EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING

  • Wei GU ,
  • Jingyuan LI ,
  • Yide WANG
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2015-03-25

  Online published: 2015-11-18

Supported by

Supported by National High Technology Research and Development Program of China (No.2013AA032402) and Project on the Integration of Industry, Education and Research of Guangdong Province (No.2015B090901044)

Abstract

Generally, it is believed that inside the material the smaller grain size is, the higher yield strength is. In addition to this effect, grain refinement method also ensures that the toughness of the material is not reduced. However, it is found that the relationship between the grain size distribution and mechanical properties is contradiction with this law after the properties have been studied in the transverse direction of a large cross-section 7050 aluminum alloy profile. That is, the impact energy and yield strength in the center with a large grain size is higher than those at the edge with the smaller grain size in the thickest section of the profile. Besides that, during the establishment of the yield strength model in over-aging 7050 aluminum alloy, there are two models for the grain boundary strengthening which are Nes model and Hall-Petch model, so the choice from these model is found to affect the final results of the yield strength model. In order to study and understand the reasons for this phenomenon, the difference of mechanical properties distribution in the cross-section of 7050 aluminum extrusion profile has been investigated by impact test and tensile test at normal temperature, meanwhile, the microstructures have been analyzed by OM, EBSD and TEM. The results show that lots of the harder deformation textures, i.e., copper texture in the core of the profile lead to higher yield strength in the core with grain size of 12 mm than that in the edge with grain size of 6 mm. The Taylor factor could be calculated after the solution strengthening by alloying elements, grain boundary strengthening by the sub-grain and the yield stress of the alloy, at last, it reaches to 3.925 in the core, while that is just 2.257 in the edge. Compared with Nes model, the Hall-Petch model is much preferable to the calculation of grain boundary strengthening in yield stress of 7050 aluminum alloys after solid solution treatment. It is established that there is a linear relationship between impact energy and grain size of three over-aging specimens.

Cite this article

Wei GU , Jingyuan LI , Yide WANG . EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING[J]. Acta Metall Sin, 2016 , 52(1) : 51 -59 . DOI: 10.11900/0412.1961.2015.00163

References

[1] Liu B, Peng C Q, Wang R C, Wang X F, Li T T. Chin J Nonferrous Met, 2010; 20: 1705
[1] (刘 兵, 彭超群, 王日初, 王小锋, 李婷婷. 中国有色金属学报, 2010; 20: 1705)
[2] Dursun T, Soutis C. Mater Des, 2014; 56: 862
[3] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775
[4] Kayser T, Klusemann B, Lambers H G, Maier H J, Svendsen B. Mater Sci Eng, 2010; A527: 6568
[5] Kayser T,Parvizian F,Klusemann B. In: Mammoli A A, Brebbia C A eds., 4th Int Conf on Computational Methods and Experiments in Materials Characterisation, Southampton, UK: WIT Press, 2009: 209
[6] Han N M, Zhang X M, Liu S D, He D G, Zhang R. J Alloys Compd, 2011; 509: 4138
[7] Li P Y, Xiong B Q, Zhang Y A, Li Z H. Trans Nonferrous Met Soc China, 2012; 22: 546
[8] Chen J Z, Zhen L, Dai S L, Shao W Z, Zhang B Y. Rare Met Mater Eng, 2008; 37: 1966
[8] (陈军洲, 甄 良, 戴圣龙, 邵文柱, 张宝友. 稀有金属材料与工程, 2008; 37: 1966)
[9] Marthinsen K, Nes E. Mater Sci Eng, 1997; A234: 1095
[10] Nes E, Marthinsen K. Mater Sci Eng, 2002; A322: 176
[11] Vershinin V V. Int J Solids Struct, 2015; 67-68: 127
[12] Dixit M, Mishra R S, Sankaran K K. Mater Sci Eng, 2008; A478: 163
[13] Wang X N, Han L Z, Gu J F. Chin J Nonferrous Met, 2013; 23: 2754
[13] (王小娜, 韩利战, 顾剑锋. 中国有色金属学报, 2013; 23: 2754)
[14] Starink M J, Wang S C. Acta Mater, 2003; 51: 5131
[15] Deschamps A, Brechet Y. Acta Mater, 1998; 47: 293
[16] Wagner J A, Shenoy R N. Metall Trans, 1991; 22A: 2809
[17] Gai P, Huang X, Zeng Y, Wang M. Metall Mater Trans, 2014; 45B: 419
[18] Güzel A, J?ger A, Parvizian F, Lambers H G, Tekkaya A E, Svendsen B, Maier H J. J Mater Process Technol, 2012; 212: 323
[19] Pérocheau F, Driver J H. Int J Plast, 2000; 16: 73
[20] Gu W, Li J Y, Wang Y D, Lu J Y, Zhou Y H. Chin J Nonferrous Met, 2014; 24: 2257
[20] (顾 伟, 李静媛, 王一德, 卢继延, 周玉焕. 中国有色金属学报, 2014; 24: 2257)
[21] Tajally M, Huda Z, Masjuki H H. Int J Impact Eng, 2010; 37: 425
[22] Sun X Y, Zhang B, Lin H Q, Zhou Y, Sun L, Wang J Q, Han E H, Ke W. Corros Sci, 2013; 77: 103
[23] Du Z W, Sun Z M, Shao B L, Zhou T T, Chen C Q. Mater Charact, 2006; 56: 121
[24] Liu D, Xiong B, Bian F, Li Z, Li X, Zhang Y, Wang F, Liu H. Mater Sci Eng, 2013; A588: 1
[25] Chen J Z. PhD Dissertation, Harbin Institute of Technology, 2008
[25] (陈军洲. 哈尔滨工业大学博士学位论文, 2008)
[26] Totten G E, MacKenzie D S. Handbook of Aluminum. Vol.1, New York: Marcel Dekker Inc., 2003: 94
Outlines

/

〈 〉