EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS

  • Jianxin DONG ,
  • Linhan LI ,
  • Haoyu LI ,
  • Maicang ZHANG ,
  • Zhihao YAO
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Online published: 2015-09-02

Supported by

Supported by National Natural Science Foundation of China (No.51571012)

Abstract

The elimination of the segregation improves the thermo plasticity of superalloy ingot during the homogenization process, but coarser grain structure and high-temperature oxidation caused in further homogenization have an adverse impact on the thermo plasticity. The inheritance of coarse grain structure in the followed hot working process increases the tendency of cogging crack and makes the grain refining harder, leading to a lower yield of the final workpiece. The microstructure characteristics and their hot deformation behaviors of GH4740H, GH4738, GH3625 and 690 alloys under different homogenizations were investigated by means of microstructure analysis methods and crack propagation testing. The experimental results show that the reasonable homogenization processing needs to take into account the segregation elimination arising thermo plasticity addition, more to consider grain coarsing and severe oxidation leading to decrease plasticity. Based on the residue dendrites can provide more recrystalazation nucleation sites, the partial homogenization possessing probably exists rationality. This research work provides an exploratory study for the improvement of the homogenization-cogging process of superalloy.

Cite this article

Jianxin DONG , Linhan LI , Haoyu LI , Maicang ZHANG , Zhihao YAO . EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS[J]. Acta Metall Sin, 2015 , 51(10) : 1207 -1218 . DOI: 10.11900/0412.1961.2015.00419

References

[1] Semiatin S L, Kramb R C, Turner R E, Zhang F, Antony M M. Scr Mater, 2004; 51: 491
[2] Malara C, Radavich J. In: Loria E A ed., Superalloys 718, 625, 706 and Derivatives 2005, Warrendale: TMS, 2005: 25
[3] Ju Q, Ma H P, Fu X D, Wang M. Rare Met Mater Eng, 2012; 41: 310 (鞠 泉, 马惠萍, 符鑫丹, 王 明. 稀有金属材料与工程, 2012; 41: 310)
[4] Semiatin S L, Weaver D S, Fagin P N, Glavicic M G, Goetz R L, Frey N D, Kramb R C, Antony M M. Metall Mater Trans, 2005; 35A: 679
[5] Zhao Y X, Fu S H, Zhang S W, Tang X, Liu N, Zhang G Q. In: Ott E A, Groh J R, Banik A, Dempster I, Gabb T P, Helmink R, Liu X B, Mitchell A, Sjoberg G P, Wusatowska-Sarnekeds A eds., Superalloys 718 and Derivatives 2010, Warrendale: TMS, 2010: 271
[6] Semiatin S L, Weaver D S, Goetz R L, Thomas J P, Turner T J. Mater Sci Forum, 2007; 550: 129
[7] Kramb R C, Antony M M, Semiatin S L. Scr Mater, 2006; 54: 1645
[8] Kermanpur A, Wang W, Lee P D, McLean M. Mater Sci Technol, 2003; 19: 859
[9] Yao Z H, Dong J X, Zhang M C. Acta Metall Sin, 2011; 47: 1581 (姚志浩, 董建新, 张麦仓. 金属学报, 2011; 47: 1581)
[10] Li L H, Dong J X, Zhang M C, Yao Z H. Acta Metall Sin, 2014; 50: 821 (李林翰, 董建新, 张麦仓, 姚志浩. 金属学报, 2014; 50: 821)
[11] Wen D X, Lin Y C, Li H B, Chen X M, Deng J, Li L T. Mater Sci Eng, 2014; A591:183
[12] Yao Z H, Zhang M C, Dong J X. Metall Mater Trans, 2013; 44A: 3084
[13] Li H Y, Kong Y H, Chen G S, Xie L X, Zhu S G, Sheng X. Mater Sci Eng, 2014; A582: 368
[14] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289 (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[15] Kong Y H, Liu R Y, Chen G S, Xie L X, Zhu S G. J Mater Eng Perform, 2013; 22: 1372
[16] Shi C X, Zhong Z Y. Acta Metall Sin, 2010; 46: 1281 (师昌绪, 仲增墉. 金属学报, 2010; 46: 1281)
[17] Wang X H, Ward R M, Jacobs M H, Barratt M D. Metall Mater Trans, 2007; 39A: 449
[18] Miao Z J, Shan A D, Wu Y B, Lu J, Xu W L, Song H W. Trans Nonferrous Met Soc China, 2011; 21: 1009
[19] Tin S, Lee P D, Kermanpur A, Rist M, McLean M. Metall Mater Trans, 2005; 36A: 2493
[20] Yeom J T, Lee C S, Kima J H, Park N K. Mater Sci Eng, 2007; A449-451: 722
[21] Dandre C A, Roberts S M, Evans R W, Reed R C. Mater Sci Technol, 2000; 16: 14
[22] Wang P, Dong J X. Rare Met Mater Eng, 2014; 43: 2502 (王 璞, 董建新. 稀有金属材料与工程, 2014; 43: 2502)
[23] Luo K J, Zhang M C, Wang B S, Dong J X. Rare Met Mater Eng, 2011; 40: 605 (罗坤杰, 张麦仓, 王宝顺, 董建新. 稀有金属材料与工程, 2011; 40: 605)
[24] High Temperature Alloys Laboratory,Beijing Institute of Iron Steel.GH132 Alloy. Beijing: National Defence Industry Press, 1980: 26 (北京钢铁学院高温合金教研室编. GH132合金.北京: 国防工业出版社, 1980: 26)
[25] Wang J, Wu Y, Dong J X, Zhang M C, Xie X S, Xu F H. Rare Met Mater Eng, 2013; 42: 1908 (王 珏, 吴 赟, 董建新, 张麦仓, 谢锡善, 徐芳泓. 稀有金属材料与工程, 2013; 42: 1908)
Outlines

/

〈 〉