EFFECT OF THE INTERMEDIATE HEAT TREATMENT PROCESSES ON THE OXIDATION CHARACTERIS- TICS OF Zr-1Nb-0.2Y ALLOY IN 420 ℃ AIR

  • Changji LI ,
  • Liangyin XIONG ,
  • Shi LIU
Expand
  • 1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2015-03-31

  Online published: 2015-11-20

Supported by

Supported by National Natural Science Foundation of China (No.91126001)

Abstract

Zr-based alloys have been used as cladding tubes in nuclear reactors for several decades due to their superior mechanical properties, good corrosion resistance and low neutron absorption cross-section. Zr alloys consist of hcp-structured a-Zr matrix and dispersed precipitate particles. These precipitate particles play a key role in improving the service performance of the alloy. In general, the manufacturing of Zr-based alloy tubes or sheets involves a series of deformation and annealing processes, which lead to a modification of the precipitate particles in size and distribution and an improvement of comprehensive properties of the alloys. In this work, the effect of intermediate heat treatment processes on precipitate particles and air oxidation characteristics of Zr-1Nb-0.2Y (mass fraction, %) alloy was studied. With increase of rolling and annealing times, the oxidation resistance of Zr-1Nb-0.2Y alloy was improved. The final product from manufacturing route II with intermediate annealing process of 640 ℃, 3 h+570 ℃, 3 h was proved to be most resistant to oxidation in 420 ℃ air. TEM images and EDS results showed that relevant parameters such as precipitate particle volume fraction, precipitate particle mean diameter, Nb+Y content (including mean content and total content) in precipitate particles were modified by intermediate annealing processes, which essentially influenced the oxidation characteristics of Zr-1Nb-0.2Y alloy. The smaller the mean size of precipitate particle and the higher the Nb+Y content in the precipitate particle are, the better the resistance to air oxidation of Zr-1Nb-0.2Y alloy.

Cite this article

Changji LI , Liangyin XIONG , Shi LIU . EFFECT OF THE INTERMEDIATE HEAT TREATMENT PROCESSES ON THE OXIDATION CHARACTERIS- TICS OF Zr-1Nb-0.2Y ALLOY IN 420 ℃ AIR[J]. Acta Metall Sin, 2016 , 52(1) : 85 -92 . DOI: 10.11900/0412.1961.2015.00184

References

[1] Cox B. J Nucl Mater, 2005; 336: 331
[2] Yilmazbayhan A, Motta A T, Comstock R J, Sabol G P, Lai B, Cai Z H. J Nucl Mater, 2004; 324: 6
[3] Gong W J, Zhang H L, Qiao Y, Tian H, Ni X D, Li Z K, Wang X T. Corros Sci, 2013; 74: 323
[4] Nikulin S A, Khanzhin V G, Rozhnov A B, Belov V A. Met Sci Heat Treat, 2009; 51: 230
[5] Petrova I I, Samsonov B N, Peletsky V E, Nikulina A V, Sokolov N B, Andreeva-Andrievskaya L N. Int J Thermophys, 2002; 23: 1347
[6] Nikulina A V. Met Sci Heat Treat, 2004; 46: 458
[7] Liu J Z. Nuclear Structure Materials. Beijing: Chemical Industry Press, 2007: 5
[7] (刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 5)
[8] Li Z K, Liu J Z, Zhou L, Li C, Zhang J J. Rare Met Mater Eng, 2002; 31: 261
[8] (李中奎, 刘建章, 周 廉, 李 聪, 张建军. 稀有金属材料与工程, 2002; 31: 261)
[9] Canay M, Danón C A, Arias D. J Nucl Mater, 2000; 280: 365
[10] Ni N, Lozano-Perez S, Sykes J M, Smith G D W, Grovenor C R M. Corros Sci, 2011; 53: 4073
[11] Seok C S, Bae B K, Koo J M, Murty K L. Eng Fail Anal, 2006; 13: 389
[12] Steinbrück M, B?ttcher M. J Nucl Mater, 2011; 414: 276
[13] Park J Y, Yoo S J, Choi B K, Jeong Y H. J Nucl Mater, 2008; 373: 343
[14] Park J Y, Choi B K, Yoo S J, Jeong Y H. J Nucl Mater, 2006; 359: 59
[15] Zhou B X, Yao M Y, Li Z K, Wang X M, Zhou J, Long C S, Liu Q, Luan B F. J Mater Sci Technol, 2012; 28: 606
[16] Zhao W J, Liu Y Z, Jiang H M, Peng Q. J Alloys Compd, 2008; 462: 103
[17] Jeong Y H, Park S Y, Lee M H, Choi B K, Baek J H, Park J Y, Kim J H, Kim H G. J Nucl Sci Technol, 2006; 43: 977
[18] Kim H G, Park J Y, Jeong Y H, Koo Y H, Yoo J S, Mok Y K, Kim Y H, Suh J M. J Nucl Sci Technol, 2014; 46: 423
[19] Duriez C, Dupont T, Schmet B, Enoch F. J Nucl Mater, 2008; 380: 30
[20] Batra I S, Singh R N, Sengupta P, Maji B C, Madangopal K, Manikrishna K V, Tewari R, Dey G K. J Nucl Mater, 2009; 389: 500
[21] Batra I S, Singh R N, Khandelwal H K, Mukherjee A, Krishnamurthy N, Gargi C, Shah B K. J Nucl Mater, 2013; 434: 389
[22] Li C J, Xiong L Y, Wu E D, Liu S. J Nucl Mater, 2015; 457: 142
[23] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1
[24] Kim H G, Choi B K, Park J Y, Jeong Y H. Corro Sci, 2009; 51: 2400
[25] Kim H G, Park S Y, Lee M H, Jeong Y H, Kim S D. J Nucl Mater, 2008; 373; 429
[26] Li Q, Liang X, Peng J C, Liu R D, Yu K, Zhou B X. Acta Metall Sin, 2011; 47: 893
[26] (李 强, 梁 雪, 彭剑超, 刘仁多, 余 康, 周邦新. 金属学报, 2011; 47: 893)
Outlines

/

〈 〉