DEGENERATION PROCESS AND MECHANISM OF PRIMARY MC CARBIDES IN A CAST Ni-BASED SUPERALLOY

  • Wen SUN ,
  • Xuezhi QIN ,
  • Jianting GUO ,
  • Langhong LOU ,
  • Lanzhang ZHOU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-07-17

  Online published: 2016-01-25

Supported by

Supported by National Natural Science Foundation of China (No.51001101) and National Energy Administration Program of China (No.NY20150102)

Abstract

Primary MC carbide is one of the most important phases in cast Ni-based superalloys. During long-term thermal exposure, the primary MC carbide is not stable and tends to degenerate, exhibiting various degeneration reactions, such as MC+γ →M6C+γ′, MC+γ→M6C + M23C6+ γ′ and MC+γ→M6C + M23C6+η. It is widely known that the degeneration of primary MC carbide has obvious influence on the microstructural evolutions of superalloys, including coarsening of γ′ phase, coarsening of grain boundaries and precipitation of topologically close-packed (TCP) phase, and consequently the mechanical properties of alloys. Much research work has focused on the degeneration mechanism of primary MC carbide during long-term thermal exposure, however, it is not very clear so far. In this work, a cast Ni-based superalloy is fabricated and thermally exposed at 850 ℃ for 500~10000 h in order to study the degeneration mechanism of primary MC carbide. The degeneration of primary MC carbide is observed by OM, SEM and TEM. High-angle annular dark field (HAADF) mode of TEM is used to clearly observe the degeneration of primary MC carbide and the element distribution in the degeneration areas. The results show that the primary MC degeneration is an inter-diffusion process which occurs between the primary carbide and the γ matrix. During the degeneration, C is released from the primary carbide, Ni, Al and Cr are provided by the γ matrix, while Ti, W and Mo come from both primary MC and γ matrix. The precipitation of η phase is determined by the atomic fraction of Ti+Nb+Ta+Hf and atomic ratio of (Ti+Nb+Ta+Hf)/Al and its amount is affected by the degeneration degree of primary MC carbide. The higher the degeneration degree, the larger the tendency for the precipitation of the η phase.

Cite this article

Wen SUN , Xuezhi QIN , Jianting GUO , Langhong LOU , Lanzhang ZHOU . DEGENERATION PROCESS AND MECHANISM OF PRIMARY MC CARBIDES IN A CAST Ni-BASED SUPERALLOY[J]. Acta Metall Sin, 2016 , 52(4) : 455 -462 . DOI: 10.11900/0412.1961.2015.00399

References

[1] Tin S, Pollock T M.Mater Sci Eng, 2003; A348: 111
[2] Chen Q Z, Kong Y H, Jones C N, Knowles D M.Scr Mater, 2004; 51: 150
[3] Chen Q Z, Jones C N, Knowles D M.Scr Mater, 2002; 47: 669
[4] Bae J S, Lee J H, Kim S S, Jo C Y.Scr Mater, 2001; 45: 03
[5] Fernandaz R, Lecomte J C, Kattamis T E.Metall Trans, 1978; 91A: 381
[6] Liu L, Sommer F, Fu H Z.Scr Metall Mater, 1994; 30: 587
[7] Chen Q Z, Jones C N, Knowles D M.Acta Mater, 2002; 50: 1095
[8] Goswami T.Int J Fatigue, 1999; 21: 55
[9] Pedron J P, Pineau A.Mater Sci Eng, 1982; A56: 143
[10] Reuchet J, Remy L.Mater Sci Eng, 1983; A58: 33
[11] Wang J, Zhou L Z, Sheng L Y, Guo J T.Mater Des, 2012; 39: 55
[12] Collins H E.Trans ASM, 1969; 62: 82
[13] Wang J, Zhou L Z, Qin X Z, Sheng L Y, Hou J S, Guo J T.Mater Sci Eng, 2012; A533: 14
[14] Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q.Mater Sci Eng, 2012; A543: 121
[15] Qin X Z, Guo J T, Yuan C, Chen C L, Hou J S, Ye H Q.Mater Sci Eng, 2008; A485: 74
[16] Yang J X, Zheng Q, Sun X F, Guan H R, Hu Z Q.Mater Sci Eng, 2006; A429: 341
[17] Yang J X, Zheng Q, Sun X F, Guan H R, Hu Z Q.J Mater Sci, 2006; 41: 6476
[18] Choi B G, Kim I S, Kim D H, Jo C Y.Mater Sci Eng, 2008; A478: 329
[19] Lvov G, Levit V I, Kaufman M J.Mater Trans, 2004; 35A: 1669
[20] Sun W, Qin X Z, Guo Y A, Guo J T, Zhou L Z, Lou L H.Mater Des, 2015; 69: 81
[21] Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R.Mater Sci Eng, 2003; A361: 191
[22] Koul A K, Castillo R.Metall Trans, 1988; 19A: 2049
[23] Sun W, Qin X Z, Guo Y A, Guo J T, Zhou L Z, Lou L H.Acta Metall Sin, 2014; 50: 744
[23] (孙文, 秦学智, 郭永安, 郭建亭, 周兰章, 楼琅洪. 金属学报, 2014; 50: 744)
[24] Zheng L, Cu C Q, Zheng Y R.Scr Mater, 2004; 50: 435
[25] Liu L R, Jin T, Zhao N R, Sun X F, Guan H R, Hu Z Q.Mater Lett, 2003; 57: 4540.
[26] Liu L R.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2004
[26] (刘丽荣. 中国科学院金属研究所博士学位论文, 沈阳, 2004)
[27] Starink M J, Cama H, Thomson R C.Scr Mater, 1998; 38: 73
[28] Zheng L.Scr Mater, 2005; 53: 943
[29] Zheng Y R, Li S S, Zheng L, Han Y F.In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloys 2008, Warrendale: TMS, 2008: 743
[30] Watanabe M, Horita Z, Sano T, Nemoto M.Acta Metall, 1994; 42: 3381.
[31] Cui C Y, Gu Y F, Harada H, Ping D H, Sato A.Metall Mater Trans, 2006; 37A: 3183
[32] Cui C Y, Gu Y F, Harada H, Ping D H, Fukuda T.Mater Sci Eng, 2008; A485: 651
[33] Bouse G K.In: Kissinger R D, Deye D J, Anton D L, Cete A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996,Warrendale: TMS, 1996: 163
[34] Seo S M, Kim I S, Lee J H, Jo C Y, Miyahara H, Ogi K.Metall Mater Trans, 2007; 38A: 883
[35] Wang J. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2011
[35] (王建. 中国科学院金属研究所硕士学位论文, 沈阳, 2011)
Outlines

/

〈 〉