EFFECTS OF ANNEALING PROCESS ON MICRO-STRUCTURE EVOLUTION AND PROTRUSION OFCOPPER FILLED IN THROUGH-SILICON VIAS

  • Si CHEN ,
  • Fei QIN ,
  • Tong AN ,
  • Ruiming WANG ,
  • Jingyi ZHAO
Expand
  • College of Mechanical Engineering and Applied Electronics Technology, Beijing University of Technology, Beijing 100124, China

Received date: 2015-06-15

  Online published: 2015-12-02

Supported by

Supported by National Natural Science Foundation of China (No.11272018)

Abstract

3D-IC integration realized by using through-silicon via (TSV) technology is the main trend in packaging industry. TSVs are usually fully filled by electroplated Cu, namely TSV-Cu, which can make products possess higher electrical performance, higher density and lighter weight. In a typical TSV forming process, the TSV-Cu is annealed to stabilize its microstructure. However, during annealing process, the Cu protrudes out of the TSV due to the large change in temperature and the mismatch of coefficient of thermal expansion between the Cu (16.7×10-6 ℃-1) and its surrounding Si (2.3×10-6 ℃-1) matrix. This protrusion is a potential threat to the TSV structural integrity, since it might lead to cracking or delamination. In this research, the effects of annealing process on microstructure evolution and protrusion of TSV-Cu are investigated. Four level sets of current density and additive concentration were used to fill Cu into the TSV by electroplating process to prepare test specimens. The TSV diameter was 30 μm, and depth was 100 μm. The pitch of two TSVs was 200 μm. The annealing process was conducted in a vacuum annealing furnace, the specimens were heated from 25 ℃ to 425 ℃, and then maintained for 30 min at 425 ℃. The microstructures of TSV-Cu before and after annealing were characterized by EBSD. The protrusion of specimens after annealing was measured by White Light Interferometer (WLI). The results show that, during the electroplating process, both current density and additive concentration have impact on the TSV-Cu grain size, higher current density and higher additive concentration help to gain a finer grained Cu, and the influence of the additive concentration is less significant than the current density. After being annealed, for all the specimens, the Cu grain size increases, the TSV-Cu protrudes with a crack along the Cu-Si interface within the Cu seed layer, and there is a positive correlation between the protrusion and the grain size of the TSV-Cu.

Cite this article

Si CHEN , Fei QIN , Tong AN , Ruiming WANG , Jingyi ZHAO . EFFECTS OF ANNEALING PROCESS ON MICRO-STRUCTURE EVOLUTION AND PROTRUSION OFCOPPER FILLED IN THROUGH-SILICON VIAS[J]. Acta Metall Sin, 2016 , 52(2) : 202 -208 . DOI: 10.11900/0412.1961.2015.00308

References

[1] Lau J H.Microelectron Int, 2011; 28: 8
[2] Ko C T, Chen K N.Microelectron Reliab, 2013; 53: 7
[3] Qin F, Xiang M, Wu W.Acta Metall Sin, 2014; 50: 722
[3] (秦飞, 项敏, 武伟. 金属学报, 2014; 50: 722)
[4] Okoro C, Levine L E, Xu R, Hummler K, Obeng Y S.IEEE Trans Electron Devices, 2014; 61: 2473
[5] Putra W N, Trigg A D, Li H Y, Gan C L.In: Lim Y K ed., 2014 IEEE 21st Int Symp on the Physical and Failure Analysis of Integrated Circuits, New York: Institute of Electrical and Electronics Engineers Inc, 2014: 295
[6] Zhang Y Z, Ding G F, Cheng P, Wang H.ECS Electrochem Lett, 2014; 3: D23
[7] Wu Z Y, Huang Z H, Ma Y C, Xiong H, Conway P P.Electron Mater Lett, 2014; 10: 281
[8] Wang H Y, Cheng P, Wang S, Wang H, Gu T, Li J Y, Gu X, Ding G F.Microelectron Eng, 2014; 114: 85
[9] De W I, Croes K, Varela P O, Labie R, Redolfi A, Van D P M, Vanstreels K, Okoro C, Vandevelde B, Beyne E.Microelectron Reliab, 2011; 51: 1856
[10] Heryanto A, Putra W N, Trigg A, Gao S, Kwon W S, Che F X, Ang X F, Wei J, Made R I, Gan C L, Pey K L.J Electron Mater, 2012; 41: 2533
[11] Malta D, Gregory C, Lueck M, Temple D, Krause M, Altmann F, Petzold M, Weatherspoon M, Miller J.In: Dias R, Sauter W eds., 2011 IEEE 61st Electronic Components and Technology Conference, New York: Institute of Electrical and Electronics Engineers Inc, 2011: 1815
[12] He H W, Song C S, Xu C, Wang L, Zhang W Q.In: Lim Y K ed., 2013 14th Int Conf on Electronic Packaging Technology, New York: IEEE Computer Society, 2013: 769
[13] Che F X, Putra W N, Heryanto A, Trigg A, Gao S, Gan C L.In: Koyanagi M, Kada M eds., 2011 IEEE Int 3D Systems Integration Conference, New York: IEEE Computer Society, 2011: 6262985
[14] Saettler P, Hecker M, Boettcher M, Rudolph C, Wolter K J.In: Gilles P, Jean M Y, Karlheinz B eds., Proc 5th Electronics System-integration Technology Conference, Piscataway: Institute of Electrical and Electronics Engineers Inc, 2014: 6962712
[15] Saettler P, Boettcher M, Wolter K J.In: McCann D, Pekin S eds., 2012 IEEE 62nd Electronic Components and Technology Conference, New York: Institute of Electrical and Electronics Engineers Inc, 2012: 619
[16] Okoro C, Labie R, Vanstreels K, Franquet A, Gonzalez M, Vandevelde B, Beyne E, Vandepitte D, Verlinden B.J Mater Sci, 2011; 46: 3868
[17] Shin H A S, Kim B J, Kim J H, Hwang S H, Budiman A S, Som H Y, Byun K Y, Tamura N, Kunz M, Kim D I, Joo Y C.J Electron Mater, 2012; 41: 712
[18] Pérez-Prado M T, Vlassak J J.Scr Mater, 2002; 47: 817
[19] Kumar P, Dutta I, Bakir M S.J Electron Mater, 2012; 41: 322
[20] Dutta I, Kumar P, Bakir M S.JOM, 2011; 63: 70
[21] Wu W, Qin F, Li W, Shi G.In: Bi K Y, Tian Z, Xu Z Q eds., 2014 15th Int Conf on Electronic Packaging Technology, Piscataway: Institute of Electrical and Electronics Engineers Inc, 2014: 688
[22] Che F X, Putra W N, Heryanto A, Trigg A, Zhang X W, Gan C L.IEEE Trans Compon Packag Manufact Technol, 2013; 3: 732
[23] Lee H, Wong S S, Lopatin S D.J Appl Phys, 2003; 93: 3796
[24] Lui G T, Chen D, Kuo J C.J Phys, 2009; 42D: 215410
[25] Okoro C, Vanstreels K, Labie R, Lühn O, Vandevelde B, Verlinden B, Vandepitte D.J Micromech Microeng, 2010; 20: 045032
[26] Yan W Z, Zhang J Z, Zhou Z G, Yue Z F.Acta Metall Sin, 2015; 51: 100
[26] (闫五柱, 张嘉振, 周振功, 岳珠峰. 金属学报, 2015; 51: 100)
[27] Hansen N.Scr Mater, 2004; 51: 801
Outlines

/

〈 〉