Orginal Article

DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION

  • Rui YANG ,
  • Yan PAN ,
  • Wei CHEN ,
  • Qiaoyan SUN ,
  • Lin XIAO ,
  • Jun SUN
Expand
  • State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China

Received date: 2015-04-13

  Online published: 2015-11-16

Supported by

Supported by National Natural Science Foundation of China (Nos.51271136, 51321003 and 51301127), National Basic Research Program of China (No.2014CB644003) and Program of Introducing Talents of Discipline to Universities of China (NoB06025)

Abstract

Ti and its alloys have potential application in micro-electromechanical systems (MEMS) for its excellent mechanical properties. The strength of micro- and nano-scale Ti and its alloys has been proven significantly increased as the sample size decreased, which is known as the "size effect", when dislocation and twinning are dominant plastic deformation modes. Martensitic transformation is an important plastic deformation mode in the Ti alloys. However, there is a limited research on the martensitic transformation in small-scale. Therefore, the study on mechanical behavior and deformation mechanism of [011]-oriented Ti-10V-2Fe-3Al (Ti1023) single crystal micropillars in a size range of 0.3~2.0 μm were investigated under uniaxial compression. The results show that Ti1023 micropillars exhibit smooth stress-strain curves in the regime of plastic deformation without a conventional strain burst phenomenon in the submicron pillars. It means continuous plastic strain hardening. The relationship between the yield stress (σ0.2), the stress for stress-induced martensite phase (SIM) transformation (σcm) and the sample size can be expressed in the forms of σ0.2d -0.18 and σcmd -0.28 , respectively. Strain hardening exponent (n) in creases with decreasing micropillar size. SEM examination together with crystallography analysis show that {112}<111> slip predominates plastic deformation mode in the Ti1023 micropillars. Transmission electron microscopy (TEM) observation of microstructures in the deformed and undeformed micropillars indicate that both nanoscale athermal ω particles and SIM phase α″ impede dislocation movement, and prohibit the formation of tangled dislocations in a collective, avalanche-like way resulting in strain bursts.

Cite this article

Rui YANG , Yan PAN , Wei CHEN , Qiaoyan SUN , Lin XIAO , Jun SUN . DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. Acta Metall Sin, 2016 , 52(2) : 135 -142 . DOI: 10.11900/0412.1961.2015.00216

References

[1] Kim J Y, Jang D C, Greer J R.Acta Mater, 2010; 58: 2355
[2] Schneider A S, Kaufmann D, Clark B G, Frick C P, Gruber P A, Mönig R, Kraft O, Arzt E.Phys Rev Lett, 2009; 103: 105501
[3] Kim J Y, Jang D C, Greer J R.Scr Mater, 2009; 61: 300
[4] Han S M, Bozorg-Grayeli T, Groves J R, Nix W D.Scr Mater, 2010; 63: 1153
[5] Kaufmann D, Mönig R, Volkert C A, Kraft O.Int J Plast, 2011; 27: 470
[6] Kaufmann D, Schneider A S, Mönig R, Volkert C A, Kraft O.Int J Plast, 2013; 49: 145
[7] Schneider A S, Clark B G, Frick C P, Gruber P A, Arzt E.Mater Sci Eng, 2009; A508: 241
[8] Huang L, Li Q J, Shan Z W, Li J, Sun J, Ma E.Nat Commu, 2011; 2: 547
[9] Greer J R, De Hosson J T M.Prog Mater Sci, 2011; 56: 654
[10] Brinckmann S, Kim J Y, Greer J R.Phys Rev Lett, 2008; 100: 155502
[11] Greer J R, Weinberger C R, Cai W.Mater Sci Eng, 2008; A493: 21
[12] Kim J Y, Jang D C, Greer J R.Int J Plast, 2012; 28: 46
[13] Frick C P, Clark B G, Arzt E.Acta Mater, 2007; 55: 3845
[14] Frick C P, Clark B G, Orso S, Petra S R.Scr Mater, 2008; 59: 7
[15] Norflleet D M, Sarosi P M, Manchiraju S, Wagner M F X, Uchic M D, Anderson P M, Mills M G.Acta Mater, 2009; 57: 3549
[16] San Juan J, Nó M L. J Alloys Compd, 2013; 577S: S25
[17] Liu L, Ding X, Li J, Lookman T, Sun J.Nanoscale, 2014; 6: 2067
[18] Withey E A, Minor A M, Chrzan D C, Morris Jr J W, Kuramoto S.Acta Mater, 2010; 58: 2652
[19] Li C.PhD Dissertation, Hunan University, Changsha, 2009
[19] (李聪. 湖南大学博士学位论文, 长沙, 2009)
[20] Duerig T W, Terlinde G T, Williams J C.Metall Trans, 1980; 11A: 1980
[21] Grujicic M, Zhang Y J.Mater Sci, 2000; 35: 4635
[22] Shu D L.Mechanical Properties of Engineering Materials. Beijing: China Machine Press, 2007: 15
[22] (束德林. 工程材料力学性能. 北京: 机械工业出版社, 2007: 15)
[23] Gu R, Ngan A H W.Scr Mater, 2013; 68: 861
[24] Jennings A T, Burek M J, Greer J R.Phys Rev Lett, 2010; 104: 135503
[25] Furuhara T, Annaka S, Tomio Y, Maki T. Mat Sci Eng, 2006; A438-440: 825
[26] Duerig T W, Albrecht J, Richter D, Fischer P.Acta Metall, 1982; 30: 2161
[27] Honeycombe R W K. The Plastic Deformation of Metal. 2nd Ed., London: Edward Arnold Ltd., 1984: 107
[28] Kim J Y, Jang D C, Greer J R.Int J Plast , 2012; 28: 46
[29] Magnin T, Driver J H.Mater Sci Eng, 1979; 39: 175
[30] Jennings A T, Gross C, Greer F, Aitken Z H, Lee S W, Weinberge C R, Greer J R.Acta Mater, 2012; 60: 3444
[31] Gu R, Ngan A H W.Acta Mater, 2012; 60: 6102
[32] Jang D C, Cai C, Greer J R.Nano Lett, 2011; 11: 1743
[33] Williams J C, Hickman B S, Marcus H L.Metall Trans, 1971; 2A: 1913
[34] Zhang J Y, Liu G, Sun J.Int J Plast, 2013; 50: 1
Outlines

/