RESEARCH PROCESS ON MICROSTRUCTURAL STABILITY AND MECHANICAL BEHAVIOR OF ADVANCED Ni-BASED SINGLE CRYSTAL SUPERALLOYS

  • Tao JIN ,
  • Yizhou ZHOU ,
  • Xinguang WANG ,
  • Jinlai LIU ,
  • Xiaofeng SUN ,
  • Zhuangqi HU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Online published: 2015-08-27

Supported by

Supported by High Technology Research and Development Program of China (No.2014AA-041701) and National Natural Science Foundation of China (Nos.51331005 and 11332010)

Abstract

Ni-based single crystal superalloys have been widely used to produce turbine blades for advanced aero-engines because of the super temperature-related microstructural stability and comprehensive mechanical properties. However, due to effects of the high temperature and complicated stresses in service, the microstructures of superalloys might gradually evolve and fail in different modes. The present paper reviews the progress of microstructural stability and mechanical behavior including the γ’ phase rafting, TCP phase precipitation, high temperature creep, low cycle fatigue and thermomechanical fatigue of single crystal superalloys. The addition of Ru improves the creep life of superalloys, but also indirectly promotes the occurrence of “topological inversion”. On the other hand, with the increase of aging temperature and time, the contents of refractory elements in m phase rise significantly. With the increase of applied tension stress, more m phase precipitate from the γ matrix, whereas inverse tendency is shown under compression stress. Numerous planar defects are formed during precipitation of m phase, and these defects promote the nucleation of P and R phases. During high temperature and low stress creep, an important dislocation a<010> superdislocation is observed, which moves in the γ’ phase slowly by a combination of slide and climb. Under very high temperature, incubation with accelerating creep rate occurs before the primary stage, which relates to the extending process of the γ width. At last, the stacking fault energy is significantly reduced after Ru additions, and thus a series of complex deformation mechanisms occur during low cycle fatigue, e.g. stacking faults penetrating γ/γ’ interface, trailing a/6<112> Shockley dislocations shearing into the γ’ phase. During thermomechanical fatigue, the life of superalloys is influenced by the site of crack initiation, microstructural evolution and oxidation resistance.

Cite this article

Tao JIN , Yizhou ZHOU , Xinguang WANG , Jinlai LIU , Xiaofeng SUN , Zhuangqi HU . RESEARCH PROCESS ON MICROSTRUCTURAL STABILITY AND MECHANICAL BEHAVIOR OF ADVANCED Ni-BASED SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2015 , 51(10) : 1153 -1162 . DOI: 10.11900/0412.1961.2015.00429

References

[1] Reed R C. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 19
[2] Hu Z Q, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31(3): 1 (胡壮麒, 刘丽荣, 金 涛, 孙晓峰. 航空发动机, 2005; 31(3): 1)
[3] Sun X F, Jin T, Zhou Y Z, Hu Z Q. Mater China, 2012; 31(12): 1 (孙晓峰, 金 涛, 周亦胄, 胡壮麒. 中国材料进展, 2012; 31(12): 1)
[4] Darolia R, Lahrman D F, Field R D, Sisson R. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1988, Champion, PA: TMS, 1988: 255
[5] Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Jo C Y. Philos Mag Lett, 2012; 92: 556
[6] Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Yoo Y S, Jo C Y. Metall Mater Trans, 2012; 43A: 3608
[7] Tan X P, Hong H U, Choi B G, Kim I S, Jo C Y, Jin T, Hu Z Q. J Mater Sci, 2013; 48: 1085
[8] Argence D, Vernault C, Desvallées Y, Fournier D. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Champion, PA: TMS, 2000: 829
[9] Zhang J X, Koizumi Y, Kobayashi T, Murakumo T, Harada H. Metall Mater Trans, 2004; 35A: 1911
[10] Wang X G, Liu J L, Jin T, Sun X F. Mater Sci Eng, 2014; A598: 154
[11] Wang X G, Liu J L, Jin T, Sun X F, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Mater Des, 2015; 67: 543
[12] Murakumo T, Kobayashi T, Koizumi Y, Harada H. Acta Mater, 2004; 52: 3737
[13] Mughrabi H. Mater Sci Technol, 2009; 25: 191
[14] Pollock T M, Argon A S. Acta Metall, 1994; 42: 1859
[15] Wang X G. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2015 (王新广. 中国科学院金属研究所博士学位论文, 沈阳, 2015)
[16] Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Jo C Y. Mater Sci Eng, 2013; A580: 21
[17] Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Adv Eng Mater, 2015; 17: 1034
[18] Rae C M F, Reed R C. Acta Mater, 2001; 49: 4113
[19] Seiser B, Drautz R, Pettifor D G. Acta Mater, 2011; 59: 749
[20] Yeh A C, Tin S. Metall Mater Trans, 2006; 37A: 2621
[21] Hobbs R A, Zhang L, Rae C M F, Tin S. Metall Mater Trans, 2008; 39A: 1014
[22] Ofori A P, Humphreys C J, Tin S, Jones C N. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Champion, PA: TMS, 2004: 787
[23] Sato A, Harada H, Yokokawa T, Murakumo T, Koizumi Y, Kobayashi T, Imai H. Scr Mater, 2006; 54: 1679
[24] Gao S, Zhou Y Z, Li C F, Cui J P, Liu Z Q, Jin T. J Alloys Compd, 2014; 610: 589
[25] Cheng K Y. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009 (成魁宇. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
[26] Tan X P. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012 (谭喜鹏. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
[27] Luo Y P. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2014 (罗银屏. 中国科学院金属研究所硕士学位论文, 沈阳, 2014)
[28] Chen J Y, Feng Q, Sun Z Q. Scr Mater, 2010; 63: 795
[29] Pollock T M, Argon A S. Acta Metall, 1992; 40: 1
[30] Field R D, Pollock T M, Murphy W H. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Champion, PA: TMS, 1992: 557
[31] Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H, Masaki S. Metall Mater Trans, 2002; 33A: 3741
[32] Huang M, Cheng Z Y, Xiong J C, Li J R, Hu J Q, Liu Z L, Zhu J. Acta Mater, 2014; 76: 294
[33] Gabrisch H, Mukherji D. Acta Mater, 2000; 48: 3157
[34] Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Mater Sci Eng, 2015; A626: 406
[35] Eggeler G, Dlouhy A. Acta Mater, 1997; 45: 4251
[36] Srinivasan R, Eggeler G F, Mills M J. Acta Mater, 2000; 48: 4867
[37] Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H. Acta Mater, 2003; 51: 5073
[38] Reed R C, Cox D C, Rae C M F. Mater Sci Eng, 2007; A448: 88
[39] le Graverend J B, Cormier J, Jouiad M, Gallerneau F, Paulmier P, Hanmon F. Mater Sci Eng, 2010; A527: 5295
[40] Caron P. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Champion, PA: TMS, 2000: 737
[41] Li Q Q. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012 (李芹芹. 中国科学院金属研究所硕士学位论文, 沈阳, 2012)
[42] Li P, Li Q Q, Jin T, Zhou Y Z, Li J G, Sun X F, Zhang Z F. Int J Fatigue, 2014; 63: 137
[43] Auerswald J, Mukherji D, Chen W, Wahi R P. Z Metallkd, 1997; 88: 652
[44] Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Scr Mater, 2015; 99: 57
[45] Zhang X. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006 (张 炫. 中国科学院金属研究所博士学位论文, 沈阳, 2006)
[46] Gabb T P, Welsch G E. Scr Metall, 1986; 20: 1049
[47] Gabb T P, Welsch G E. Acta Metall, 1989; 37: 2507
[48] Milligan W W, Jayaraman N. Mater Sci Eng, 1986; 82: 127
[49] Zhou H, Ro Y, Harada H, Aoki Y, Arai M. Mater Sci Eng, 2004; A381: 20
[50] Han G M. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010 (韩国明. 中国科学院金属研究所硕士学位论文, 沈阳, 2010)
[51] Kraft S, Zauter R, Mughrabi H. Fatigue Fract Eng Mater Struct, 1993; 16: 237
[52] Liu F, Wang Z G, Ai S H, Wang Y C, Sun X F, Jin T, Guan H R. Scr Mater, 2003; 48: 1265
[53] Zhang J X, Harada H, Ro Y, Koizumi Y, Kobayashi T. Acta Mater, 2008; 56: 2975
[54] Moverare J J, Johansson S, Reed R R. Acta Mater, 2009; 57: 2266
[55] Zhang J. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006 (张 剑. 中国科学院金属研究所博士学位论文, 沈阳, 2006)
[56] Xu Y B. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2013 (徐砚博. 中国科学院金属研究所硕士学位论文, 沈阳, 2013)
Outlines

/

〈 〉