Orginal Article

PREDICTION OF THE SOLIDIFICATION PATH OF Al-6.32Cu-25.13Mg ALLOY BY A UNIFIED MICROSEGREGATION MODEL COUPLED WITH THERMO-CALC

  • Erhu YAN ,
  • Lixian SUN ,
  • Fen XU ,
  • Daming XU
Expand
  • 1 School of Materials Science and Engineering, Guilin University of Electronic Technology, Guilin 541004, China
    2 School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China

Received date: 2015-09-18

  Online published: 2016-03-16

Supported by

Supported by National Natural Science Foundation of China (No.51361005), Natural Science Foundation of Guangxi Province (Nos.2015GXNSFBA139208, 2014GXNSFDA118005 and UF14023Y) and Guangxi Key Laboratory of Information Materials (No.1210908-217-Z)

Abstract

The solidification path of alloy reveals the detailed relationship between the solute concentration in liquid and the temperature during the solidification process. The best and most accurate method to predict the solidification path of multicomponent/multiphase alloys is to establish proper microsegregation modeling coupled with phase diagram calculations according to the CALPHAD method. Recently, several alloy systems such as Al-Cu, Al-Mg and Cu-Mg have been developed, which have aroused the interest of many researchers. Up to now, the research about Al-Cu-Mg ternary alloy, especially containing higher Mg content, is relatively rare. The purpose of the present work is to investigate the solidification path of Al-6.32Cu-25.13Mg (mass fraction, %) ternary eutectic alloy at different cooling rates and solid back diffusion coefficients by an extended unified microsegregation model coupled with Thermo-Calc. Solidification experiments and subsequent microstructural characterization are combined with numerical calculation of solidification paths. It was shown that the cooling rates Rf had no obvious effect on the solidification path which was (L+α)→(L+α+T)→(L+α+β+T); but the solid back diffusion coefficient Φ had a great effect on the solidification path, which evolved gradually from (L+α)→(L+α+T)→(L+α+β+T) into (L+α)→(L+α+T) when Φ increased from 0 to 1. The volume fractions of primary α phase Vα, binary eutectic V2E and ternary eutectic V3E at each solidification path were calculated. It was shown that V2E decreased with the increase of Rf whereas V3E increased and Vα was almost invariant. The dependence of V2E, V3E and Rf were determined by linear regression analysis given as: V2E=-2.5lgRf+64.9, V3E=2.5lgRf+22.12. The increase in Φ led to increases in Vα and V2E and decrease in V3E. The predicted solidification paths and volume fractions of Al-6.32Cu-25.13Mg ternary eutectic alloy at different cooling rates were in good agreement with experimental results.

Cite this article

Erhu YAN , Lixian SUN , Fen XU , Daming XU . PREDICTION OF THE SOLIDIFICATION PATH OF Al-6.32Cu-25.13Mg ALLOY BY A UNIFIED MICROSEGREGATION MODEL COUPLED WITH THERMO-CALC[J]. Acta Metall Sin, 2016 , 52(5) : 632 -640 . DOI: 10.11900/0412.1961.2015.00492

References

[1] Djordje M, Joachim G, Rainer S F.Acta Mater, 2008; 56: 5214
[2] Dou K, Qing J S, Wang L, Zhang X F, Wang B, Liu Q, Dong H B.Acta Metall Sin, 2014; 50: 1505
[2] (窦坤, 卿家胜, 王雷, 张晓峰, 王宝, 刘青, 董洪标. 金属学报, 2014; 50: 1505)
[3] Wang N, Li C R, Du Z M.Acta Metall Sin, 2008; 44: 1111
[3] (王娜, 李长荣, 杜振民. 金属学报, 2008; 44: 1111)
[4] Zhang W B, Sha C S, Du Y, Wen G H, Xie W, Wang S Q.Acta Metall Sin, 2011; 47: 1307
[4] (张伟彬, 沙春生, 杜勇, 温光华, 谢文, 王社权. 金属学报, 2011; 47: 1307)
[5] Mehrabian R, Flemings M C.Metall Trans, 1970; 1B: 455
[6] Gao Q N, Wang J, Shang S L, Liu S H, Du Y, Liu Z.Calphad, 2014; 47: 196
[7] Feng H, Zhang M, Chen H M, Liang J L, Tao X M, Ouyang Y H, Du Y.J Phase Equilib Diff, 2014; 35: 256
[8] Chen F Y, Jie W Q.Acta Metall Sin, 2003; 39: 597
[8] (陈福义, 介万奇. 金属学报, 2003; 39: 597)
[9] Yoo H, Kim C J.Int J Heat Mass Transfer, 1998; 30: 3268
[10] Roósz A, Exner H E.Acta Matall Mater, 1990; 38: 375
[11] Xie F Y, Kraft T, Zuo Y, Moon C H, Chang Y A.Acta Metall Sin (Engl Lett), 1999; 2: 489
[12] Kraft T, Rettenmayr M, Exner H E.Modell Simul Mater Sci Eng, 1996; 4: 161
[13] Zhao G W, Xu D M, Fu H Z.Int J Mater Res, 2008; 99: 680
[14] Brooks J A, Baskes M I, Greulich F A.Metall Trans, 1991; 22A: 915
[15] Flemings M C, Brody H D.Trans Metall Soc AIME, 1966; 236: 615
[16] Clyne T W, Kurz W.Metall Trans, 1981; 12A: 965
[17] Ohnaka I.Trans Iron Steel Inst Jpn, 1986; 26:1045
[18] Kobayashi S.Trans Iron Steel Inst Jpn, 1988; 28: 728
[19] Nastac L, Stefanescu D M.Metall Trans, 1993; 24A: 2107
[20] Larouche D.Calphad, 2007; 31: 490
[21] Du Q, Eskin D G, Katgerman L.Calphad, 2008; 32: 478
[22] Hao D, Hu B, Zhang K, Zhang L J, Du Y.J Mater Sci, 2014; 49: 1157
[23] Chen F Y, Jie W Q.Acta Metall Sin, 2004; 40: 664
[23] (陈福义, 介万奇. 金属学报, 2004; 40: 664)
[24] Zhao G W, Li X Z, Xu D M, Guo J J, Du Y, He Y H.Calphad, 2012; 36: 155
[25] Buhler T, Fries S G, Spencer P J, Lukas H L.J Phase Equilib, 1998; 19: 317
[26] Xu D M.Metall Mater Trans, 2001; 32B: 1129
[27] Yan E H, Li X Z, Rettenmayr M, Liu D M, Su Y Q, Guo J J, Xu D M, Fu H Z.Int J Hydrogen Energy, 2014; 39: 3505
[28] Xu D M.Metall Mater Trans, 2002; 33B: 451
[29] Xu D M, Fu H Z, Guo J J, Jia J, Li Q C.J Harbin Inst Technol, 2003; 35: 1156
[29] (徐达鸣, 傅恒志, 郭景杰, 贾钧, 李庆春. 哈尔滨工业大学学报, 2003; 35:1156)
[30] Zhao G W, Xu D M, Song M H, Fu H Z, Du Y, He Y H.Acta Metall Sin, 2009; 45: 956
[30] (赵光伟, 徐达鸣, 宋梦华, 傅恒志, 杜勇, 贺跃辉. 金属学报, 2009; 45: 956)
[31] Wang Z, Wang F Z, He Y H, Wang X, Ma S, Wang H M.Acta Metall Sin, 2014; 50: 1393
[31] (王哲, 王发展, 何银花, 王欣, 马姗, 王辉绵. 金属学报, 2014; 50: 1393)
[32] Nishida Y, Aiga F, Itoh S.J Cryst Growth, 2014; 405: 110
[33] Flemings M C. Solidification Processing.New York: McGraw-Hill Book Co NY, 1974: 134
[34] Kurz W, Fisher D J.Fundamentals of Solidification. Lausanne, Switzerland: Trans Tech Publications, 1989: 68
[35] Singh S N, Bardes B P, Flemings M C.Metall Trans, 1970; 1: 1383
Outlines

/

〈 〉