INFLUENCE OF DIFFERENT THERMOMECHANICAL PROCESSES ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF Al-Mg-Si-Cu ALLOY SHEETS

  • Yan ZHANG ,
  • Mingxing GUO ,
  • Hui XING ,
  • Fei WANG ,
  • Xiaofeng WANG ,
  • Jishan ZHANG ,
  • Linzhong ZHUANG
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing,Beijing 100083

Online published: 2015-08-13

Supported by

Supported by National High Technology Research and Development Program of China (No.2013-AA032403), National Natural Science Foundation of China (Nos.51571023 and 51301016), Fundamental Research Funds for the Central Universities (Nos.FRFTP-14-097A2 and FRF-TP-15-051A3) and Beijing Laboratory of Metallic Materials and Processing for Modern Transportation (No. FRF-SD-B-005B)

Abstract

To reduce the weight of car body, Al-Mg-Si-Cu alloys are becoming increasingly attractive as a candidate for material substitution used to produce the outer body panels of automobiles because of their favorable bake-hardening response. However, the formability still needs to be further improved compared to steels. In this work, the effect of the thermomechanical processing on the mechanical properties and microstructure of Al-Mg-Si-Cu alloy is studied through tensile test, OM, SEM and TEM observation, as well as EBSD characterization. The results reveal that there is almost no change in both strengths and strain-hardening exponent n of the sheets in T4P condition after different thermomechanical processing, but the average plasticity strain ratio r-, planar anisotropy ∆r and elongations in the three directions show obvious differences. The sheet undergone hot rolling, cold rolling, intermediate annealing, cold rolling and solution (processing Ⅱ) has a better formability (r-= 0.6187) and a weaker planar anisotropy than that subjected to hot rolling, intermediate annealing and then cold rolling before solution treatment (processing I). Although the particle stimulated nucleation (PSN) effect of processing I is remarkable during solution treatment, due to the appropriate controlling cold deformation and distribution of second-phase particles with different sizes in processing Ⅱ, most of the recrystallization grains are equiaxial and the recrystallization texture is only consisted of CubeND, Cube and H with a low intensity. At last, according to the relationship between the microstructure and the thermomechanical processing, the microstructure evolution model during different thermomechanical processes is established.

Cite this article

Yan ZHANG , Mingxing GUO , Hui XING , Fei WANG , Xiaofeng WANG , Jishan ZHANG , Linzhong ZHUANG . INFLUENCE OF DIFFERENT THERMOMECHANICAL PROCESSES ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF Al-Mg-Si-Cu ALLOY SHEETS[J]. Acta Metall Sin, 2015 , 51(12) : 1425 -1434 . DOI: 10.11900/0412.1961.2015.00063

References

[1] Yu Z Q, Lin Z Q, Zhao Y X. Mater Des, 2007; 28: 203
[2] Gao Q M, Cao L S, Yu X D. Light Alloy Fabr Technol, 2009; 37: 30
[2] (高琪妹, 曹力生, 于晓丹. 轻合金加工技术, 2009; 37: 30)
[3] Engler O, Hirsch J. Mater Sci Forum, 1996; 217: 479
[4] Bennett T A, Petrov R H, Kestens L A I. Scr Mater, 2010; 63: 461
[5] Troeger L P, Starke Jr E A. Mater Sci Eng, 2000; A293: 19
[6] Peng X Y, Guo M X, Wang X F, Cui L, Zhang J S, Zhuang L Z. Acta Metall Sin, 2015; 51: 169
[6] (彭祥阳, 郭明星, 汪小峰, 崔 莉, 张济山, 庄林忠. 金属学报, 2015; 51: 169)
[7] Lievers W B, Pilkey A K, Lloyd D J. Mater Sci Eng, 2003; A361: 312
[8] Lankford W T, Snyder S C, Bauscher J A. Trans Am Soc Met, 1950; 42: 1197
[9] Hirofumi I, Takayuki T. Mater Trans, 2007; 48: 2014
[10] Leu D K. Int J Mach Tools Manuf, 1997; 37: 201
[11] Humphreys F J. Acta Metall, 1977; 25: 1323
[12] Orsund R, Nes E. Scr Mater, 1988; 22: 665
[13] Davies R K, Randle V, Marshall G J. Acta Mater, 1998; 46: 6021
[14] Bennett T A, Petrov R H, Kestensv L A I. Scr Mater, 2010; 62: 78
[15] Higginson R L, Aindow M, Bate P S. Mater Sci Eng, 1997; A225: 9
[16] Ito K, Musick R, Lucke K. Acta Metall, 1983; 31: 2137
[17] Jensen D J, Hansen N, Humphreys E J. Acta Metall, 1985; 33: 2155
[18] Hansen N, Jensen D J. Metall Trans, 1986; 17A: 253
[19] Hirsch J, Nes E, Lucke K. Acta Metall, 1987; 35: 427
[20] Kashihara K, Inagaki H. Metall Trans, 2009; 50A: 528
[21] Humphreys F J. Acta Metall, 1977; 25: 1323
[22] Engler O. Mater Sci Technol, 1996; 12: 859
Outlines

/

〈 〉