Orginal Article

EFFECT OF SOLID SOLUTION TREATMENT ONMICROSTRUCTURE AND MECHANICALPROPERTIES OF HOT-PRESS CoCrW ALLOYS

  • Xiaohong YOU ,
  • Ganggang WANG ,
  • Jun WANG ,
  • Tao XU ,
  • Hongyu ZHANG ,
  • Hua WEI
Expand
  • 1 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030000, China
    2 Military Representative Office in Factory, Xi'an 710077, China
    3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-05-03

  Online published: 2016-02-25

Supported by

Supported by National Natural Science Foundation of China (No.51201161)

Abstract

Co-based alloy has high strength, good corrosion and wear resistance, and is widely used in aviation industry, nuclear industry. The cast Co-based alloys has high hardness brittleness, but the toughness is low, which limits its wide use. The CoCrW alloy prepared by powder metallurgy process has high toughness, at the same time, the mechanical properties of the CoCrW alloy can be changed by heat treatment. In this work, the effect of solid solution treatment on the microstructure and mechanical properties of the hot pressed alloy was studied by SEM, XRD and TEM, hardness test, room-temperature tensile and wear experiment. The results show that the microstructure of the as-hot pressed and solid solution state CoCrW alloy are both composed of M23C6, M6C, CrCo intermetallic compounds and γ-Co matrix, the contents of M23C6 and prior particle boundaries decrease remarkably after solution treatment, meanwhile, the toughness and wear resistance of the alloy are improved. With the increase of solid solution temperature and time, the hardness and tensile strength at room temperature of CoCrW alloys in crease first and then decrease.

Cite this article

Xiaohong YOU , Ganggang WANG , Jun WANG , Tao XU , Hongyu ZHANG , Hua WEI . EFFECT OF SOLID SOLUTION TREATMENT ONMICROSTRUCTURE AND MECHANICALPROPERTIES OF HOT-PRESS CoCrW ALLOYS[J]. Acta Metall Sin, 2016 , 52(2) : 161 -167 . DOI: 1011900/0412.1961.2015.00245

References

[1] Kuzucu V, Ceylan M, Celik H, Aksoy I.J Mater Process Technol, 1997; 69: 257
[2] Lemarie E, Calvar M L.Wear, 2001; 249: 338
[3] Otterloo J D, Hosson J D.Acta Mater, 1997; 45: 1225
[4] Ashworth M A, Bryar J C, Jacobs M H, Davies S.Powder Metall, 1999; 42: 243
[5] Ahmed R, Ashraf A, Elameen M, Faisal N F, El-Sherik A M, Elakwah Y O, Goosen M F A.Wear, 2014; 312: 70
[6] Northwood D O.Mater Des, 1985; 6: 58
[7] Frenk A, Kurz W.Wear, 1994; 174: 81
[8] Crook P.Adv Mater Process, 1994; 145: 27
[9] Sims C T, Stoloff N S, Hagel W C. Superalloys II. New York: Wiley, 1987: 140
[10] Fu Z M, Song K J.Chinese Sci Bull, 1987; 5: 390
[10] (傅祖明, 宋科匠. 科学通报, 1987; 5: 390)
[11] Yu H, Ahmed R, Lovelock H D.In: Davies S ed., Proc World Congress Eng 2007, Vol II, London: Newswood Limited, 2007: 435
[12] Malayoglu U, Neville A.Wear, 2003; 255: 181
[13] Malayoglu U, Neville A.Wear, 2005; 259: 219
[14] Huang P Y. Powder Metallurgy Principle.2nd Ed., Beijing: Metallurgical Industry Press, 2006: 331
[14] (黄培云. 粉末冶金原理. 第2版, 北京: 冶金工业出版社, 2006: 331)
[15] Ahmed R, Lovelock H D, Davies S, Faisal N H.Tribol Int, 2013; 57: 8
[16] Jiang W H, Guan H R, Hu Z Q.Mater Sci Eng, 1999; A271: 101
[17] Larson J M.In: Hausner H H, Smith W E eds., Proc 1973 Int Pow der Metall Conf, Berlin: Springer, 1974: 537
[18] Wallace W, Dunthorne H B, Sprague R A.Can Metall Quart, 1974; 13: 517
[19] Kear K H.In: Hausner H H ed., Proc 1970 Int Powder Metally Conf, Berlin: Springer, 1971: 85
[20] Guo W M, Wu J T, Zhang F G, Zhao M H.J Iron Steel Res Int, 2006; 13(5): 65
[21] Rao G A, Kumar M, Srinivas M, Sarma D S.Mater Sci Eng, 2003; A355: 114
[22] Mao J, Yang W H, Wang W X, Zou J W, Zhou R F.Acta Metall Sin, 1993; 29: 187
[22] (毛健, 杨万宏, 汪武祥, 邹金文, 周瑞发. 金属学报, 1993; 29: 187)
[23] Prakash T L, Tewari S N.In: Ramakrishnan P ed., Powder Metall Related High Temperature Materials. Zurich: Trans Tech Publications, 1985: 402
[24] Wu C F, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J.Acta Metall Sin, 2009; 45: 1013
[24] (吴朝锋, 马明星, 刘文今, 钟敏霖, 张伟明, 张红军. 金属学报, 2009; 45: 1013)
[25] John R, David F.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Champion: TMS, 2004: 381
Outlines

/