CORROSION BEHAVIOR OF ALLOY 800 IN NaOH AND ETA SOLUTIONS AT 300 ℃

  • Jiazhen WANG ,
  • Jianqiu WANG ,
  • En-Hou HAN
Expand
  • Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-09-19

  Online published: 2016-02-04

Supported by

Supported by National Key Science and Technology Project of China (No.2011ZX06004-009) and National Basic Research Program of China (No.2011CB610500)

Abstract

Many components in secondary side of pressurized water reactors (PWRs) are made of carbon steels and low alloy steels. The corrosion products produced by the flow accelerated corrosion (FAC) of these components can deposite on the surface of steam generator (SG) tubes and decrease the heat transfer efficiency of SG tubes. Moreover, the enrichment of foreign ions (e.g. Cl- and Pb2+) occurs with the sedimentation of corrosion products and causes the local environment degradation, and thus accelerates the failure of SG tubes. In order to decrease the FAC of carbon steels and low alloy steels, pH controllers are often added to adjust the pH value of secondary water. The water chemistry environment of secondary side in PWRs has experienced various treatment techniques, such as phosphate treatment, all volatile treatment (AVT), morpholine (MPH) treatment, ethanolamine (ETA) treatment, and boric acid treatment. In comparision with AVT, ETA can significantly reduce the concentration of Fe in the steam-water phase region and water supply system because of its higher alkalinity and lower molar concentration in feedwater. Due to the high resistance to corrosion and stress corrosion cracking in high temperature and high pressure water, alloy 800 is often used as steam generator tubes in nuclear power plants and thus becomes increasingly attractive among researchers. However, few studies focus on the effect of ETA on the corrosion behavior of alloy 800 in high temperature and high pressure water. This work mainly aims to investigate the corrosion behavior of alloy 800 in NaOH and ETA solutions at 300 ℃ by potentiodynamic polarization curve, electrochemical impedance spectra (EIS), SEM and XPS. The electrochemical results demonstrate that the addition of ETA decreases the current density of anodic and cathodic reactions, and increases the corrosion potential of alloy 800. Besides, ETA addition significantly increases the resistance of inner oxide layer and makes the oxide film more compact, which increases the film resistance of alloy 800 in high temperature water. Through the morphology observation and composition analysis, it is found that ETA addition can promote the formation of Cr-rich layer and increase the ratio of chromium in the oxide films although the deposition of magnetite is enhanced on the surface of alloy 800. For stainless steels and nickel-based alloys in high temperature water, the Cr-rich oxide layer can inhibit the diffusion process of O and metal ions, and reduces the corrosion rates of alloys. Therefore, the corrosion resistance of alloy 800 is enhanced after ETA is added in high temperature water.

Cite this article

Jiazhen WANG , Jianqiu WANG , En-Hou HAN . CORROSION BEHAVIOR OF ALLOY 800 IN NaOH AND ETA SOLUTIONS AT 300 ℃[J]. Acta Metall Sin, 2016 , 52(5) : 599 -606 . DOI: 10.11900/0412.1961.2015.00490

References

[1] Staehle R W, Gorman J A.Corrosion, 2003; 59: 931
[2] Li X H.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012
[2] (郦晓慧. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
[3] Pandey M D, Datla S, Tapping R L, Lu Y C.Nucl Eng Des, 2009; 239: 1862
[4] Sui G, Titchmarsh J M, Heys G B, Congleton J.Corros Sci, 1997; 39: 565
[5] Ziemniak S E, Guilmette P A, Turcotte R A, Tunison H M.Corros Sci, 2008; 50: 449
[6] Le Canut J M, Maximovitch S, Dalard F. J Nucl Mater, 2004; 334: 13
[7] Wang J Q, Li X H, Huang F, Zhang Z M, Wang J Z, Staehle R W.Corrosion, 2014; 70: 598
[8] Huang F, Wang J Q, Han E-H, Ke W.Corros Sci, 2013; 76: 52
[9] Staehle R W, Gorman J A.Corrosion, 2004; 60: 115
[10] Staehle R W, Gorman J A.Corrosion, 2004; 60: 5
[11] Shutikov A V, Ivanov V N, Tyapkov V F, Yerpylyova S F, Bykova V V.Therm Eng, 2008; 55: 402
[12] Tao J. Master Thesis, Shanghai Jiaotong University, 2005
[12] (陶钧. 上海交通大学硕士学位论文, 2005)
[13] Li Q. Master Thesis, Harbin Engineering University, 2005
[13] (李强. 哈尔滨工程大学硕士学位论文, 2005)
[14] Zhu Z P, Zhao Y F, Zhou Y, Guo X C, Deng Y P.Corros Sci Prot Technol, 2012; 24: 285
[14] (朱志平, 赵永福, 周瑜, 郭小翠, 邓奕鹏. 腐蚀科学与防护技术, 2012; 24: 285)
[15] Wang J Z, Wang J Q.J Mater Sci Technol, 2015; 31: 1039
[16] Macdonald D D, Scott A C, Wentrcek P. J Electrochem Soc, 1979; 126: 908
[17] Jonscher A K.Phys Status Solidi, 1975; 32A: 665
[18] Liu X H, Wu X Q, Han E-H.Acta Metall Sin, 2014; 50: 64
[18] (刘侠和, 吴欣强, 韩恩厚. 金属学报, 2014; 50: 64)
[19] Bénézeth P, Wesolowski D, Palmer D, Machesky M.J Solution Chem, 2009; 38: 925
[20] Turner C W, Klimas S J.Reprot, TR-108004, Palo Alto: EPRI, 1997
[21] Turner C W, Guzonas D D, Klimas S J.Reprot, TR-110083, Palo Alto: EPRI, 1999
[22] Sui G, Titchmarsh J M, Heys G B, Congleton J.Corros Sci, 1997; 39: 565
[23] Machet A, Galtayries A, Marcus P, Combrade P, Jolivet P, Scott P.Surf Interface Anal, 2002; 34: 197
[24] Robertson J.Corros Sci, 1991; 32: 443
[25] Dieckmann R, Mason T O, Hodge J D, Schmalzried H.Ber Bunsenges Physik Chem, 1978; 82: 778
[26] Dieckmann R.Solid State Ionics, 1984; 12: 1
[27] Calinski C, Strehblow H H.J Electrochem Soc, 1989; 136: 1328
[28] Zhang Z M, Wang J Q, Han E-H, Ke W.Corros Sci, 2011; 53: 3623
[29] Huang F, Wang J Q, Han E-H, Ke W.J Mater Sci Technol, 2012; 28: 562
[30] Machet A, Galtayries A, Zanna S, Klein L, Maurice V, Jolivet P, Foucault M, Combrade P, Scott P, Marcus P.Electrochim Acta, 2004; 49: 3957
[31] Biesinger M C, Brown C, Mycroft J R, Davidson R D, McIntyre N S.Surf Interface Anal, 2004; 36: 1550
[32] Pratt A R, McIntyre N S.Surf Interface Anal, 1996; 24: 529
[33] Sun H, Wu X Q, Han E-H.Corros Sci, 2009; 51: 2840
[34] Sun H, Wu X Q, Han E-H.Corros Sci, 2009; 51: 2565
[35] Huang J B, Wu X Q, Han E-H.Corros Sci, 2010; 52: 3444
[36] Liu X H, Wu X Q, Han E-H.Corros Sci, 2011; 53: 3337
[37] Stellwag B.Corros Sci, 1998; 40: 337
Outlines

/

〈 〉