Orginal Article

MICROSTRUCTURE AND WEAR RESISTANCE OF TiAlZrCr/(Ti, Al, Zr, Cr)N GRADIENT FILMS DEPOSITED BY MULTI-ARC ION PLATING

  • Shilu ZHAO ,
  • Zhen ZHANG ,
  • Jun ZHANG ,
  • Jianming WANG ,
  • Zhenggui ZHANG
Expand
  • 1 School of Mechanical Engineering, Shenyang University, Shenyang 110044, China
    2 BMW Brilliance Automotive Ltd., Shenyang 110143, China

Received date: 2015-10-08

  Online published: 2016-03-10

Supported by

Supported by Natural Science Foundation of Liaoning Province (No.2014020096), Shenyang Science and Technology Plan Project (No.F14-231-1-19) and Shenyang Yongyuan Guanghui Machinery Factory Transverse Project (No.201521010100051)

Abstract

Nowadays, the cutting tools are exposed to much more severe operating conditions, i.e. high cutting speed, high feed rate, aggressive mechanical and thermal loading. As a result, the existing hard films have frequently encountered wear-related failures. Such situation requires the new generation hard films concurrently displaying superior hardness, excellent adhesive strength and outstanding wear resistance. Previous studies have demonstrated some promising mechanical properties (hardness and adhesion strength) of TiAlZrCr/(Ti, Al, Zr, Cr)N quaternary gradient films as compared to those of the (Ti, Al)N binary and (Ti, Al, Zr)N or (Ti, Al, Cr)N trinary nitride films. However, the research on wear resistance of hard films under the conditions of high speed and dry friction has been seldom reported. In this work, using combined Ti-Al-Zr alloy and pure Cr targets, TiAlZrCr/(Ti, Al, Zr, Cr)N quaternary nitride films were deposited on high speed steel W18Cr4V substrates by multi-arc ion plating (MAIP) process at various bias voltages of -50, -100, -150 and -200 V. Surface morphology and crystalline struc ture of the gradient films were analyzed by SEM and XRD. Wear resistance of the films was evaluated by abrasion tester at both ambient (15 ℃) and elevated (500 ℃) temperatures. The worn surface morphology was then investigated by SEM. The results show that the deposited TiAlZrCr/(Ti, Al, Zr, Cr)N quaternary nitride films exhibited TiN-type (fcc-NaCl type) structure. The films have uniform and dense columnar morphologies. Furthermore, it was confirmed that the primary wear mechanism was adhesive wear (caused by plastic deformation) accompanied by a slight abrasion. The average values of friction coefficient varied at 0.25~0.30 at ambient temperature and 0.30~0.35 at elevated temperature, respectively. Finally, the best wear resistance was achieved when the bias voltage increased to -200 V.

Cite this article

Shilu ZHAO , Zhen ZHANG , Jun ZHANG , Jianming WANG , Zhenggui ZHANG . MICROSTRUCTURE AND WEAR RESISTANCE OF TiAlZrCr/(Ti, Al, Zr, Cr)N GRADIENT FILMS DEPOSITED BY MULTI-ARC ION PLATING[J]. Acta Metall Sin, 2016 , 52(6) : 747 -754 . DOI: 10.11900/0412.1961.2015.00522

References

[1] Mitsuo A, Uchida S, Nihira N, Iwaki M. Surf Coat Technol, 1998; 103-104: 98
[2] Zhang S H, Wang L, Wang Q M, Li M X.Surf Coat Technol, 2013; 214: 160
[3] Zhao S L, Zhang J, Liu C S.Acta Metall Sin (Engl Lett), 2010; 23: 473
[4] Chang Z K, Xiao J Q, Chen Y Q, Liu S C, Gong J, Sun C.Acta Metall Sin, 2012; 48: 547
[4] (常正凯, 肖金泉, 陈育秋, 刘山川, 宫骏, 孙超. 金属学报, 2012; 48: 547)
[5] Yousaf M I, Pelenovich V O, Yang B, Liu C S, Fu D J.Surf Coat Technol, 2015; 265: 117
[6] Du G Y, Ba D C, Tan Z, Sun W, Liu K, Han Q K.Surf Coat Technol, 2013; 229: 172
[7] Sheng Y L, Sheng C W, Jen S C, Jow L H.Surf Coat Technol, 2007; 202: 977
[8] Fox-rabinovich G S, Beake B D, Yamamoto K, Aguirre M H, Veldhuis S C, Dosbaeva G, Elfizy A, Biksa A, Shuster L S.Surf Coat Technol, 2010; 204: 3698
[9] Xu Y X, Chen L, Yang B, Peng Y B, Du Y, Feng J C, Pei F.Surf Coat Technol, 2013; 235: 506
[10] Yang S M, Chang Y Y, Lin D Y, Wang D Y, Wu W.Surf Coat Technol, 2008; 202: 2176
[11] Shi J, Pei Z L, Gong J, Sun C, Muders C M, Jiang X.Acta Metall Sin, 2012; 48: 1349
[11] (时婧, 裴志亮, 宫骏, 孙超, Muders C M, 姜辛. 金属学报, 2012; 48: 1349)
[12] Tetsuhide S, Hidetoshi K, Tomotaro W, Yoshikazu T, Hiroshi N, Kazuo M, Ming Y.Surf Coat Technol, 2014; 250: 44
[13] Xu J H, Ju H B, Yu L H.Acta Metall Sin, 2012; 48: 1132
[13] (许俊华, 鞠洪博, 喻利花. 金属学报, 2012; 48: 1132)
[14] Niu Y S, Wei J, Yu Z M.Surf Coat Technol, 2015; 275: 332
[15] Zhang M, Kim K H, Xu F F, Yang X X. Surf Coat Technol, 2013; 228(S1): S529
[16] Mori T, Noborisaka M, Watanabe T, Suzuki T.Surf Coat Technol, 2012; 213: 216
[17] Gao J, Li C R, Wang N, Du Z M.Int J Miner Metall Mater, 2008; 15: 420
[18] Wang B Y, Li Z X, Yan P, Du J H.Rare Met Mater Eng, 2008; 37: 1407
[18] (王宝云, 李争显, 严鹏, 杜继红. 稀有金属材料与工程, 2008; 37: 1407)
[19] Weber F R, Fontaine F, Scheib M, Bock W. Surf Coat Technol, 2004; 177-178: 227
[20] Chang Y Y, Lai H M.Surf Coat Technol, 2014; 259: 152
[21] Musil J, Daniel R.Surf Coat Technol, 2003; 166(2-3): 243
[22] Zhao S L, Zhang J, Chen W H, Wang S H.Chin J Vaccum Sci Technol, 2013; 33: 214
[22] (赵时璐, 张钧, 陈卫华, 王双红. 真空科学与技术学报, 2013; 33: 214)
[23] Zhao S L, Zhang J, Zhang Z, Wang S H, Zhang Z G.Int J Miner Metall Mater, 2014; 21: 77
[24] Zhao S L, Zhang J, Chen W H, Wang S H.Rare Met Mater Eng, 2014; 43: 341
[24] (赵时璐, 张钧, 陈卫华, 王双红. 稀有金属材料与工程, 2014; 43: 341)
[25] Xu J H, Wang X, Ma S L, Liu Y, Xu K W.Chin J Mater Res, 2008; 22: 201
[25] (徐建华, 王昕, 马胜利, 刘阳, 徐可为. 材料研究学报, 2008; 22: 201)
[26] Zhao S L.PhD Dissertation, Northeastern University, Shenyang, 2010
[26] (赵时璐. 东北大学博士学位论文, 沈阳, 2010)
Outlines

/