A NOVEL MODEL BASED ON VISCOELASTIC THEO- RY TO PREDICT THE TIME-DEPENDENT SPRINGBACK FOR DP600 STEEL SHEET

  • Shuai SUN ,
  • Daxin E
Expand
  • School of Materials, Beijing Institute of Technology, Beijing 100081

Online published: 2015-08-10

Supported by

Supported by National Natural Science Foundation of China (No.51175044)

Abstract

DP600 steel sheet with high strength has drawn much attention in the automotive industry, but the shape change following forming and unloading has not been known widely. The time-dependent springback of DP600 steel sheet was investigated under different pre-strains by uniaxial tension. According to the viscous behaviors under the elastic and plastic loading tests, the lower limit of integration in the constitutive equation of linear viscoelasticity was modified and the creep compliance was gained from the creep curve at a constant stress level of 309 MPa at room temperature. The predicted curve was acquired by using the superposition of the unloading impulse and the historical loading curve. The results reveal that the strain rates with high initial values gradually decreased following unloading at room temperature. As the pre-strain went up, both the absolute anelastic strain of time-dependent springback and the anelastic proportion of the total springback increased. Meanwhile, the direction of the time-dependent springback was same as that of the initial springback and opposite to the loading direction. In the same springback period, the ratio of the unloading stress to the creep springback strain tended to vary more linearly with the pre-strain than those obtained from immediate unloading. The simulated results using the revised model are in good agreement with the experimental data.

Cite this article

Shuai SUN , Daxin E . A NOVEL MODEL BASED ON VISCOELASTIC THEO- RY TO PREDICT THE TIME-DEPENDENT SPRINGBACK FOR DP600 STEEL SHEET[J]. Acta Metall Sin, 2015 , 51(11) : 1356 -1364 . DOI: 10.11900/0412.1961.2015.00176

References

[1] Wagoner R H, Lim H, Lee M G. Int J Plasticity, 2013; 45: 3
[2] Fei D Y, Hodgson P. Nucl Eng Des, 2006; 236: 1847
[3] Geng L M, Wagoner R H. Int J Mech Sci, 2002; 44: 123
[4] Li K P, Carden W P, Wagoner R H. Int J Mech Sci, 2002; 44: 103
[5] E D X, Liu Y F. Mater Des, 2010; 31: 3
[6] Cleveland R M, Ghosh A K. Int J Plasticity, 2002; 18: 769
[7] Correia J P M, Sim?es F, Gracio J J, Barlat F, Ahzi S. Mater Sci Eng, 2007; A456: 170
[8] Ryou H, Chung K. Compos Sci Technol, 2009; 69: 292
[9] Zener C. Elasticity and Anelasticity of Metals. Chicago: University of Chicago Press, 1948: 3
[10] Nowick A S,Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic Press, 1972: 21
[11] Munitz A, Kaufman M J. J Mater Sci, 2013; 48: 5361
[12] Li B, McClelland Z, Horstemeyer S J, Aslam I, Wang P T, Horstemeyer M F. Mater Des, 2015; 66: 575
[13] Wang J F, Wagoner R H, Carden W D, Matlock D K, Barlat F. Int J Plasticity, 2004; 20: 12
[14] Lim H, Lee M G, Sung J H, Kim J H, Wagoner R H. Int J Plasticity, 2012; 29: 42
[15] Yang T Q,Luo W B,Xu P,Wei Y T,Gang Q G. Viscoelastic Theory and Application. Beijing: Science Press, 2004: 3 (杨挺青,罗文波,徐 平,危银涛,刚芹果. 黏弹性理论与应用. 北京: 科学出版社, 2004: 3)
[16] Zang S L, Lee M G, Kim J H. Int J Mech Sci, 2013; 77: 194
[17] Michael E, Kassner, Kamia S. J Mater Res Technol, 2014; 3: 280
[18] Nie D F, Zhao J, Zhang J S. Acta Metall Sin, 2011; 47: 179 (聂德福, 赵 杰, 张俊善. 金属学报, 2011; 47: 179)
[19] Shui L, Jin T, Tian S G, Hu Z Q. Acta Metall Sin, 2007; 43: 47 (水 丽, 金 涛, 田素贵, 胡壮麒. 金属学报, 2007; 43: 47)
[20] Nie D F, Zhao J. Acta Metall Sin, 2009; 45: 840 (聂德福, 赵 杰. 金属学报, 2009; 45: 840)
[21] Sorvari J, Malinen M. Int J Solids Struct, 2006; 44: 1291
[22] Sorvari J, Malinen M, Hamalainen J. Int J Non-Linear Mech, 2006; 41: 1050
[23] Findley W N, Lai J S, Onaran K. Creep and Relaxation of Nonlinear Viscoelastic Materials. New York: North-Holland Publishing Company, 1976: 50
[24] Park S W, Schapery R A. Int J Solids Struct, 1999; 36: 1653
[25] Schapery R A, Park S W. Int J Solids Struct, 1999; 36: 1677
[26] Sorvari J, Malinen M. Mech Time-Depend Mater, 2007; 11: 143
Outlines

/