Orginal Article

EFFECT OF METASTABLE AUSTENITE ON MECHANI-CAL PROPERTY AND MECHANISM IN CRYOGENICSTEEL APPLIED IN OCEANEERING

  • Changjun WANG ,
  • Jianxiong LIANG ,
  • Zhenbao LIU ,
  • Zhiyong YANG ,
  • Xinjun SUN ,
  • Qilong YONG
Expand
  • 1 Institute of Special Steels, Central Iron and Steel Research Institute, Beijing 100081, China
    2 Institute of Engineering Steels, Central Iron and Steel Research Institute, Beijing 100081, China

Received date: 2015-06-15

  Online published: 2016-01-19

Supported by

Supported by National Basic Research Program of China (No.2014CB643306)

Abstract

With the development of marine resources and its emerging markets, the marine equipments such as offshore drilling platform, subsea oil and gas transportation pipeline, and storage equipment of oil and gas are developing actively. It is urgent to develop a new type of steel with low cost and excellent toughness to satisfy the demand of marine equipment. In this work, the morphology of austenite and phase transition process in medium manganese steel during quenching and tempering (QT) and quenching, lamellarizing and tempering (QLT) heat treatments were investigated by using EBSD, HRTEM and thermal dilatometer. The results show that the discrepancy of stability in austenite caused by its shape, size and location leads to the more excellent toughness during QLT heat treatment compared to QT. It has been found from thermodynamical and dynamical viewpoint that the formation rates of reverted austenite during QLT heat treatment are significantly larger relative to QT due to the partition process of C and Mn elements in the lamellarizing stage. Moreover, two growth models of film-type reverted austenite are distinct during two heat treatments: the unidimensional two-sided growth mode during QT and unidimensional one-sided growth mode during QLT.

Cite this article

Changjun WANG , Jianxiong LIANG , Zhenbao LIU , Zhiyong YANG , Xinjun SUN , Qilong YONG . EFFECT OF METASTABLE AUSTENITE ON MECHANI-CAL PROPERTY AND MECHANISM IN CRYOGENICSTEEL APPLIED IN OCEANEERING[J]. Acta Metall Sin, 2016 , 52(4) : 385 -393 . DOI: 10.11900/0412.1961.2015.00312

References

[1] Liu Z Y, Tang S, Chen J, Wang G D.Angang Technol, 2015; 391(1): 1
[1] (刘振宇, 唐帅, 陈俊, 王国栋. 鞍钢技术, 2015; 391(1): 1)
[2] Lu X H, Gao S, Zhang C Y.Met Form, 2015; (6): 8
[2] (芦晓辉, 高珊, 张才毅. 金属加工(热加工), 2015; (6): 8)
[3] Song Y, Li X, Rong L.Mater Sci Eng, 2011; A528: 4075
[4] Strife J R, Passoja D E.Metall Trans, 1980; 11A: 1341
[5] Fultz B, Kim J I, Kim Y H.Metall Trans, 1985; 16A: 2237
[6] Fultz B, Morris Jr J W.Metall Trans, 1985; 16A: 2251
[7] Zhang F T, Wang J W, Guo Y Y.Acta Metall Sin, 1984; 20: 405
[7] (张弗天, 王景韫, 郭蕴宜. 金属学报, 1984; 20: 405)
[8] Morris Jr J W, Guo Z, Krenn C R.ISIJ Int, 2001; 41: 599
[9] Morris Jr J W. ISIJ Int, 1998; 38: 1277
[10] Guo Z, Morris Jr J W.Scr Mater, 2005; 53: 933
[11] Wang C F, Wang M, Shi J.Scr Mater, 2008; 58: 492
[12] Hughes G M, Smith G E, Crocker A G.Mater Sci Technol, 2011; 27: 767
[13] Chiang J, Lawrence B, Boyd J D.Mater Sci Eng, 2011; A528: 4516
[14] Haidemenopoulos G N, Grujicic M, Olson G B.J Alloys Compd, 1995; 220(1): 142
[15] Horn R M, Ritchie R O.Metall Trans, 1978; 9A: 1039
[16] Lee S J, Park Y M, Lee Y K.Mater Sci Eng, 2009; A515: 32
[17] Timokhina I B, Hodgson P D, Pereloma E V.Metall Mater Trans, 2004; 35A: 2331
[18] Sugimoto K, Misu M, Kobayashi M.ISIJ Int, 1993; 33: 775
[19] Chen H C, Era H, Shimizu M.Metall Trans, 1989; 20A: 437
[20] Lambert A, Drillet J, Gourgues A F.Sci Technol Weld Join, 2000; 5: 168
[21] Ikawa H, Oshige H, Tanoue T.Trans Jpn Weld Soc, 1980; 11: 87
[22] Bayraktar E, Kaplan D.J Mater Process Technol, 2004; 153: 87
[23] Lan L, Qiu C, Zhao D.J Mater Sci, 2012; 47: 4732
[24] Bonnevie E, Ferriere G, Ikhlef A.Mater Sci Eng, 2004; A385: 352
[25] Wells C, Mehl R F.Transactions, 1940; 140: 279
[26] Xu Z, Zhao L C.Phase Transition Principle of Metal Solid State. Beijing: Science Press, 2004: 16
[26] (徐洲, 赵连城. 金属固态相变原理. 北京: 科学出版社, 2004: 16)
[27] Porter D A, Easterling K E.Phase Transformations in Metals and Alloys. Boca Raton: CRC Press, 1992: 32
[28] Xu Z Y.Thermodynamics of Materials. Beijing: Higher Education Press, 2009: 72
[28] (徐祖耀. 材料热力学. 北京: 高等教育出版社, 2009: 72)
[29] Aaronson H I, Laird C, Kinsman K R. Phase Transformations. Metals Park: ASM, 1970: 196
[30] Cahn J W, Kalonji G, Aaronson H I.Solid-Solid Phase Transformations. New York: AIME, 1982: 48
[31] Yong Q L.Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 86
[31] (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 86)
[32] Luo H W, Shi J, Wang C.Acta Mater, 2011; 59: 4002
Outlines

/

〈 〉