RESEARCH PROGRESS IN A HIGH PERFORMANCE CAST & WROUGHT SUPERALLOY FOR TURBINE DISC APPLICATIONS

  • Yuefeng GU ,
  • Chuanyong CUI ,
  • Yong YUAN ,
  • Zhihong ZHONG
Expand
  • 1 National Institute for Materials Science, Tsukuba, 305-0047, Japan
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    3 Xi'an Thermal Power Research Institute Co., Ltd., Xi'an 710032
    4 School of Materials Science and Engineering, Hefei University of Technology, Hefei 230009

Online published: 2015-09-08

Supported by

Supported by National Natural Science Foundation of China (Nos.51171179, 51271174, 51331005, 51401071 and 11332010)

Cite this article

Yuefeng GU , Chuanyong CUI , Yong YUAN , Zhihong ZHONG . RESEARCH PROGRESS IN A HIGH PERFORMANCE CAST & WROUGHT SUPERALLOY FOR TURBINE DISC APPLICATIONS[J]. Acta Metall Sin, 2015 , 51(10) : 1191 -1206 . DOI: 10.11900/0412.1961.2015.00442

References

[1] Guo J T. Materials Science and Engineering for Superalloy. Vol.3, Beijing: Science Press, 2010: 650 (郭建亭. 高温合金材料学(下册). 北京: 科学出版社, 2010: 650)
[2] Jiang H F. Gas Turbine Experiment Res, 2002; 15(4): 1 (江和甫. 燃气涡轮试验与研究, 2002; 15(4): 1)
[3] Reed R C. The Superalloys Fundaments and Application. Cambridge: Cambridge University Press, 2006: 259
[4] Gu Y F, Cui C Y, Harada H, Fukuda T, Ping D H, Mitsuhashi A, Kato K, Kobayashi T, Fujioka J. In: Reed R C, Green A K, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloy 2008, Pittsburgh: TMS, 2008: 53
[5] Cao W D. In: Green K A, Pollock T M, Harada H Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Pittsburgh: TMS, 2004: 91
[6] Reed R C, Jackson M, Na Y S. Metall Mater Trans, 1999; 30A: 521
[7] Gabb T P, Telesman J, Kantzos P T, O'Connor K. Characterization of the Temperature Capabilities of Advanced Disk Alloy ME3. Washington: National Aeronautics and Space Administration,NASA/TM-2002-211796, 2002
[8] Gu Y F, Fukuda T, Cui C Y, Harada H, Mitsuhashi A, Yokokawa T, Fujioka J, Koizumi Y, Kobayashi T. Metall Mater Trans, 2009; 40A: 3047
[9] Yokokawa T, Gu Y F, Cui C Y, Koizumi Y, Fujioka J, Harada H, Fukuda T, Mitsuhashi A. JIM, 2010; 74: 221
[10] Gu Y F, Harada H, Cui C Y, Ping D H, Sato A, Fujioka J. Scr Mater, 2006; 55: 815
[11] Cui C Y, Gu Y F, Harada H, Sato A. Metall Mater Trans, 2005; 36A: 2921
[12] Guard R, Westbrook J. Trans Am Inst Mining Metall Eng, 1959; 215: 807
[13] Takasugi T, Takazawa M, Izumi O. J Mater Sci, 1990; 25: 4239
[14] Suzuki T, Oya Y, Ochiai S. Metall Trans, 1984; 15: 173
[15] Aoki K, Wang X M, Memezawa A, Masumoto T. Mater Sci Eng, 1994; A179: 390
[16] Cui C Y, Gu Y F, Ping D H, Harada H. Intermetallics, 2008; 16: 910
[17] Guo J T. Materials Science and Engineering for Superalloy. Vol.2, Beijing: Science Press, 2010: 663 (郭建亭. 高温合金材料学(中册). 北京: 科学出版社, 2010: 663)
[18] Cui C Y, Gu Y F, Harada H, Ping D H, Sato A. Metall Mater Trans, 2006; 37A: 3183
[19] Cui C Y, Gu Y F, Ping D H, Harada H, Fukuda T. Mater Sci Eng, 2008; A485: 651
[20] Cui C Y, Gu Y F, Ping D H, Harada H. Metall Mater Trans, 2009; 40A: 282
[21] Ping D H, Cui C Y, Gu Y F, Harada H. Ultramicroscopy, 2007; 107: 791
[22] Cui C Y, Gu Y F, Ping D H, Fukuda T, Harada H. Mater Trans, 2008; 49: 424
[23] Xu L, Cui C Y, Sun X F. Mater Sci Eng, 2011; A528: 7851
[24] Yuan Y, Gu Y F, Cui C Y, Osada T, Zhong Z H, Tetsui T, Yokokawa T, Harada H. J Mater Res, 2011; 26: 2833
[25] Yuan Y, Gu Y F, Cui C Y, Osada T, Yokokawa T, Harada H. Adv Eng Mater, 2011; 13: 296
[26] Fukuda T, Mitsuhashi A, Kato K, Gu Y F, Harada H. J Gas Turbine Soc Jpn, 2007; 35(3): 132
[27] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775
[28] Osada T, Gu Y F, Yokokawa T, Harada H. JIM, 2010; 74: 279
[29] Osada T, Gu Y F, Yuan Y, Yokokawa T, Harada H. JIM, 2010; 74: 688
[30] Zhong Z H, Gu Y F, Yuan Y, Osada T, Cui C Y, Yokokawa T, Tetsui T, Harada H. Metall Mater Trans, 2012; 43A: 1017
[31] Yuan Y, Gu Y F, Zhong Z H, Osada T, Yokokawa T, Harada H. In: Huron E S, Reed R C, Hardy M C, Mills M J, Montero R E, Telesman J eds., Superalloy 2012, Pittsburgh: TMS, 2012: 35
[32] Yuan Y, Gu Y F, Zhong Z H, Osada T, Yokokawa T, Harada H. Scr Mater, 2012; 67: 137
[33] Cui C Y, Gu Y F, Yuan Y, Harada H. Scr Mater, 2011; 64: 502
[34] Cui C Y, Jin T, Sun X F. J Mater Sci, 2011; 46: 5546
[35] Tian C G, Cui C Y, Xu L, Gu Y F, Sun X F. J Mater Sci Technol, 2013; 29: 873
[36] Cai Y L, Tian C G, Fu S H, Han G M, Cui C Y, Zhang Q C. Mater Sci Eng, 2015; A638: 314
[37] Xu Y J, Qi D Q, Du K, Cui C Y, Ye H Q. Scr Mater, 2014; 87: 37
[38] Gu Y F, Cui C Y, Ping D H, Harada H, Fukuda T, Fujioka J. Mater Sci Eng, 2009; A510-511: 250
[39] Yuan Y, Gu Y F, Cui C Y, Osada T, Tetsui T, Yokokawa T, Harada H. Mater Sci Eng, 2011; A528: 5106
[40] Yuan Y, Gu Y F, Zhong Z H, Osada T, Cui C Y, Tetsui T, Yokokawa T, Harada H. J Microscopy, 2012; 248: 34
[41] Tian C G, Han G M, Cui C Y, Sun X F. Mater Des, 2014; 64: 316
[42] Tian C G, Cui C Y, Sun X F. Metall Mater Trans, 2015; 46A: 4601
[43] Xu L, Chu Z K, Cui C Y, Gu Y F, Sun X F. Acta Metall Sin, 2013;49: 863 (徐 玲, 储昭贶, 崔传勇, 谷月峰, 孙晓峰. 金属学报, 2013; 49: 863)
[44] Zhang Z J, Zhang P, Li L L, Zhang Z F. Acta Mater, 2012; 60: 3113
[45] Zhong Z H, Gu Y F, Yuan Y, Yokokawa T, Harada H. Mater Sci Eng, 2012; A552: 434
[46] Zhong Z H, Gu Y F, Yuan Y, Cui C Y, Yokokawa T, Harada H. Mater Sci Eng, 2012; A552: 464
[47] Zhong Z H, Gu Y F, Yuan Y, Cui C Y, Yokokawa T, Harada H. J Mater Sci, 2011; 46: 7573
[48] Osada T, Nagashima N, Gu Y F, Yuan Y, Yokokawa T, Harada H. Scr Mater, 2011; 64: 892
[49] Osada T, Gu Y F, Nagashima N, Yuan Y, Yokokawa T, Harada H. Acta Mater, 2013; 61: 1820
Outlines

/

〈 〉