STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES

  • Jiaojiao LI ,
  • Zengyun JIAN ,
  • Man ZHU ,
  • Junfeng XU ,
  • Fang'e CHANG ,
  • Min XIANG
Expand
  • School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710021

Online published: 2015-08-13

Supported by

Supported by National Basic Research Program of China (No.2011CB610403), National Natural Science Foundation of China (Nos.51371137, 51071115, 51171136, 51301125 and 51401156), Natural Science Basic Research Plan in Shaanxi Province of China (Nos.2012JM6010 and 2014JM6225) and Scientific Research Program Funded by Shaanxi Provincial Education Department (No.2013JK0907)

Abstract

The properties of the glasses and crystals of GexSe90-xSb10 (x=20, 23, 25, 30) prepared with melt quenching method have been analyzed by DSC. The glass transition temperature (Tg) of GexSe90-xSb10 glasses at different heating rates, the specific heat capacity and the entropy of the glasses and the crystals have been obtained. And on this basis, the kinetics ideal glass transition temperature (T0), the thermodynamics ideal glass transition temperature (TK) (Kauzmann temperature) and the kinetic fragility index (m) of GexSe90-xSb10 glasses have been determined. It is found that Tg, the specific heat capacity and the entropy increase with increasing the heating rate. Tg and T0 first increase and then decrease with increasing the Ge content, while TK increases linearly with the increase of Ge content. The m, Tg/TK, Tg/Tm and Tg/T0 are estimated to be 20.7~23.2, 1.183~1.352, 0.678~0.742 and 1.006~1.019, respectively. For each GexSe90-xSb10 glass in this work, its m is smaller than 30 and Tg/TK is larger than 1.1, which means that the GexSe90-xSb10 glass should be considered as a strong melt. The value of Tg/Tm is larger than 2/3, which indicates that amorphous GexSe90-xSb10 can be formed easily.

Cite this article

Jiaojiao LI , Zengyun JIAN , Man ZHU , Junfeng XU , Fang'e CHANG , Min XIANG . STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES[J]. Acta Metall Sin, 2015 , 51(11) : 1384 -1390 . DOI: 10.11900/0412.1961.2015.00072

References

[1] Angell C A. Science, 1995; 267: 1924
[2] Fontana G D, Battezzati L. Acta Mater, 2013; 61: 2260
[3] Mukherjee S, Schroers J, Johnson W L, Rhim W K. Phys Rev Lett, 2005; 94: 245501
[4] Turnbull D. Contemp Phys, 1969; 10: 473
[5] Kauzmann W. Chem Rev, 1948; 43: 219
[6] Jian Z Y, Zhou J, Chang F E, Jie W Q. Acta Metall Sin, 1999; 45: 1146 (坚增运, 周 晶, 常芳娥, 介万奇. 金属学报, 1999; 45: 1146)
[7] Debenedetti P G, Stillinger F H. Nature, 2001; 410: 259
[8] Gibson J M. Science, 2009; 326: 942
[9] Angell C A. J Non-Cryst Solids, 1985; 73: 1
[10] Cai A H, Ding D W, Xiong X, Liu Y, An W K, Zhou G J, Luo Y, Li T L, Li X S. Mater Des, 2014; 63: 233
[11] Gallino I, Schroers J, Busch R. J Appl Phys, 2010; 108: 063501
[12] Jiang Q K, Wang X D, Nie X P, Zhang G Q, Ma H, Fecht H J,Bendnarcik J, Franz H, Liu Y G, Cao Q P, Jiang J Z. Acta Mater, 2008; 56: 1785
[13] Battezzati L, Castellero A, Rizzi P. J Non-Cryst Solids, 2007; 353: 3318
[14] Battezzati L. Rev Adv Mater Sci, 2008; 18: 184
[15] Glade S C, Busch R, Lee D S, Johnson W L, Wunderlich R K, Fecht H J. J Appl Phys, 2000; 87: 7242
[16] Evenson Z, Busch R. Acta Mater, 2011; 59: 4404
[17] Jiang Q, Xu X Y, Li J C. Acta Metall Sin, 1997; 33: 6 (蒋 青, 徐晓亚, 李建忱. 金属学报, 1997; 33: 6)
[18] Legg B A, Schroers J, Busch R. Acta Mater, 2007; 55: 1109
[19] Jia R, Bian X F, Wang Y Y. Chin Sci Bull, 2011; 56: 3912
[20] Lu Z P, Li Y, Liu C T. J Appl Phys, 2003; 93: 286
[21] Senkov O N. Phys Rev, 2007; 76B: 104202
[22] Jiang Q K, Zhang G Q, Yang L, Wang X D, Saksl K, Franz H,Wunderich R, Fecht H, Jiang J Z. Acta Mater, 2007; 55: 4409
[23] Fiore G, Battezzati L. J Alloys Compd, 2009; 483: 54
[24] Fan G J, L?ffler J F, Wunderlich R K, Fecht H J. Acta Mater, 2004; 52: 667
[25] Zhu M, Li J J, Yao L J, Jian Z Y, Chang F E, Yang G C. Thermochim Acta, 2013; 565: 132
[26] Gallino I, Gross O, Fontana G D, Evenson Z, Busch R. J Alloys Compd , 2014; 615: S35
[27] Zhang X H, Guimond Y, Bellec Y. J Non-Cryst Solids, 2003; 326: 519
[28] Varshneya A K, Mauro D J. J Non-Cryst Solids, 2007; 353: 1291
[29] Vázquez J, Barreda D G, López-Alemany P L, Villares P, Jiménez-Garay R. J Alloys Compd, 2005; 390: 94
[30] Lee J H, Lee W H, Park J K, Yi J H, Shin S Y, Park B J, So B, Heo J, Choi J H, Kim H J, Choi Y G. J Non-Cryst Solids, doi:
[31] Soltana A S, Abu-Sehly A A, Joraid A A, Alamri S N. Thermochim Acta, 2013; 574: 73
[32] Tlchy L, Tichá H. J Non-Cryst Solids, 1995; 189: 141
[33] Guo H, Tao H Z, Gong Y Q, Zhao X J. J Non-Cryst Solids, 2008; 354: 1159
[34] Dinsdale A T. Calphad, 1991; 15: 317
[35] Angell C A. MRS Bull, 2008; 33: 544
[36] Martinez L M, Angell C A. Nature, 2001; 410: 663
[37] Ito K, Moynihan C T, Angell C A. Nature, 1999; 398: 492
[38] Angell C A. J Non-Cryst Solids, 1988; 102: 205
[39] Kissinger H E. Anal Chem, 1957; 29: 1702
[40] Rabinal M K, Sangunni K S, Gopal E S R. J Non-Cryst Solids, 1995; 188: 98
[41] Zhang C Z. PhD Dissertation, Shandong University, Jinan, 2011 (张春芝. 山东大学博士学位论文, 济南, 2011)
[42] Guo Y F, Yavari A R, Zhang T. J Alloys Compd, 2012; 536: 91
[43] Angell C A. Physica, 1997; 107D: 122
[44] Sreeram A N, Varshneya A K, Swiler D R. J Non-Cryst Solids, 1991; 128: 294
Outlines

/

〈 〉