Orginal Article

EFFECTS OF SOLUTION TREATMENT ON MICRO-STRUCTURE AND WEAR-RESISTANT PROPERTIES OF CoCrW ALLOYS

  • Bo HE ,
  • Qingwu NIE ,
  • Hongyu Zhang ,
  • Hua WEI
Expand
  • 1 School of Mechatronics Engineering, Shenyang Aerospace University, Shenyang 110136, China
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-09-17

  Online published: 2015-11-30

Supported by

Supported by National Natural Science Foundation of China (No.51201161) and Natural Science Foundation of Liaoning Province (No.2013024011)

Abstract

CoCrW alloy is a kind of stellite alloy, which has high strength, good wear resistance, and is widely used in aviation industry, nuclear industry and other fields. For a long time, the CoCrW alloy is mainly used as coating to have an effect on wear and the corrosion resistance. With the development of the industry, the conventional cast CoCrW alloy has been widely studied. The mechanical properties of the cast CoCrW alloy can be changed by heat treatment, which is of high hardness and great brittleness. In this work, hardness and wear-resistant properties of the CoCrW alloys as-cast and after solution treatment were studied by combining XRD, SEM, EDS, hardness test and wear resistance test, and effects of the solution temperature on the microstructure and wear-resistant properties were also investigated. The results showed that the microstructures of the CoCrW alloys as-cast and after solution treatment were both composed of M23C6, M6C and γ-Co matrix, but the size, morphology and distribution of carbides occurred in the alloy changed obviously by solution treatment. The dissolution of a large amount of carbides in the alloy after solution treatment was mainly responsible for the decrease in hardness and wear resistance of the alloy compared with that of the as-cast one. With the increase of the solution temperature, the Cr, W and other alloying elements in the carbides were dissolved into the γ-Co matrix so as to strengthen the matrix resulting in the improvement of the hardness and the associated wear resistance of the alloy. The mechanism that controlling the wear-resistant property of CoCrW alloys as-cast and after solution treatment was the interaction of abrasive wear, adhesive wear and oxidation wear.

Cite this article

Bo HE , Qingwu NIE , Hongyu Zhang , Hua WEI . EFFECTS OF SOLUTION TREATMENT ON MICRO-STRUCTURE AND WEAR-RESISTANT PROPERTIES OF CoCrW ALLOYS[J]. Acta Metall Sin, 2016 , 52(4) : 484 -490 . DOI: 10.11900/0412.1961.2015.00488

References

[1] Alireza K, Liu R, Liang M, Yang Q.Mater Des, 2014; 56: 487
[2] Yamanaka K, Mori M, Kuramoto K J, Chiba A.Mater Des, 2014; 55: 987
[3] Yamanaka K, Mori M, Chiba A.Mater Sci Eng, 2014; C40: 127
[4] Malayoglu U, Neville A.Wear, 2003; 255: 181
[5] Wang Q L, Zhang L, Dong J D, Sun Y M.J Xuzhou Inst Technol, 2010; 25(3): 7
[5] (王庆良, 张磊, 董建东, 孙彦敏. 徐州工程学院学报, 2010; 25(3): 7)
[6] Zhong M L, Liu W J.Acta Metall Sin, 2002; 38: 495
[6] (钟敏霖, 刘文今. 金属学报, 2002; 38: 495)
[7] Li F, Hu K A, Li J L, Zhao B Y.Wear, 2002; 249: 877
[8] Rosalbino F, Scavino G.Electrochim Acta, 2013; 111: 656
[9] Yang Z Y.Rare Met, 2004; 23: 53
[10] Xu X Y, Xu B S, Liu W J, Liu S C, Zhou Z R.Rare Met Mater Eng, 2003; 32: 855
[10] (徐向阳, 徐滨士, 刘文今, 刘世参, 周仲荣. 稀有金属材料与工程, 2003; 32: 855)
[11] Liu X B, Liu H Q, Meng X J, Sun C F, Wang M D, Qi L H, Shi G L, Wu S H.Mater Chem Phys, 2014; 143: 616
[12] Hou Q Y, Gao J S, Zhou F.Surf Coat Technol, 2005; 194: 238
[13] Wang L C, Li D Y.Wear, 2003; 255: 535
[14] Gupta R K, Karthikeyan M K, Bhalia D N, Ghosh B R, Sinha P P.Met Sci Heat Treat, 2008; 50: 175
[15] Wu C F, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J.Acta Metall Sin, 2009; 45: 1013
[15] (吴朝锋, 马明星, 刘文今, 钟敏霖, 张伟明, 张红军. 金属学报, 2009; 45: 1013)
[16] Da Silva W S, Souza R M, Mello J D B, Goldenstein H.Wear, 2011; 271: 1819
[17] Li J N, Gong S L, Wang J, Shan F H, Li H X, Wu B.Acta Metall Sin, 2014; 50: 547
[17] (李嘉宁, 巩水利, 王娟, 单飞虎, 李怀学, 吴冰. 金属学报, 2014; 50: 547)
[18] Cai Z B, Zhu M H, Liu J, Xu Y, Yu J, Zhou Z R.Lubr Eng, 2006; (4): 26
[18] (蔡振兵, 朱旻昊, 刘军, 徐轶, 俞佳, 周仲荣. 润滑与密封, 2006; (4): 26)
[19] Liu H C, Pang Y X, Guo Y J.Lubr Eng, 2001; (2): 39
[19] (刘厚才, 庞佑霞, 郭源君. 润滑与密封, 2001; (2): 39)
[20] Zhang Z Z, Xue Q J, Liu W M, Shen W C.Tribol Int, 1998; 31: 361
[21] Zhang Z Y, Lu X C, Han B L, Luo J B.Mater Sci Eng, 2007; A444: 92
[22] Zhou B, Shi S F, Wang X Y.Rare Met Mater Eng, 2006; 35: 105
[22] (周炳, 史胜凤, 王小祥. 稀有金属材料与工程, 2006; 35: 105)
[23] Shin J C, Doh J M, Yoon J K, Lee D Y, Kim J S.Surf Coat Technol, 2003; 166: 117
[24] Zeng M Q, Zhang Y, Ouyang L Z, Luo K C, Zhu M.Acta Metall Sin, 2002; 38: 814
[24] (曾美琴, 张耀, 欧阳柳章, 罗堪昌, 朱敏. 金属学报, 2002; 38: 814)
[25] Xu H B, Jian X G, Wu J S, Zhang J G.Acta Metall Sin, 2001; 37: 889
[25] (徐寒冰, 简小刚, 吴建生, 章靖国. 金属学报, 2001; 37: 889)
Outlines

/