大学博士学位论文, 2007) |
/
| 〈 |
|
〉 |