STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL

  • Yongwei SUN ,
  • Jizhi CHEN ,
  • Jun LIU
Expand
  • 1 College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001
    2 Luoyang Ship Material Research Institute, Luoyang 471000

Online published: 2015-07-16

Abstract

0Cr16Ni5Mo steel is the most popular material used for fasteners and bolts in the marine engineering equipment. With the light weight trend of equipment, the strength grades of the steel become higher. 0Cr16Ni5Mo steel combines high strength, high hardness and high fracture toughness with good ductility. However, high strength steel is prone to degradation by hydrogen, resulting in the loss of its excellent mechanical properties. And the presence of diffusible hydrogen near a notch tip is easily to cause crack propagation. The susceptibility to hydrogen embrittlement of steel is largely determined by the hydrogen diffusivity and the behaviors of hydrogen trapping in the steel. Therefore, the hydrogen trapping behaviors of 1000 MPa grade 0Cr16Ni5Mo steel have been investigated by means of thermal desorption spectroscopy (TDS). Meanwhile, the hydrogen embrittlement susceptibility of the notch and smooth specimens was evaluated by slow strain rate tests (SSRT), and the fracture morphology was also observed. The results showed that the main hydrogen traps of experimental steel was contained dislocations and grain boundaries. The elongation of hydrogen charged specimens was decreased obviously rather than tensile strength. With the increase in hydrogen concentration, the fracture surfaces of hydrogen charged specimens was displayed a transition from ductile microvoid coalescence to a mixed morphology of dimples, quasi-cleavage and intergranular features. The steel had little irreversible hydrogen due to less C content, and had much susceptibility with reversible hydrogen contained. The model of hydrogen induced stress was calculated on basis of Eshelby equivalent inclusion, validating the relationship between stress concentration and hydrogen concentration.

Cite this article

Yongwei SUN , Jizhi CHEN , Jun LIU . STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL[J]. Acta Metall Sin, 2015 , 51(11) : 1315 -1324 . DOI: 10.11900/0412.1961.2015.00033

References

[1] Kuduzovi? A, Poletti M C, Sommitsch C, Domankova M, Mitsche S, Kienreich R. Mater Sci Eng, 2014; A590: 66
[2] Tian Y, Wang M Q, Li J X, Shi J, Hui W J, Dong H. Acta Metall Sin, 2008; 44: 403 (田 野, 王毛球, 李金许, 时 捷, 惠卫军, 董 瀚. 金属学报, 2008; 44: 403)
[3] Li H L, Hui W J, Wang Y B, Dong H, Weng Y Q, Chu W Y. Acta Metall Sin, 2001; 37: 512 (李会录, 惠卫军, 王燕斌, 董 瀚, 翁宇庆, 褚武扬. 金属学报, 2001; 37: 512)
[4] Xiao J M. Acta Metall Sin, 1997; 33: 113 (肖纪美. 金属学报, 1997; 33: 113)
[5] Chu W Y,Qiao L J,Li J X,Su Y J,Yan Y,Bai Y,Ren X C,Huang H Y. Hydrogen Embrittlement and Stress Corrosion Cracking. Beijing: Science Press, 2013: 557 (褚武扬,乔利杰,李金许,宿彦京,岩 雨,白 洋,任学冲,黄海友. 氢脆和应力腐蚀. 北京: 科学出版社, 2013: 557)
[6] Hui W J,Weng Y Q,Dong H. The Steels of High-Strength Fasteners. Beijing: Metallurgical Industry Press, 2009: 64 (惠卫军,翁宇庆,董 瀚. 高强度紧固件用钢. 北京: 冶金工业出版社, 2009: 64)
[7] Ham J, Jang Y, Lee G, Kim B, Rhee K, Cho C. Mater Sci Eng, 2013; A581: 83
[8] Fransplass H, Langseth M, Hopperstad O S. Int J Mechani Sci, 2011; 53: 946
[9] Chu W Y, Li J X, Huang Z H. Corrosion, 1999; 55: 892
[10] Troiano A R. Trans ASM, 1960; 52: 54
[11] Oriani R A. Acta Metall, 1970; 18: 147
[12] Thomans D. Acta Metall Mater, 1994; 42: 2043
[13] Birnbaum H K, Sofronis P. Mater Sci Eng, 1994; A176: 191
[14] Yokota T, Shiraga T. ISIJ Int, 2003; 43: 534
[15] Kissinger H E. Anal Chem, 1982; 29: 135
[16] Gu J L, Chang K D, Fang H S, Bai B Z. ISIJ Int, 2002; 42: 1560
[17] Pressouyre G M. Metall Trans, 1979; 10A: 1571
[18] Escobar D P, Verbeken K, Duprez L. Mater Sci Eng, 2012; A551: 50
[19] Hirth J P. Metall Trans, 1980; 11A: 861
[20] Sofronis P, Birnbaum H K. J Mech Phys Solids, 1995; 43: 49
[21] Nabarro F R N. Proc Roy Soc, 1940; 175A: 519
[22] Li J C M, Oriani R A, Darken L S. Z Physik Chem Neue Folge, 1966; 49: 271
[23] Sofronis P, McMeeking R M. J Mech Phys Solids, 1989; 37: 317
[24] Chateau J P, Delafosse D, Magnin T. Acta Mater, 2002; 50: 1507
[25] Eshelby J D. Proc Roy Soc, 1957; 241A: 376
[26] Li H L, Chu W Y, Gao K W, Qiao L J. Acta Metall Sin, 2002; 38: 849 (李会录, 褚武扬, 高克玮, 乔利杰. 金属学报, 2002; 38: 849)
[27] Hardie D, Liu S E. Corros Sci, 1996; 38: 721
[28] Nagao A, Smith C D, Dadfarnia M, Sofronis P, Robertson I M. Proce Mater Sci, 2014; 3: 1700
[29] Robertson I M. Eng Fract Mech, 1999; 64: 649
[30] Abhay K J, Narayanan P R, Sreekumar K, Mittal M C, Ninan K N. Eng Fail Analy, 2008; 15: 431
Outlines

/

〈 〉