AUSTENITE TRANSFORMING IN CONTINUOUS COOLING PROCESS UNDER DIFFUSION CONTROL MODEL

  • Lei WANG ,
  • Di TANG ,
  • Yong SONG
Expand
  • Engineeing Research Institute, University of Science and Technology Beijing, Beijing 100083

Online published: 2015-08-10

Supported by

Supported by Fundamental Research Funds for the Central Universities (No.FRF-IC-14-005)

Abstract

Austenite-ferrite transformation in low carbon steels has a fundamental role in phase transformation and is industrial importance. The kinetics of austenite transformation can be described by the kinetics of austenite-ferrite interface migration. Two classical models, the diffusion-controlled growth model and the interface-controlled model, can be used to describe the growth of proeutectoid ferrite during g→a isothermal transformation. The austenite transformation in continuous cooling process is more common in production. In continuous cooling process, the equilibrium carbon concentrations in austenite and ferrite change with temperature and the kinetics of austenite transformation is different from that in isothermal process. Based on the models for g→a isothermal transformation, a diffusion control model is established for the growth of proeutectoid ferrite during the decomposition of supersaturated austenite in continuous cooling process. The interface position of proeutectoid ferrite varying with temperature is described with the model. The soft impingement effect at the later stage of transformation is considered. The carbon concentration at the austenite side of interface is difficult to reach the equilibrium carbon concentration when the cooling rate is high. A parameter as the function of cooling rate is proposed to modify the carbon concentration at the austenite side of interface. The polynomial diffusion field approximation is assumed in front of the interface. Simulation is done by utilizing the model to analyze the growth of proeutectoid ferrite in continuous cooling process with different bulk concentrations, austenite grain sizes and cooling rates. The interface position of proeutectoid ferrite as a function of temperature or time is obtained under different cooling conditions. Also, carbon diffusion length at the austenite side of interface as a function of time and carbon profile as a function of interface position are obtained under different cooling conditions. Furthermore, the proeutectoid ferrite fraction as a function of temperature can be acquired. The change law of carbon diffusion length with interface position and the change law of interface position with square root of time are discussed. The simulation results of diffusion control for austenite transforming in Fe-0.17C (mass fraction, %) alloy with grain size of 17 mm and different cooling rates show a good agreement with the literature results previously reported.

Cite this article

Lei WANG , Di TANG , Yong SONG . AUSTENITE TRANSFORMING IN CONTINUOUS COOLING PROCESS UNDER DIFFUSION CONTROL MODEL[J]. Acta Metall Sin, 2015 , 51(11) : 1341 -1348 . DOI: 10.11900/0412.1961.2015.00305

References

[1] Liu Z Y, Yang Z G, Li Z D, Liu Z Q, Zhang C. Acta Metall Sin, 2010; 46: 390 (刘志远, 杨志刚, 李昭东, 刘振清, 张 弛. 金属学报, 2010; 46: 390)
[2] Svoboda J, Fischer F, Fratzl P, Gamsjager E, Simha N K. Acta Mater, 2001; 49: 1249
[3] Bos C, Sietsma J. Scr Mater, 2007; 57: 1085
[4] Capdevila C, Caballero F, de Andres C G. Metall Mater Trans, 2001; 32A: 661
[5] Chen H, van der Zwaag S. J Mater Sci, 2011; 46: 1328
[6] Fazeli F, Militzer M. Metall Trans, 2005; 36A: 1395
[7] Gamsjager E, Militzer M, Fazeli F, Svoboda J, Fischer F D. Compu Mater Sci, 2006; 37: 94
[8] Purdy G, ?gren J, Borgenstam A, Brechet Y, Enomoto M, Furuhara T, Gamsjager E, Gouné M, Hillert M, Hutchinson C, Militzer M, Zurob H. Metall Mater Trans, 2011; 42A: 3703
[9] Bhadeshia H K D H. Prog Mater Sci, 1985; 29: 321
[10] van der Ven A, Delaey L. Prog Mater Sci, 1996; 29: 181
[11] Zener C. J Appl Phys, 1949; 20: 950
[12] Christian J W. The Theory of Transformations in Metals and Alloys. Oxford: Pergamon Press, 2002: 1
[13] Sietsma J, van der Zwaag S. Acta Mater, 2004; 52: 4143
[14] Xu Z Y. Principle of Phase Transformation. Beijing: Science Press, 1988: 1 (徐祖耀. 相变原理. 北京: 科学出版社, 1988: 1)
[15] Fan K, Liu F, Liu X N, Zhang Y X, Yang G C, Zhou Y H. Acta Mater, 2008; 56: 4309
[16] Offerman S E, van Dijk N H, Sietsma J, Lauridsen E M, Margulies L, Grigull S, Poulsen H F, van der Zwaag S. Acta Mater, 2004; 52: 4757
[17] Wang H F, Liu F, Zhang T, Yang G C, Zhou Y H. Acta Mater, 2009; 57: 3072
[18] Krielaart G P, Sietsma J, van der Zwaag S. Mater Sci Eng, 1997; 237: 216
[19] Serajzadeh S. J Mater Process Technol, 2004; 146: 311
[20] Hawbolt E, Chau B, Brimacombe J. Metall Trans, 1985; 16A: 565
[21] Johnson J W, Mehl R F. Trans AIME, 1939; 135: 416
[22] Avrami M. J Chem Phys, 1939; 7: 1103
[23] ?gren J. Acta Metall Mater, 1982; 30: 841
[24] Kumar M, Sasikumar R, Nair P K. Acta Mater, 1998; 46: 6291
[25] Offerman S, van Dijk N, Sistsma J, Grigull S, Lauridsen E M, Margulies L, Poulsen H F, Rekveldt M T, van der Zwaag S. Science, 2002; 298: 1003
Outlines

/

〈 〉