Abstract

The service environment faced by marine equipment and its key friction pair parts are much more severe than that on land surface. The life cycle and safety of the hydraulic and power transmission system, which directly get in touch with the seawater, depends largely on the tribological behavior of the components in the seawater. Titanium alloy is an ideal material used for ocean engineering, however due to its poor friction performance its life cycle may be shortened when working in the environment with friction and wear. In order to improve the tribological performance of titanium alloy in seawater, laser processing was used to build super hydrophobic with grid and dot micro-structure on Ti6Al4V alloy surface. Tribological performance was evaluated by HSR-2M high speed reciprocating friction test machine in artificial seawater, and compared with in water (distilled water). The results show that the friction coefficients and wear losses (volume) of super hydrophobic Ti6Al4V alloy surface are significantly smaller than that of the Ti6Al4V alloy substrate. The friction coefficients of surface with dot and grid reduced by 17.8% and 11.7%, and wear losses (volume) reduced by 36.8% and 57.5% respectively in artificial seawater. The friction coefficient of super hydrophobic Ti6Al4V alloy surface in artificial seawater is smaller than that in water while the wear loss has the opposite phenomena. The tribological performances of titanium alloy in artificial seawater are significantly improved by the build of super hydrophobic Ti6Al4V alloy surface.

Cite this article

Feng LIAN , Luping ZANG , Qiukuan XIANG , Huichen ZHANG . TRIBOLOGICAL PERFORMANCE OF SUPER HYDRO-PHOBIC TITANIUM ALLOY SURFACE INARTIFICIAL SEAWATER[J]. Acta Metall Sin, 2016 , 52(5) : 592 -598 . DOI: 10.11900/0412.1961.2015.00342

References

[1] Guo F, Wang Y X, Xue Q J, Wang L P.J Tribol, 2014; 34: 608
[1] (郭峰, 王永欣, 薛群基, 王立平. 摩擦学学报, 2014; 34: 608)
[2] Cui G J, Bi Q L, Zhu S Y, Yang J, Liu W M.Tribol Int, 2012; 53: 76
[3] Wang Z T, Zhou X H, Zhao G G.Trans Nonferrous Met Soc China, 2008; 18: 831
[4] Feng S R, Tang H B, Zhang S Q, Wang H M.Trans Nonferrous Met Soc China, 2012; 22: 1667
[5] Zaveri N, Mahapatra M, Deceuster A, Peng Y, Li L J, Zhou A H.Electrochim Acta, 2008; 53: 5022
[6] Zhong H S, Li J L, Wang Y X, Wang L P, Xue Q J.J Vac Sci Technol, 2014; 34: 961
[6] (钟华生, 李金龙, 王永欣, 王立平, 薛群基. 真空科学与技术学报, 2014; 34: 961)
[7] Deng K, Yu M, Dai Z D, Liang J, Zhang G A, Liu W M.Rare Met Mater Eng, 2014; 43: 1099
[7] (邓凯, 于敏, 戴振东, 梁军, 张广安, 刘维民. 稀有金属材料与工程, 2014; 43: 1099)
[8] Xi J M, Feng L, Jiang L.Appl Phys Lett, 2008; 92: 53101
[9] Burton Z, Bhushan B.Ultramicroscopy, 2006; 106: 709
[10] Mehdi S, Ahmet T A.Appl Surf Sci, 2009; 256: 710
[11] Wan Y, Wang Z Q, Liu Y F.J Inorg Mater, 2012; 27: 390
[11] (万勇, 王中乾, 刘义芳. 无机材料学报, 2012; 27: 390)
[12] Wang H Y, Meng Y, Zhao J Y, Zhu Y J.J Mater Eng, 2014; (3): 90
[12] (汪怀远, 孟旸, 赵景岩, 朱艳吉. 材料工程, 2014; (3): 90)
[13] Thieme M, Streller F, Simon F, Frenzel R, White A J.Appl Surf Sci, 2013; 283: 1041
[14] Jung Y C, Bhushan B.Nanotechnology, 2006; 17: 4970
[15] Wang S T, Feng L, Jiang L.Appl Surf Sci, 2006; 18: 767
[16] Liang J S, Liu K Y, Wang D Z, Li H, Li P F, Li S Z, Su S J, Xu S C, Luo Y.Appl Surf Sci, 2015; 338: 126
[17] Kang Z X, Guo M J.Acta Metall Sin, 2013; 49: 629
[17] (康志新, 郭明杰. 金属学报, 2013; 49: 629)
[18] Lin Y Z, Wang T C.J Shandong Univ Sci Technol (Nat Sci), 2008; 27(2): 44
[18] (林跃忠, 王铁成. 山东科技大学学报(自然科学版), 2008; 27(2): 44)
[19] Zhang H, Lamb R, Lewis J.Sci Technol Adv Mater, 2005; 6: 236
[20] Cassie A B D, Baxter S.Trans Faraday Soc, 1944; 40: 546
[21] Xia F, Jiang L.Adv Mater, 2008; 20: 2842
[22] Wen S Z. Nano Tribology.Beijing: Tsinghua University Press, 1998: 103
[22] (温诗铸. 纳米摩擦学. 北京: 清华大学出版社, 1998: 103)
[23] Wang J H, Song M, Li J L, Wang X B.Tribology, 2011; 31: 118
[23] (王建华, 宋敏, 李金龙, 王晓波. 摩擦学学报, 2011; 31: 118)
[24] Chen J, Yan F Y.Trans Nonferrous Met Soc China, 2012; 22: 1356
[25] Ding H Y, Dai Z D.Tribology, 2008; 28: 139
[25] (丁红燕, 戴振东. 摩擦学学报, 2008; 28: 139)
Outlines

/

〈 〉