Orginal Article

QUANTITATIVE 3D CHARACTERIZATION ON OXIDE INCLUSIONS IN SLAB OF Ti BEARING FERRITIC STAINLESS STEEL USING HIGH RESOLUTION SYNCHROTRON MICRO-CT

  • Wen YANG ,
  • Lifeng ZHANG ,
  • Ying REN ,
  • Haojian DUAN ,
  • Ying ZHANG ,
  • Xianghui XIAO
Expand
  • 1 School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
    2 Advanced Photon Source, Argonne National Laboratory, Argonne, IL 60439, USA

Received date: 2015-04-17

  Online published: 2015-10-16

Supported by

Supported by National Natural Science Foundation of China (Nos.51274034, 51334002 and 51404019)

Abstract

Non-metallic inclusions especially oxides are detrimental to the quality of ferritic stainless steel products. Accurate characterization on inclusions is conducive to further research on the inclusion control. There are some disadvantages in traditional 2D or 3D inclusion detection methods, tomography is thus employed to characterize inclusions in steel in the current work. Oxide inclusions in the slab of Ti bearing ferritic stainless steel were characterized 3 dimensionally using high resolution synchrotron micro computed tomography (Micro-CT), and the variations of quantity, volume and size of oxide inclusions along the thickness of continuous casting slab were analyzed quantitatively and compared with the 2D results detected by ASPEX, an automated scanning SEM. It was found that non-destructive detection could be well done by Micro-CT more accurately. The detected oxides by Micro-CT were mainly global, and the number of inclusions decreased with increasing size. In general, the number density and volume fraction of oxides were largest in the center of slab thickness, and decreased with the distance from center, reached the smallest value near the surface of slab. Contrarily, the average of equivalent diameter of oxide inclusions was largest near slab surface, and was smallest near quarter of thickness on the loose side.

Cite this article

Wen YANG , Lifeng ZHANG , Ying REN , Haojian DUAN , Ying ZHANG , Xianghui XIAO . QUANTITATIVE 3D CHARACTERIZATION ON OXIDE INCLUSIONS IN SLAB OF Ti BEARING FERRITIC STAINLESS STEEL USING HIGH RESOLUTION SYNCHROTRON MICRO-CT[J]. Acta Metall Sin, 2016 , 52(2) : 217 -223 . DOI: 10.11900/0412.1961.2015.00226

References

[1] Zhang L F, Li Y L, Ren Y.Iron Steel, 2013; 48(11): 1
[1] (张立峰, 李燕龙, 任英. 钢铁, 2013; 48(11): 1)
[2] Zhang L F, Li Y L, Ren Y.Iron Steel, 2013; 48(12): 1
[2] (张立峰, 李燕龙, 任英. 钢铁, 2013; 48(12): 1)
[3] Ren Y, Zhang L F, Yang W.Steelmaking, 2014; 30(1): 71
[3] (任英, 张立峰, 杨文. 炼钢, 2014; 30(1): 71)
[4] Ha H Y, Park C J, Kwon H S.Corros Sci, 2007; 49: 1266
[5] Chang E, Zheng H G, Zhang L, Yang J.Shanghai Met, 2008; 30(6): 18
[5] (常锷, 郑宏光, 张丽, 杨军. 上海金属, 2008; 30(6): 18)
[6] Zhang L F, Yang W, Zhang X W, Luo Y, Liu Y.Iron Steel, 2014; 49(2): 1
[6] (张立峰, 杨文, 张学伟, 罗艳, 刘洋. 钢铁, 2014; 49(2): 1)
[7] Zhang L F, Zhang X W, Luo Y, Liu Y, Zhang Y, Yang W.In: The Chinese Society for Metals ed., Proc 9th CSM Steel Congress, Beijing: Metallurgical Industry Press, 2013: 1
[7] (张立峰, 张学伟, 罗艳, 刘洋, 张莹, 杨文. 见: 中国金属学会编, 第九届中国钢铁年会论文集, 北京: 冶金工业出版社, 2013: 1)
[8] Asghar Z, Requena G, Degischer H P, Cloetens P.Acta Mater, 2009; 57: 4125
[9] Maire E, Grenier J C, Daniel D, Baldacci A, Klöcker H, Bigot A.Scr Mater, 2006; 55: 123
[10] Nagasekhar A V, Cáceres C H, Kong C.Mater Charact, 2010; 61: 1035
[11] Tiryakioğlu M.Mater Sci Eng, 2008; A473: 1
[12] Maire E.Annual Rev Mater Res, 2012; 42: 163
[13] Meidani H, Desbiolles J L, Jacot A, Rappaz M.Acta Mater, 2012; 60: 2518
[14] Felberbaum M, Rappaz M.Acta Mater, 2011; 59: 6849
[15] Wan Q, Zhao H D, Zou C.Acta Metall Sin, 2013; 49: 284
[15] (万谦, 赵海东, 邹纯. 金属学报, 2013; 49: 284)
[16] Yi J, Gao Y, Lee P, Flower H, Lindley T.Metall Mater Trans, 2003; 34A: 1879
[17] Li P, Lee P, Lindley T, Maijer D, Davis G, Elliott J.Adv Eng Mater, 2006; 8: 476
[18] Wan Q, Zhao H D, Zou C.ISIJ Int, 2014; 54: 511
[19] Rashed H, Robson J, Bate P, Davis B.Mater Sci Eng, 2011; A528: 2610
[20] Nicoletto G, Konečná R, Fintova S.Int J Fatigue, 2012; 41: 39
[21] Li M, Wang L, Almer J D.Acta Mater, 2014; 76: 381
[22] Zhang H, Toda H, Qu P C, Sakaguchi Y, Kobayashi M, Uesugi K, Suzuki Y.Acta Mater, 2009; 57: 3287
[23] Ferrié E, Buffière J Y, Ludwig W, Gravouil A, Edwards L.Acta Mater, 2006; 54: 1111
[24] Ludwig W, Buffiere J, Savelli S, Cloetens P.Acta Mater, 2003; 51: 585
[25] Li T, Shimasaki S, Taniguchi S, Uesugi K, Narita S.ISIJ Int, 2013; 53: 1943
[26] Fang K M, Ni R M.Metall Trans, 1986; 17A: 315
[27] Yang W, Zhang L F, Wang X H, Ren Y, Liu X F, Shan Q L.ISIJ Int, 2013; 53: 1401
Outlines

/

〈 〉