Orginal Article

ELEMENT LOSS OF AZ91D MAGNESIUM ALLOY DURING SELECTIVE LASER MELTING PROCESS

  • Kaiwen WEI ,
  • Zemin WANG ,
  • Xiaoyan ZENG
Expand
  • 1 School of Optical and Electronic Information, Huazhong University of Science and Technology, Wuhan 430074, China
    2 Wuhan National Laboratory of Optoelectronics, Huazhong University of Science and Technology, Wuhan 430074, China

Received date: 2015-04-13

  Online published: 2016-02-25

Supported by

Supported by National Natural Science Foundation of China (No.51075164), High Technology Research and Development Program of China (No.2013AA031606) and Fundamental Research Funds for the Central Universities (NoHUST-2014QT006)

Abstract

Magnesium alloys have attracted more attentions due to their low densities and excellent specific strengths. However, proper manufacturing methods are still needed to promote further applications of magnesium alloys due to the shortcomings of conventional processing methods. As one of the most promising additive manufacturing technologies, selective laser melting (SLM) was utilized to process the most commonly-used AZ91D magnesium alloy in this work. Element vaporization mechanism during the forming process and the influence of element vaporization on chemical composition, microstructure, and mechanical properties of the final products were investigated using OM, SEM, EDS, XRF and XRD. The results show that the relative content of Mg in the SLM-processed samples (86.61%~88.68%) was lower than that in the original AZ91D powders (90.63%) , whereas the relative content of Al in the former ones (10.40%~12.56%) was higher than its counterpart in the latter ones (8.97%). This variation matches well with the calculation by Langmuir model, demonstrating that element vaporization of AZ91D mainly targets at Mg. With the increase of laser energy density (EV), weight ratio of Mg to Al (η) in the SLM-processed samples first increased, then decreased and finally tended to be constant. η of the sample prepared at 55.6 J/mm3 (sample No.8) presented a smallest difference with that of the original powders. A model illustrating analytic relationship between η and EV was established by mathematical regression with the fitting index R2 being 0.858. The sample processed at 166.7 J/mm3 (sample No.1) underwent one of the most remarkable compositional variation and exhibited a typical solidified microstructure similar to the die-cast AZ91D in which net-like β-Mg17Al12 precipitates were distributed around the α-Mg matrix. However, β-Mg17Al12 content as well as solid solubility of Al in α-Mg matrix was much higher in sample No.1. The enhanced tensile strength and micro-hardness as well as the deteriorated elongation of sample No.1 could be attributed to the composition variation during SLM process.

Cite this article

Kaiwen WEI , Zemin WANG , Xiaoyan ZENG . ELEMENT LOSS OF AZ91D MAGNESIUM ALLOY DURING SELECTIVE LASER MELTING PROCESS[J]. Acta Metall Sin, 2016 , 52(2) : 184 -190 . DOI: 10.11900/0412.1961.2015.00212

References

[1] Mordike B L, Ebert T.Mater Sci Eng, 2001; A302: 37
[2] Wang Y X, Fu J W, Wang J, Luo T J, Dong X G, Yang Y S.Acta Metall Sin, 2011; 47: 410
[2] (王亚霄, 付俊伟, 王晶, 罗天骄, 董旭光, 杨院生. 金属学报, 2011; 47: 410)
[3] Frank W.Acta Biomater, 2010; 6: 1680
[4] Zhen R, Sun Y S, Bai J, Sun J J, Pi J H.Acta Metall Sin, 2012; 48: 733
[4] (甄睿, 孙扬善, 白晶, 孙晶晶, 皮锦红. 金属学报, 2012; 48: 733)
[5] Kulekci M K.Int J Adv Manuf Technol, 2008; 39: 851
[6] Blawert C, Hort N, Kainer K U.Trans Indian Inst Met, 2004; 57: 397
[7] Zheng Y F, Gu X N, Li N, Zhou W R.Mater Chin, 2011; 30(4): 30
[7] (郑玉峰, 顾雪楠, 李楠, 周维瑞. 中国材料进展, 2011; 30(4): 30)
[8] Rashid R A R, Sun S J, Wang G, Dargusch M S.Int J Pr Eng Man, 2013; 14: 1263
[9] Zhang X H, Jiang J F, Luo S J.Chin J Nonferrous Met, 2009; 19: 1720
[9] (张晓华, 姜巨福, 罗守靖. 中国有色金属学报, 2009; 19: 1720)
[10] Zhang J L, Feng Z Y, Hu L Q, Wang S B, Xu B S.Acta Metall Sin, 2012; 48: 607
[10] (张金玲, 冯芝勇, 胡兰青, 王社斌, 许并社. 金属学报, 2012; 48: 607)
[11] Li Q, Li Z F, Li Y F, Luo S J, Gao X R.Foundry, 2008; 57: 895
[11] (李强, 李周复, 李远发, 罗守靖, 高小荣. 铸造, 2008; 57: 895)
[12] Wu L, Zhu H T, Gai X Y, Wang Y Y.J Prosthet Dent, 2014; 111: 51
[13] Ma M M, Wang Z M, Gao M, Zeng X Y.J Mater Process Technol, 2015; 215: 142
[14] Gu D D, Hagedorn Y C, Meiners W, Meng G B, Batista R J S, Wissenbach K, Poprawe R.Acta Mater, 2012; 60: 3849
[15] Gu D D, Shen Y F, Lu Z J.Mater Lett, 2009; 63: 1577
[16] Liu S H, Liu J L, Liu H, Duan Y W, Quan W W.Laser Technol, 2010; 34: 459
[16] (刘顺洪, 柳家良, 刘辉, 段元威, 权雯雯. 激光技术, 2010; 34: 459)
[17] Kolodziejczak P, Kalita W.J Mater Process Technol, 2009; 209: 1122
[18] Guan K, Wang Z M, Gao M, Li X Y, Zeng X Y.Mater Des, 2013; 50: 581
[19] Wang Z M, Guan K, Gao M, Li X Y, Chen X F, Zeng X Y.J Alloys Compd, 2012; 513: 518
[20] Block-Bolten A, Eagar T W.Metall Mater Trans, 1984; 15B: 461
[21] Khan P A A, Debroy T.Metall Mater Trans, 1984; 15B: 641
[22] Gale W F, Totemeier T C.Smithells Metals Reference Book. 8th Ed., Oxford, UK: Elsevier, 2004: 8
[23] Abderrazak K, Bannour S, Mhiri H, Lepalec G, Autric M.Comp Mater Sci, 2009; 44: 858
[24] Yadroitsev I, Yadroitsava I, Bertrand P, Smurov I.Rapid Prototyping J, 2012; 18: 201
[25] Kouadri A, Barrallier L.Mater Sci Eng, 2006; A429: 11
[26] Min D, Shen J, Lai S Q, Chen J, Xu N, Liu H.Opt Laser Eng, 2011; 49: 89
[27] Dargusch M S, Pettersen K, Nogita K, Nave M D, Dunlop G L.Mater Trans, 2006; 47: 977
[28] Dahle A K, Lee Y C, Nave M D, Schaffer P L, StJohn D H.J Light Met, 2001; 1: 61
[29] Wahba M, Mizutani M, Kawahito Y, Katayama S.Mater Des, 2012; 33: 569
[30] Niknejad S T, Liu L, Nguyen T, Lee M Y, Esmaeili S, Zhou N Y.Metall Mater Trans, 2013; 44A: 3747
[31] Wang Z M, Gao M, Tang H G, Zeng X Y.Mater Charact, 2011; 62: 943
[32] Liu L M.Welding and Joining of Magnesium Alloys. Cambridge, UK: Woodhead Publishing, 2010: 51
[33] Zhang G J, Long S Y, Cao F H.Spec Cast Nonferrous Alloys, 2009; 29: 848
[33] (张广俊, 龙思远, 曹凤红. 特种铸造及有色合金, 2009; 29: 848)
Outlines

/

〈 〉